摘要
测定了300系不锈钢在稀硫酸介质中磨损率、摩擦系数及钝化膜破坏后的修复时间,还观察了磨痕形貌。实验表明高合金化的不锈钢磨蚀失重大于一般的304不锈钢。本文结果预示着发展耐磨蚀合金的道路不同于耐蚀合金。
The corrosive wear rates, friction coefficient and reformation period
of passive film of stainless steel specimens were determined in dilute H_2SO_4 solu-
tion and then the morphology of the wear tracks was observed. The experiment
shows that the corrosive wear rate of high alloy stainless steel is higher than that
of 304 stainless steel. It is suggested that the way to develop an alloy to be appli-
ed to corrosive wear is not the same as those used in corrosion environment.
出处
《金属学报》
SCIE
EI
CAS
CSCD
北大核心
1991年第4期B021-B024,共4页
Acta Metallurgica Sinica
关键词
不锈钢
腐蚀
磨损
稀硫酸介质
corrosive wear
stainless steel
corrosive wear resisting alloy