静电纺丝聚乳酸/磷酸钙复合纳米纤维的力学性能 被引量:4

The mechanical properties of electrospun PLA/calcium phosphate composite nonafibers
原文传递
导出
摘要 运用静电纺丝技术制备了聚乳酸纳米纤维和聚乳酸/磷酸钙复合纳米纤维。对两种电纺纳米纤维的表面形态进行了扫描电子显微镜(SEM)的表征及单轴拉力测试表征。讨论了聚乳酸纳米纤维和聚乳酸/磷酸钙复合纳米纤维的力学性能。结果表明掺加了磷酸钙的聚乳酸纳米纤维的力学性能得到明显提高。 PLA nanofibers and PI.A/calcium phosphate composite nanofibers were prepared by eleetrospinning technology. The morphology of the two kinds of nanofihers were characterized by scanning electron microscopy (SEM). The mechanicaI properties of the PLA nanofierbs and pLA/Calcium Phosphate composite nanofihers were characterized by uniaxial tensile test respectively. And the properties of the PLA nanofibers,and PLA/Calcium Phosphate composite nanofibets were discussed. The result demonstrated the mechanical properties of PLA nanofibers mixed with calcium phosphate were increased.
作者 肖斌 李从举
出处 《化工新型材料》 CAS CSCD 北大核心 2008年第9期53-55,共3页 New Chemical Materials
基金 国家自然科学基金项目(50503001) 教育部新世纪优秀人才支持计划项目(NCET-05-0204) 北京市教委科技发展计划重点项目(KZ200510012010) 北京市属高等学校拔尖创新人才计划资助
关键词 力学性能 电纺 聚乳酸 磷酸钙 mechanical property, electrospinning, PLA, calcium phosphate
  • 相关文献

参考文献14

  • 1AnnChristine Albertsson and Indra K. Varma aliphatic polyesters: Synthesis, properties and applications [J]. J Chem Mater Sci, 2001, 157:31- 40.
  • 2Kricheldorf H R. Syntheses and application of polylaetides [J]. J Chemosphere, 2001 ,43:4954.
  • 3Dhirendra S K, Kyle W R, Frank K K. Bioresorbable nanofibePbased systems for wound healing and drug delivery: Optimization of fabrication parameters[J]. J Biomed Mater Res Part B:Appl. Biomater, 2004 70B(2):286-296.
  • 4Durselen L, Dauner M, Hierlemann H. Control of material stiffness during degradation for constructs made of absorbable polymer fibers [J].J Biomed Mater Res Part B: Appl Biomater, 2003, 67B(2) :697-701.
  • 5Bini T B, Gao S J, Xu X Y. Peripheral nerve regeneration by microbraided poly ( L-lactide-co-glycolide) biodegradable polymer fibers [J]. J Biomed Mater Res, 2004, 68A(2) : 286 -295.
  • 6瞿丽曼,肖沪卫.聚乳酸领域国内外专利特点分析及我国发展对策[J].化工进展,2005,24(7):818-819. 被引量:14
  • 7赖琛,唐绍裘,王迎军,魏小焜,张世英.微乳法合成磷酸钙纳米纤维及其机理探讨[J].化工学报,2005,56(5):942-946. 被引量:4
  • 8张骏,章庆国,张娇.新型多孔双相磷酸钙支架与兔骨髓间充质干细胞相容性的体外实验研究[J].中国美容医学,2007,16(5):588-592. 被引量:3
  • 9Webster T J, Doremus R H, Siegel R W, Bizios R, Ergun C. Enhanced functions of osteoblasts on nanophase ceramics [J].Biomaterials, 2000, 21:1803-1810.
  • 10Liao S S, Cui F Z, Zhang W, Feng Q L. Hierarchically biomimetic bone scaffold materials: nano-HA/Collagen/PLA corn posite [J]. J Biomed Mater Res, 2004,69:158

二级参考文献34

  • 1吕晶,张泉.聚乳酸复合纤维的性能及应用[J].产业用纺织品,2004,22(9):1-5. 被引量:8
  • 2李军.聚乳酸 可降解 用途广 市场好[J].医药化工,2004(6):14-17. 被引量:1
  • 3赵.生物降解塑料在包装领域的应用[J].国外塑料,2004,22(7):64-66. 被引量:1
  • 4许建中.骨组织工程的研究与开发进展[J].第三军医大学学报,2005,27(16):1625-1627. 被引量:10
  • 5杨帆 李明亚 金描真.一种用于治疗骨关节炎中药复方的聚乳酸微球及其制备方法[P].CN1559534.2005.
  • 6阎玉华 万涛.复合型聚乳酸缓释人工神经导管材料及制备方法[P].CN1562383.2005.
  • 7Williams DF. Biomaterials and tissue engineering in reconstructive surgery[J]. Sadhana-Acad Proc Eng Sci, 2003, 28: 563 -574.
  • 8Legeros RZ, Lin S, Rohanizadeh R, et al. Biphasic calcium phosphate bioceramics: preparation, properties and applications [J]. J Mater Sci: Mater Med, 2003, 14:201 -209.
  • 9Langer R, Vacanti JP. Tissue engineering [J]. Science, 1993, 260(5110): 920-926.
  • 10Stock UA, Vaeanti JP. Tissue engineering:current state and prospects[J]. Annu Rev Med, 2001, 52:443-451.

共引文献18

同被引文献42

引证文献4

二级引证文献33

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部