镍基铸造高温合金Ni80Cr20和NiCoCrMoX真空感应熔炼过程中Se元素的控制研究 被引量:2

Study on Controlling of Element Se during Vacuum Induction Smelting of Nickel-based Cast Superalloys Ni80Cr20 and NiCoCrMoX
在线阅读 下载PDF
导出
摘要 高性能航空发动机离不开性能优异的镍基铸造高温合金材料,而高纯净度是性能优良的镍基铸造高温合金的最重要的标志。为了得到高纯净度高温合金材料,需要对其中的杂质元素、气体元素、微量有害元素等进行有效控制,使其达到一个极低的水平(通常为10^(-6)级)。Se元素是影响高温合金性能的主要微量有害元素之一。本文对真空感应熔炼过程中镍基铸造高温合金中Se元素挥发性进行了一系列研究。结果表明,真空感应熔炼过程中,通过有效控制精炼温度、精炼时间和真空度,可使得镍基铸造高温合金Ni80Cr20和NiCoCrMoX中的Se元素含量降低到0.2×10^(-6)以下。 High performance aero-engine requires nickel-based cast superalloy materials with excellent performance and good purity,which is the most important symbol of nickel-based cast superalloys.In order to get the high-purity superalloys,it is necessary to effectively control the impurity elements,gas elements,harmful microelements,etc.,so that they can stay a very low level(usually 10^(-6) level).Selenium is one of the most major harmful microelements which can influence the properties of superalloys.In this paper,a series of studies have been carried out on volatility of selenium in nickel-based cast superalloys during vacuum induction smelting.The results show that selenium in nickel-based cast superalloys Ni80Cr20 and NiCoCrMoX can be reduced to 0.2×10^(-6) or less by controlling the refining temperature,refining time and vacuum during the process of vacuum induction smelting.
作者 张春晓 李树索 吴华杰 马思阳 马琛 裴延玲 叶超 ZHANG Chunxiao;LI Shusuo;WU Huajie;MA Siyang;MA Chen;PEI Yanling;YE Chao
出处 《大型铸锻件》 2024年第6期40-43,78,共5页 Heavy Casting and Forging
关键词 镍基铸造高温合金 Ni80Cr20 NiCoCrMoX 真空感应熔炼 Se元素 nickel-based cast superalloys Ni80Cr20 NiCoCrMoX vacuum induction smelting selenium
  • 相关文献

参考文献7

二级参考文献24

共引文献68

同被引文献51

引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部