摘要
针对江西某难选铜矿石的特征,进行了合理的选矿工艺流程和新药剂制度的研究。试验研究表明,采用铜部分优先、混选精矿再磨分选工艺流程,较大幅度地提高该难选铜矿石的分选指标,可获得品位21.15%、回收率83.62%的选铜技术指标。通过连续工业试验获得的选矿技术指标与原有的生产指标对比,新的浮选工艺制度可以提高铜品位1.07%和回收率18.33%。
In light of the characteristics of certain refractory copper ore from Jiangxi, investigation was made on its rational benefieiation process and new reagent regime. The results show that a process consisting of a partial copper preferential flotation and the regrinding and flotation of mixed concentrate can greatly improve the separation indexes of this refractory copper ore, with the copper concentrate grading 21.15% at a recovery of 83.62%. The continuous industrial test of this new process shows a copper grade increase of 1.07% and recovery increase of 18.33% compared with those of the original process.
出处
《金属矿山》
CAS
北大核心
2008年第11期46-48,57,共4页
Metal Mine
关键词
难选铜矿
铜硫分离
混选精矿再磨分选工艺
Refractory copper ore, Copper - sulphur separation, Regrinding of mixed concentrate