五种烤瓷合金在人工唾液中的离子析出研究 被引量:12

Ion release of five metal-ceramic alloys soaked in artificial saliva
暂未订购
导出
摘要 目的通过测定镍铬合金、镀金镍铬合金、涂金泥镍铬合金、钛合金和金钯合金5种烤瓷合金在人工唾液中,连续时间段内析出金属离子的种类和数量,为各类合金耐腐蚀性能的比较提供一定的实验依据。方法将各类合金制作的试件分别浸泡于ISO/TR10271标准唾液(37℃,pH=6)的实验介质中,运用原子吸收光谱分析仪在连续时间段内测定各类合金试件浸泡液中析出金属离子的种类和数量。结果钛合金离子析出量最多,但其中未检测出Ti;镀金镍铬合金和涂金泥镍铬合金离子析出量次之,镍铬合金离子析出量居第三,金钯合金离子析出量最少。结论金钯合金的离子析出量相对较少,耐腐蚀性能相对较好;镀金和涂金泥技术对镍铬合金的耐腐蚀性能未见显著改善;钛合金的离子析出量较镍铬合金还多,其耐腐蚀性能尚不够理想。 Objective To evaluate the ion release (including ion release rates, and ion types) of five types of metal- ceramic alloys such as nickel -chromium (Ni -Cr) alloy, gold plated Ni -Cr alloy, gold- mud coated Ni -Cr alloy, Ti -6Ak- 4V alloy and gold- palladium(Au- Pd) alloy soaked in artificial saliva. Methods Each specimen was soaked in artificial saliva ( ISO/TR10271, 37℃ and pH = 6) for 1, 3, 6 and 12 weeks, and the released ion amounts and types, release rate in saliva were then tested and analyzed with Atomic Absorption Speetrophotometry at each time point under a temperature of 37℃ and pH of 6. Results The ion release rate of Ti - 6Al - 4V alloy was the highest among the 5 groups, while that of Au - Pd ahoy was the lowest. The Au ion release rate of nickel - chromium alloy plated or coated with gold was higher than that of conventional nickel - chromium alloy. Conclusion Au - Pd alloy has superior corrosion resistance. The integration between gold and nickel - chromium ahoy is vulnerable, nickel - chromium alloy plated or coated with gold both have no persistent corrosion resistance. The corrosion resistance of Ti -6Al -4V alloy is not ideal.
作者 曾强 李玉玲
出处 《现代口腔医学杂志》 CAS CSCD 北大核心 2008年第6期621-623,共3页 Journal of Modern Stomatology
基金 广西科学基金课题资助项目(No0575056)
关键词 烤瓷合金 腐蚀 离子析出 人工唾液 Metal - ceramic alloys Corrossion Ion - release Artificial saliva
  • 相关文献

参考文献14

  • 1Berzins DW, Kawashima I, Graves R, et al. Electrochemical characteristics of high - Pd alloys irt relatlott to Pd - allergy. Dental Material, 2000,16 (4) :266 - 273.
  • 2Grimando NJ. Biocompatibility of nickel and cobalt dental alloys. Gen Dent, 2001,49(5) : 498 -503.
  • 3ISO/TR10271 Dentistry - Determination of tarnish and corrosion of metals and alloys. First edition ,Printed in Switzerland, 1993,3.
  • 4Hayes RB. The carcinogenicity of metals in humans. Cancer Causes Control, 1997,8(3) :371 -385.
  • 5Syverud M, Dahl JE, Hero H. Corrosion and biocompatibility testing of palladium alloy castings . Dent Mater,2001,17 ( 1 ) :7 - 13.
  • 6Wataha JC. Biocompatibility of dental casting alloys. J Prosthet Dent, 2000,83(2) :223 -234.
  • 7Wataha JC, Craig RG, Hanks CT. The release of elements of dental casting alloys into cell -culture medium. J Dent Res,1991,70(6) : 1014 -1018.
  • 8Kuphasuk C, Oshida Y, Andres C J, et al. Electrochemical corrosion of titanium and titanium - based alloys. J Prosthet Dent, 2001, 85(2) :195 - 202.
  • 9郭吕华,魏娟,张恒俊.前牙金瓷龈边缘和全瓷龈边缘烤瓷修复的美观效果观察[J].广东牙病防治,2001,9(4):272-273. 被引量:32
  • 10刘绍梅,贾安琦.镍铬合金涂覆有机金浆后的电化学腐蚀研究[J].西南国防医药,2004,14(4):369-371. 被引量:9

二级参考文献39

  • 1薛淼.牙科贵金属合金的过去和现状[J].口腔材料器械杂志,2004,13(3):160-162. 被引量:2
  • 2王晟,胡孝渊,储爱东.镍铬合金烤瓷冠过敏症:4例报道[J].上海口腔医学,2004,13(4):350-352. 被引量:32
  • 3徐君伍.口腔修复学(第3版)[M].北京:人民卫生出版社,1993,1..
  • 4张振庭.使金属烤瓷冠美观的牙体预备方法[英][J].国外医学:口腔医学分册,1988,15:119-119.
  • 5[3]Wataha JC,Craig RG, Hanks CT. J Dent Res, 1991 ;70(6): 1014
  • 6[4]Aziz - Kerrzo M, Conroy KG,Fenelon AM,et al. Electrochemical studies on the stability and corrosion resistance of titanium -based implant materials[J]. Biomaterials, 2001 ; 22:1531 - 1539
  • 7[5]Gill FG, Sanchez LA, Espias A, et al. Int Dent J, 1999;49 (6): 361
  • 8Wataha JC. J Prosthet Dent, 2000, 83 (2):223-234.
  • 9Wataha JC, Craig RG, Hanks CT. J Dent Res, 1991, 70(6) : 1014-1018.
  • 10Sun Z, Watatha JC, Hanks CT. J Biomed Mater Res, 1997,34 (1) :27-37.

共引文献54

同被引文献138

引证文献12

二级引证文献43

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部