摘要
制备了生物可降解的材料聚乳酸 ,用粘度法测定其分子量 ,并选用 A、B、C三种不同分子量的聚乳酸为药物的载体 ,制备了酮洛芬微球 ( AS、BS、CS) ,测定其粒径和体外溶出速率。结果表明催化剂四苯基锡用量增加 ,所得的聚乳酸分子量增加。而制备酮洛芬微球的聚乳酸分子量越大 ,其微球粒径越大 。
Three batches of polylactic acid (PLA) were prepared from lactic acid using tetraphenyl tin as a catalyst.Their molecular weights were evaluated by viscosimetry. PLA microspheres containing ketoprofen were made by the oil/water solvent evaporation process. The diameter of microspheres was measured by microscope. In vitro release of the ketoprofen from the PLA microspheres in phosphate buffer was investigated. The results indicate that the amount of catalyst affected the molecular weight of PLA which varied from 21000 to 69000. The release rates and diameters of the microsphere were found to be dependent on the molecular weight of PLA.
出处
《中国药科大学学报》
CAS
CSCD
北大核心
2000年第2期99-101,共3页
Journal of China Pharmaceutical University
关键词
聚乳酸
微球
酮洛芬
制备
释放度
Polylactic Acid
Microsphere
Ketoprofen
Preparation
Release