期刊文献+

年产20t纳米ZnO中试研究及生产 被引量:11

The pilot test with 20t/year production of nanometer-size zinc oxide preparation
在线阅读 下载PDF
导出
摘要 用均匀沉淀法制备纳米ZnO中试研究表明 :尿素水解和沉淀反应采用间歇操作的搅拌釜式反应器是合适的 ;小试提供的原料路线是可行的 ,工艺条件是正确的 ;进一步放大在满足工艺条件的前提下 ,反应前升温的供热强度不小于 60kJ/(min·L) ;反应结束后的冷却换热强度不小于 2 7kJ/(min·L)。中试装置的生产能力为 2 0t/年 ,产品纳米氧化锌粒径为 35~80nm ,收率达到 80 %。 The homogeneous precipitation method is used for preparing nanometer size zinc oxide in the pilot test. The test results show that the batch stirring reactor is suitable for hydrolysis of urea and precipitation reaction, the raw material and process conditions in lab.test are applicable for pilot scale.In the pilot test, the heating strength is not less than 60kJ/(min·L) for temperature raise stage before reaction and the cooling strenth is not less than 27kJ/(min·L) for cooling stage after reaction.The production amount of pilot test installation is 20t/year,the particle diameter of nanometer size ZnO prepared is 35~80nm and yield 80%.
出处 《功能材料》 EI CAS CSCD 北大核心 2001年第4期410-412,共3页 Journal of Functional Materials
关键词 均匀沉淀法 生产 纳米氧化锌 nanometer size zinc oxide homogeneous precipitation method pilot test manufacture
  • 相关文献

参考文献3

二级参考文献9

共引文献67

同被引文献184

引证文献11

二级引证文献85

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部