摘要
用收集气体和定电阻放电的方法,研究了几种粘合剂在单独使用或混合使用时对无汞碱性锌锰电池负极析气及电池放电性能的影响。研究结果表明:单独使用或混合使用的粘合剂可以阻滞负极的析气行为,不同种类与组成的粘合剂对电池放电性能的影响不同,且CMC不宜与PAA混用。
The effect of adhensives on negative electrode gas evolution and on discharge performance of mercury-free alkaline Zn/MnO2 battery were experimented by the method of collecting evolution gas and by the battery discharge in fixed resistance.The results showed that adhensive agents in different kind and different mixture ratio could decrease negative electrode gas evolution,and its effects on discharge performance of battery were also different.And the mixtures of CMC with PAA could not be used.
出处
《电池工业》
CAS
2001年第4期153-154,共2页
Chinese Battery Industry
关键词
无汞碱锰电池
粘合剂
电池性能
锌粉
Alkaline zinc-manganese battery;Gas evolution;Adhansives