期刊文献+

3种非贵金属烤瓷合金的耐蚀性研究 被引量:4

Study on corrosion resistance of three non-noble porcelain alloys
暂未订购
导出
摘要 目的研究钴铬(Co-Cr)、镍铬(Ni-Cr)、镍铬铍(Ni-Cr-Be)3种非贵金属烤瓷合金在氯化钠溶液中的电化学腐蚀行为。方法铸造Co-Cr、Ni-Cr、Ni-Cr-Be 3种烤瓷合金的试件各5个,采用动电位极化法绘制合金的电极化曲线,测定合金的自腐蚀电位(Ecorr)、自腐蚀电流密度(Icorr)、钝化区间以及过钝化电位。采用扫描电子显微镜观察合金的显微组织,能谱扫描分析第二相成分。结果 Co-Cr合金的钝化膜完整、均匀、致密,耐蚀性最好;Ni-Cr合金局部的氧化膜致密性差,耐蚀性次之;Ni-Cr-Be合金中存在贫Cr、Mo的Ni-Be共晶相,耐蚀性最差。结论临床上应避免使用含Be的牙科烤瓷合金,Co-Cr合金的生物相容性优异,在牙科修复领域具有广阔的应用前景。 Objective To study the electrochemical corrosion behavior of Co-Cr,Ni-Cr and Ni-Cr-Be based porce-lain alloys in NaCl solution.Methods Five samples of each alloy were made respectively,electric polarization curve of each alloy was obtained using potentiodynamic polarization technique.Self-corrosion potential(Ecorr),self-corrosion current density(Icorr),passive region and transpassivation potential were tested.Microstructure and constituent was examined using scanning electron microscopy and energy dispersive spectroscopy.Results Co-Cr alloy possessed the most desirable corrosion resistance because of its integrated,homogeneous and compact passive film.The poor compactness of Ni-Cr alloy's passive film decreased its corrosion resistance.Ni-Cr-Be alloy exhibited the worst corrosion resistance due to the Cr and Mo depleted Ni-Be eutectic phases in the alloy.Conclusion Taking biological security into consi-deration,it is necessary to avoid the application of porcelain alloys with Be element.Co-Cr alloy with better biocompa-tibility possesses much broader prospect in the field of dental restoration.
出处 《华西口腔医学杂志》 CAS CSCD 北大核心 2011年第5期485-487,493,共4页 West China Journal of Stomatology
关键词 烤瓷合金 电化学腐蚀 耐蚀性 porcelain alloy electrochemical corrosion corrosion resistance
  • 相关文献

参考文献8

二级参考文献76

共引文献61

同被引文献31

引证文献4

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部