导出
摘要 用C-Si-Al复合还原剂在等高子感应炉内进行Cr-Ni精矿的熔融还原及合金化,钢中Cr和Ni的合金化目标值在20min内可达到18%和9%,Cr和Ni的收得率分别为82%-85%和95%-98%,碳含量可达到0.326%. When smelting reduction and alloying of chromium and nickel concentrate with C-Si-Al as compound is conducted in a plasma induction furnace, the alloying target value of 18% Cr and 9% Ni could be achieved in 20 min, the recovery rate of Cr and Ni would reach 82%-85% and 95%-98%respectively. Content of C could be limited within 0.326%. The properties of electrochemical reaction between plasma and plasma smelting slag and also analysed.
出处 《金属学报》 SCIE EI CAS CSCD 北大核心 1999年第7期731-734,共4页 Acta Metallurgica Sinica
基金 国家自然科学基金!59774014 武汉市科技攻关武科计[1998]104资助
关键词 等离子体 熔融还原 合金化 铬镍精矿 plasma smelting reduction ionized driving power alloying target value
  • 相关文献

参考文献6

共引文献3

同被引文献15

引证文献2

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部