摘要 首次报道熔体提拉法生长Cr∶LiCAF(Cr3+∶LiCaAlF6)晶体的生长工艺,研制出质量较好的晶体尺寸达20~25×90~120mm。测定了晶体对809nm红外波段的吸收系数μ为10-2量级,晶体中无OH-。Cr∶LiCAF可调谐灯泵激光器获得的宽带能量输出1.6J,阈值50.5J,调谐范围为730~848nm,用KDP调Q,单脉冲宽度48ns,峰值功率达1.3×106W。 Single crystal of Cr 3+ ∶LiCaLF 6 were grown for the first time in china by CZ technique without pure Pt growth chamber or in a flowing atmosphere of HF. the dimension of crystals were up to  20~25×90~120mm.The absorption coefficient of crystal at 809nm was 10 -2 cm -1 and no traces of OH were found in the boules by infrared spectroscopy.A flashlamp pumped Cr∶LiCAF tunable laser output energy of 1.6J,laser threshold 50.5J, from 730~848nm were observed,pulse width 48ns,peakpower 1.3×10 6Wwere obtained by Q switching with KD P .
出处 《人工晶体学报》 EI CAS CSCD 北大核心 1998年第1期39-42,共4页 Journal of Synthetic Crystals
基金 国家863资助
关键词 LiCaALF6 引上法 晶体生长 激光晶体 掺铬 性能 Cr 3+ ∶LiCaAlF 6, crystal pulling, tunable laser crystal, laser property
  • 相关文献

参考文献3

二级参考文献3

  • 1程立森,人工晶体学报,1994年,23卷,243页
  • 2程立森,1993年
  • 3Stephen A. Payne,L. L. Chase,L. K. Smith,Bruce H. T. Chai. Flashlamp-pumped laser performance of LiCaAIF6:Cr3+[J] 1990,Optical and Quantum Electronics(1):S259~S268

共引文献7

同被引文献5

引证文献1

二级引证文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部