在实验室条件下,通过调整配料结构,可以实现烧结铁份的提高;在烧结提高TFe降低SiO2时,采取提高碱度、用活性灰代替生石灰、添加硼化物、燃料分加、熔剂分加、精矿预制粒、澳矿分加、提高料层厚度等措施,可起到强化提高TFe降低SiO2烧结的作用。
In laboratory conditions, the structure by adjusting the ingredients can be achieved sintered iron were increased ; in sintering to improve TFe lower SiO2, and take a raise alkalinity, with the activity of ash instead of lime, add borides, fuel sub-Canada, flux points Canada and pre-concentrate tablets, Australian mining sub-Canada, to improve measures such as material thickness, can serve to strengthen to improve TFe lower SiO2 sintering effect.
出处
《四川冶金》
CAS
2012年第5期18-23,共6页
Sichuan Metallurgy
关键词
钒钛磁铁矿
烧结
提高铁份
实验研究