期刊文献+

用抑制剂DG11降低安徽某硫化铜精矿氟镁含量 被引量:3

Reducing the Content of Fluorine and Magnesium in a Copper Sulfide Concentrate in Anhui Province Using the Inhibitor DG11
在线阅读 下载PDF
导出
摘要 安徽某硫化铜矿选矿厂铜精矿铜品位为18.20%,F、Mg O含量分别为0.25%和9.26%,不仅铜品位偏低,且F、Mg O含量不满足冶炼厂对铜精矿F含量小于0.1%、Mg O含量小于5%的要求。研究查明,含F、Mg O易泥化、易浮滑石、蛇纹石和绿泥石等以微细粒大量混杂进入铜精矿是造成现场铜精矿F、Mg O含量超标的主要原因。以广东省资源综合利用研究所研发的DG11为含氟镁脉石矿物的抑制剂,采用1粗1精1扫、中矿顺序返回浮选流程处理现场铜精矿,最终获得了铜品位为25.11%、铜回收率为97.45%,F和Mg O含量分别为0.082%和2.02%的铜精矿,既显著提高了精矿铜品位,又大幅度降低了精矿氟、镁含量,达到冶炼厂对铜精矿F和Mg O含量的要求。 The copper concentrate products of a sulfide copper ore dressing plant in Anhui province containing 18. 20%Cu,0. 25% F,9. 26% Mg O. Not only the copper grade is low,but also the content of fluorine and magnesium exceeds the standard of the smelting plant requires( content of F〈0. 1%,content of Mg O〈5%). Studies have shown that easy mudding and easy floating talc,serpentine and chlorite exist in the form of fine particles,these minerals containing F,Mg O and in large mixed into the copper concentrate,which is the main cause of fluoride,magnesium content in on-site copper concentrate exceeds the standard. Using DG11 developed by Guangdong Institute of Resources Comprehensive Utilization as inhibitor of the gangue minerals which contain fluorine and magnesium. Through the process of one roughing-one cleaning-one scavenging,and middling returning in proper order into the flow,the results show that the copper concentrate have 25. 11% grade and 97. 45%recovery rate,including 0. 082% F,2. 02% Mg O. It not only improves the grade of copper concentrate,but also greatly reduces the content of fluorine and magnesium in the concentrate,and reached the requirements of copper smelting plant.
出处 《金属矿山》 CAS 北大核心 2016年第7期121-124,共4页 Metal Mine
关键词 铜精矿 抑制剂DG11 Copper concentrate Fluorine Magnesium Inhibitor DG11
  • 相关文献

参考文献6

二级参考文献39

共引文献40

同被引文献136

引证文献3

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部