摘要
本实验主要是应用化学共沉淀法制备超细易烧的[MgO-Y2O3]-ZrO2粉末。通过实验得知:烧结特性对于快速沉淀,清洗十分敏感,通过改进实验方法,获得一种制备工艺简单,可用常规烧结,适用于生产的方法。
The fine [MgO-Y2O3]-ZrO2 powder has been prepared by chemical common-precipatation. The rusult shows that the sintering characteristcs are quite sensitive to the precipatating rate and the washing. By modifying the method we have got a simple processing suitable for industry production.
出处
《青岛大学学报(自然科学版)》
CAS
2000年第3期72-75,共4页
Journal of Qingdao University(Natural Science Edition)