含H_2S/CO_2油田腐蚀环境防腐选材调研
被引量:5
摘要
伊拉克米桑油田储层流体中高含腐蚀性气体CO2及H2S,2个主力油层Asmari和Mishrif,其中Asmari层,CO2分压为0.2 MPa,不含HS2气体;而Mishrif层CO2分压最高为1.3 MPa,H2S分压最高达到了0.8 MPa,CO2/H2S分压比范围2-6,属于高含硫化氢范围,此范围内,H2S的存在会对CO2腐蚀有促进作用。
基金
米桑油田油套管防腐研究(横向项目)
参考文献14
-
1朱培珂,邓金根,黄凯文,罗宇维,朱江林,吴山.油气田现场腐蚀检测装置设计与应用[J].科技导报,2014,32(19):68-72. 被引量:6
-
2Smith L,Celant M,Pourbaix A.A guideline to thesuccessful use of duplex stainless steels for flowlines[C] //Duplex America 2000conference.2000:18.
-
3Hiroshi H,Toshiyuki S,etc.Corrosion Behaviors of Cras Under CO2-H2S Environment with Organic Acids[C] //NACE Corrosion2012,paper No.0001129,2012.
-
4Mohd Z I,Neil H,etc.Corrosion Behavior Of Super 13Cr Martensitic Stainless Steels In Completion Fluids[C] //NACE Corrosion2003,paper No.03097,2003.
-
5Hisashi A,Yuji A,etc.Welded Joints Properties Of Super13Cr Martensitic Stainless Steel Considering Applicability To Field Fabrication[C] //NACECorrosion2002,paper No.02043,2002.
-
6H.A.Nasr-El-Din,A.S.Al-Khuraidah,etc.Recent Developments In High-Temperature Acidizing With Super 13Cr Completions:Laboratory Testing[C] //SPE Corrosion2002,SPE78557,2002.
-
7Mitsuo K,Yukio M,etc.Effect Of Retained Austenite On Corrosion Performance For Modified 13%Cr Steel Pipe[C] //NACE Corrosion2000,paper No.00137,2000.
-
8Takaaki T,Mitsuo K,etc.Development of new 13Cr steel pipe with high strength and good toughness[C] //NACE Corrosion2002,paper No.02044,2002.
-
9Yukio M,Mitsuo K,etc.Effects of chemical components on resistance to intergranular stress corrosion cracking in supermartensitic stainless steel[C] //NACE Corrosion2007,paper No.07092,2007.
-
10Hisashi A,Kunio K,etc.Effect of chromium and molybdenum on corrosion resistance of super 13Cr martensitic stainless steel in CO2 environment[C] //NACE Corrosion1998,paper No.98113,1998.
二级参考文献12
-
1李建平,赵国仙,郝士明.几种因素对油套管钢CO_2腐蚀行为影响[J].中国腐蚀与防护学报,2005,25(4):241-244. 被引量:51
-
2Hideki T, Masakatsu U, Yamamoto E, et al. Research into material selection for down-hole tubing by using dynamic field tester[C], 10th Abu Dhabi International Petroleum Exhibition and Conference, Abu Dhabi, October 13-16, 2002.
-
3Kermani B, Martin J W, Esaklul K A. Materials design strategy: Effects of H2S/CO2 corrosion on materials selection[C]. Corrosion, San Diego, California, March 12-16, 2006.
-
4Moosavi A N, Rumash K, Kadri M. Material selection for duwnhole sour environments[C]. 2008 Abu Dhabi International Petroleum Exhibition and Conference, Abu Dhabi, November 3-6, 2008.
-
5中华人民共和国国家质量监督检验检疫总局.GB/T3098.6-2000紧固件机械性能不锈钢螺栓、螺钉和螺柱[S].北京:中国标准出版社,2001.
-
6国家质量技术监督局.GB/T5783-2000六角头螺栓全螺纹[S].北京:中国标准出版社,2000.
-
7中华人民共和国国家质量监督检验检疫总局.GB/T13927-2008工业阀门压力试验[S].北京:中国标准出版社,2009.
-
8The Corrosion Society. NACE RP 0775-2005 preparation, installation, analysis, and interpretation of corrosion coupons in oilfieht operations [S]. Houston: NACE International, 2005.
-
9孙海.天然气压气站内腐蚀挂片监测管道内腐蚀[J].腐蚀与防护,2011,32(3):239-242. 被引量:13
-
10史涛,梁爱国,李甫,刘林江.油气管道腐蚀挂片悬挂装置的研制与应用[J].油气储运,2012,31(9):695-696. 被引量:10
共引文献5
-
1朱培珂,闫伟,李令东,段保平,沈雪峰,王芹.油管钢在模拟超临界CO_2中耐蚀特性的研究[J].表面技术,2016,45(12):167-173. 被引量:13
-
2闫化云.海上油田结垢问题探讨[J].涂层与防护,2018,39(1):15-20. 被引量:8
-
3朱培珂,崔明月,杨军征,路辉.采用新型测试装置在高含H2S油田现场检测腐蚀[J].石油工业技术监督,2019,35(9):37-39. 被引量:1
-
4刘海涵,黄传超,武丕烈.M油田A油层油井油套管防腐选材研究[J].石化技术,2021,28(9):50-52.
-
5李铭,苟浩瑞,于永洁,周俊岑,甘芳吉.金属管道腐蚀在线监测信号漂移的修正方法[J].郑州大学学报(工学版),2023,44(3):88-93. 被引量:1
同被引文献42
-
1姜志阳,徐艳迪,付国强.普光高含硫酸性气田主体开发用管道材料选用[J].石油工程建设,2009,35(S1):4-7. 被引量:4
-
2Hayes J R, Gray J J, Szmodis A W, et al. Influence of chromium and molybdenum on the corrosion of nickel-based alloys [J ~. Corrosion, 2006, 62(6) : 491-500.
-
3Kimura M, Miyata Y, Toyooka T, et al. Effect of test method on SSC performance of modified 13Cr steel[R]. NACE International, Houston, TX(US), 1998.
-
4Habicht W, Boukis N, Franz G, et al. Investigation of nickel-based alloys exposed to supercritical water environments [J]. Mierochimiea Acta, 2004, 145(1/4) : 57-62.
-
5Morton D S, Attanasio S A, Fish J S, et al. Influence of dissolved hydrogen on nickel alloy SCC in high temperature water[R]. Lockheed Martin, Schenectady, NY(US), 1999.
-
6Morton D S, Attanasio S A, Young G A. Primary water SCC understanding and characterization through fundamental testing in the vicinity of the nickel/nickel oxide phase transition [R]. Lockheed Martin Corporation, Schenectady, NY 12301 (US) , 2001.
-
7Ganesan P, Clatworthy E F, Harris J A. Development of a time- temperature transformation diagram for alloy 925 [J]. Corrosion, 1988, 44(11) : 827-835.
-
8Wang Z, Huang Y, Yang Y, et ah Atomic-size effect and solid solubility of muhicomponeut alloys[J]. Seripta Materialia, 2015, 94: 28-31.
-
9Michler T, Naumann J, Balogh M P. Hydrogen environment embrittlement of solution treated Fe-Cr-Ni super alloys [J]. Materials Science and Engineering: A, 2014, 607: 71-80.
-
10Harry Chandler. Heat Treater's Guide: Practices and Procedures for Nonferrous Alloys[M]. Ohio: ASM International, 1996.
引证文献5
-
1黄国平,唐瑞,刘海定,王东哲,李永友.铁镍基合金3YC61的强韧化工艺[J].金属热处理,2016,41(6):151-154.
-
2姜大伟.组合测井方法在深层气井套管质量评价中的应用[J].石油管材与仪器,2021,7(2):82-85. 被引量:3
-
3于昊成.海洋石油平台污油泵换型改造研究[J].机电工程技术,2023,52(5):291-294. 被引量:4
-
4张田,孟嘉岩,常城,张旭,陈希.湿H_(2)S环境下某气田高压压缩机橇选材设计[J].山东化工,2023,52(12):209-211. 被引量:1
-
5姜营.油田典型腐蚀环境的腐蚀机理及选材分析[J].化工装备技术,2023,44(5):32-34. 被引量:2
二级引证文献10
-
1张鸿文,赵帅,祝儒涛.海洋石油平台污油泵机械密封冲洗系统改造技术[J].中国石油和化工标准与质量,2024,44(3):160-162. 被引量:1
-
2杨海维.采油厂集输管道和设备硫化氢腐蚀评估与维护分析[J].中国设备工程,2024(8):180-182. 被引量:1
-
3王东升,杨天郁,胡志成.海洋平台海水提升泵选型及状态监测[J].机电工程技术,2024,53(5):282-285.
-
4武林芳,马焕英.MTD多层管柱探伤测井技术在海上油气田的应用[J].石油地质与工程,2025,39(2):122-126.
-
5朱莉娅,侯广信,陈志凌,李睿智,马强.泵用机械密封和辅助冲洗系统研究现状及发展方向[J].中国海上油气,2025,37(3):223-234. 被引量:1
-
6崔建松,王川,苏宏禹,张想,姜俊杰,茅巧智,孔利庆.海上油田离心泵机械密封冲洗防堵塞优化技术及应用[J].工程机械,2025,56(8):142-145.
-
7邵现振,任兰庆,陈军,赵会议,刘均荣,赵源,隋义勇.热采井水平筛管段防套损工艺参数界限研究[J].油气地质与采收率,2025,32(5):190-202.
-
8冯香,李玉玲,张超.海洋注气高压压缩机成橇的可靠性设计要点[J].石油和化工设备,2025,28(11):110-115.
-
9万明奇,张国庆,王洪福,姚远,谭红莹.海洋石油工程硫化氢腐蚀检测与防治[J].涂层与防护,2025,46(11):49-55.
-
10高德利,李宁,黄文君,董雪林,石小磊.超深井套管柱力学与控制研究若干进展及展望[J].中国石油大学学报(自然科学版),2026,50(1):84-98.
-
1魏志华,蔡卫.钢结构厂房托梁拔柱与结构加固技术研究[J].中国建筑金属结构,2013(10X):29-29. 被引量:1
-
2希望深蓝推出热水双段型冷水机组[J].制冷与空调,2013,13(4):102-102.
-
3李聚文.变频器定期检查的注意事项[J].啤酒科技,2012(3):49-49.
-
4Sabine Muhlenkamp.腐蚀性气体的检测能够抵抗沼气腐蚀的检测传感器[J].流程工业,2012(15):40-41.
-
5张玉芳.用于含CO_2/H_2S环境的缓蚀剂研制[J].石油与天然气化工,2005,34(5):407-409. 被引量:22
-
6木具.别墅家具时尚 防腐选材尤重[J].国际木业,2011(6):31-31.
-
7电线使用一定年限后会不会引起火灾?[J].消防与生活,2007(9):28-28.
-
8封洪庆.我厂尿素硝铵系统建构筑物的防腐选材及其施工[J].泸天化科技,1989(2):41-42.
-
9工业烟囱的腐蚀与控制[J].全面腐蚀控制,2006,20(2):48-48.
-
10希望深蓝发布热水型双段型冷水机组[J].供热制冷,2013(5):72-72.