炼油污水储罐的腐蚀与防护 被引量:2

Corrosion of Refinery Waste Water Tanks and Protection
在线阅读 下载PDF
导出
摘要 锦州石化公司 3 0 0 0m3炼油污水储罐因Cl- ,NH3,CN- 和酚等腐蚀介质的影响 ,致使原环氧防腐蚀涂层失效并有 3 0 0多处点蚀穿孔。经试验 ,聚硫橡胶改性环氧树脂对上述介质有良好的耐蚀性 ,随后用环氧聚硫橡胶玻璃鳞片玻璃钢内衬对储罐进行了修复 ,经近 4年使用 。 On the 3000 m 3 refinery waste water tank in Jinzhou Petrochemical Company, the epoxy resin corrosion protection coating failed and more than 300 pittings were found due to the corrosion media of Cl -, NH 3 and CN -. The test demonstrated that the polysulfide-rubber-modified epoxy was highly resistant to the corrosion by above corrosive media. The tank was then repaired using FRP lining with polysulfide rubber glass scale and has been operating for four years without any problem ever since.
作者 沈丽霞
出处 《石油化工腐蚀与防护》 CAS 2002年第4期22-23,共2页 Corrosion & Protection In Petrochemical Industry
关键词 炼油 污水储罐 腐蚀 防护 聚硫橡胶 改性 环氧树脂 玻璃鳞片 玻璃钢 衬里 waste water tank, corrosion, polysulfide-rubber-modified epoxy, glass scale, FRP, lining
  • 相关文献

参考文献1

二级参考文献3

共引文献6

同被引文献32

引证文献2

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部