摘要
梅山尾矿有用铁矿物主要为赤褐铁矿和菱铁矿,通过强磁、重选、磨矿、细筛、反浮选、煅烧工艺的合理配置,使该尾矿在较低的选别成本下,得到了满足市场要求的最终铁精矿。
There were valuable iron minerals hematite, limonite and siderite in tailings of Meishan Iron Mine. The tailings were concentrated by the rational flowsheet configuration of high intensity magnetic separation, gravity separation, grinding, fine screening, reverse flotation and calcination processes under low cost, which achieved the final iron concentrate that met the needs of market.
出处
《矿业快报》
2006年第9期13-14,45,共3页
Express Information of Mining Industry
关键词
赤褐铁矿
碳酸铁
强磁
细筛
重选
反浮选
煅烧
Hematite and limonite
Iron carbonate
High intensity magnetic separation
Finescreening
Gravity separation
Reverse flotation
Calcination