期刊文献+

UOE直缝埋弧焊管横向屈服强度测定的影响因素 被引量:1

Influence Factors on Transverse Yield Strength Measurement of UOE Submerged Arc Welding Pipe
在线阅读 下载PDF
导出
摘要 针对UOE直缝埋弧焊管横向屈服强度测定的3个重要影响因素.分别讨论了钢管横向板拉伸试样的压平影响和钢管横向圆棒拉伸试验的应变时效现象.并分析了拉伸试验速率的影响。得出了横向板拉伸试样的屈服强度低于圆棒拉伸的结果是由于试样的不平直原因引起的结论,同时对UOE铜管圆棒拉伸应变时效的防止和不同实验室拉伸速率的统一提出了建议。 For the main three influence factors on transverse yield strength measurement of UOE pipe, the influence of flattening in pipe transverse rectangular tensile test and the strain aging phenomenon in pipe transverse round tensile test were discussed, and the influence of tensile test speed was analyzed respectively. It was concluded that the reason of the yield strength of transverse rectangular tensile lower than that of transverse round tensile was that the transverse rectangular test pieces was out-of-straight. Moreover, suggestion was put forward about the prevention of strain aging in UOE pipe round tensile test and the uniform of tensile speed in different laboratories.
出处 《理化检验(物理分册)》 CAS 2013年第11期748-751,共4页 Physical Testing and Chemical Analysis(Part A:Physical Testing)
关键词 UOE钢管 压平 应变时效 拉伸速率 UOE pipe flattening strain aging tensile speed
  • 相关文献

参考文献6

二级参考文献60

共引文献92

同被引文献17

  • 1刘美华,李鸿琦,王静,王江宏,佟景伟.纳米压痕测量精度的影响因素[J].机械工程材料,2008,32(8):4-7. 被引量:11
  • 2CUI H X, WANG W Q, LI A J, et al. Failure analysis on the brittle fracture of 20 steel thick wall and high pressure pipe in an ammonia synthesis unit [J]. Engineering Failure Analysis, 2010, 17 (6): 1359-1376.
  • 3CUI H X, WANG W Q, LI A J, et al. Study on the brittle fracture of the Q245 steel high pressure piping in an ammonia synthesis unit[C]//Proceedings of the 12th International Conference on Pressure Vessel Technology. J ej u Island : [s. n. ],2009.
  • 4PETHICA J B, OI.IVER W C. Mechanical properlies of nanometer volumes of material: Use of elastic response of small area indentations[C]// BARNETT D M, BRAVMAN J C, NIX W D, et al. Thin Films Stress and Mechanical Properties, MRS Symposium Proceedings. Pittsburgh..Es.n.7, 1989, 130: 13-23.
  • 5HAGGAG F M, LUCAS G E. Determination of ltiders strains and flow properties in steels from hardness/microhardness tests [J]. Metallurgical and Materials Transactions A, 1983, 14(8): 1607 1613.
  • 6HAGGAG F M. Field indentation microprobe for structural integrity evaluation: US, 4852397 [P]. 1989 08-01.
  • 7TABOR D. The hardness of metals EM2. Oxford: Clarendon Press, 1951: 1-9.
  • 8HAGGAG F M, NANSTAD R K, HUTTON J T, et al. Use of automated ball indentation to measure flow properties and estimate fracture toughness in metallic materials[C]//BRAUN A A, ASHBAUGH N E, SMITH F M. Applications of Automation Technology to Fatigue and Fracture Testing. Philadelphia: American Society for Testing and Materials, 1990:188-208.
  • 9HAGGAG F M. In-situ measurements of mechanical properties using novel automated ball indentation system[C] //CORWIN W R, HAGGAG F M, SERVER W I.. Small Specimen Test Techniques Applied to Nuclear Reactor Vessel Thermal Ammaling and Plant Life Extension. Philadctphia: American Society for Testing and Materials, 1993: 27-44.
  • 10HAGGAG F M, MURTY K L. A novel stress strain microprobe for nondestructive evaluation of mechanical properties of materials[C]//LIAW P K, BUCK O, ARSENAULT R J, et al. Nondestructive Evaluation and Materials Properties 111 Warrendalc: The Minerals, Metals & Materials Society, 1997: 101-106.

引证文献1

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部