湘钢高铁低硅烧结技术的生产实践 被引量:3

Production practice of high iron and low silicon sintering technology in Xiangtan Iron and Steel Co.,Ltd
原文传递
导出
摘要 通过对高铁低硅烧结成矿机理分析,发现改善固相反应条件,提高CaO的矿化度是提升产、质量的关键。湘钢360 m^2烧结机通过实施厚料层烧结、提高生石灰用量、降低漏风率等措施使烧结矿产、质量指标明显改善,转鼓强度提高了1.6%,利用系数提高0.15 t/(m^2·h),固体燃耗降低5.21kg/t。 Through the analysis of the sintering mechanism of high iron and low silicon sintering, it is found that the key to improve the production quality is to improve the conditions of solid phase reaction and increase the degree of mineralization of CaO. Through deep - bed sintering, increasing the rate of lime, reducing the rate of air leakage and other measures to make the sinter yield and quality index were improved in Xiangtan Steel 360 m2 Sintering Machine, the drum strength is increased 1.6%, the utilization coefficient is improved 0.15 t/( m2 · h), solid fuel consumption is decreased 5.21 kg/t.
出处 《烧结球团》 北大核心 2017年第6期39-42,62,共5页 Sintering and Pelletizing
关键词 高铁低硅 固相反应 厚料层烧结 CaO矿化度 high iron and low silicon solid state reaction deep -bed sintering CaO mineralization
  • 相关文献

参考文献2

二级参考文献14

  • 1中野正则 笠间俊次 细谷阳三.铁矿石シンタ—ク—キ构造に及ぼす石灰石粒度的影响[J].铁と钢,1985,(99):711-716.
  • 2志垣一郎ら.石灰石粗粒化によゐ烧结矿の生产性および还原粉化性の改善[J].铁と钢,1985,(71):1880-1887.
  • 3川口尊三ら.烧结矿CaO成分、SiO2成分低减の烧结生产性および品质に及ぼす影响[J].CAMP-ISIJ,1997,(10):949-949.
  • 4大山ら.プレ—ト型装入装置におけゐ烧结ベツドの空隙率と烧结生产性及ぼす磁场の影响[J].铁と钢,2000,(86):309-314.
  • 5小西ら.烧结ベツド内の通气性におよぼす下部通气孔の影响[J].CAMP-ISIJ,1995,(8):915-915.
  • 6野田英俊ら.高PCI操业下におけゐ低SiO2烧结矿の评价[J].CAMP-ISIJ,1997,(10):948-948.
  • 7市川孝一ら.低SiO2烧结矿の被还原性および高温性状评价[J].CAMP-ISIJ,1998,(11):850-850.
  • 8市川孝一ら.高微粉炭吹きNFDA1み高炉操业にNCACAした低SiO2烧结矿の制造技术[J].CAMP-ISIJ,2000,(13):702-705.
  • 9市川孝一ら.低SiO2烧结矿の还原溶融举动[J].CAMP-ISIJ,2000,(13):802-802.
  • 10松村藤ら.低スラグ烧结矿制造におけゐ技术课题[J].CAMP-ISIJ,2000,(13):718-721.

共引文献14

同被引文献47

引证文献3

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部