过氧化物预硫化天然胶乳胶膜的热氧降解及防护 被引量:1

Thermo-oxidative Degradation of Peroxids Prevulcanized Natural Rubber Latex Film and Its Prevention
在线阅读 下载PDF
导出
摘要 用热重法-微分热重法(TG-DTG)和差热分析(DTA),测定加入不同防老剂的过氧化物预硫化胶乳(PPVL)胶膜的有关热动力学参数来评价它们的耐热氧降解性能,筛选出的防老剂2246、2246/264能给PPVL胶膜好的抗热氧降解性能,2246、264并用有协同效应。 The thermo-oxidative degradation of the peroxide prevulcanized latex (PPVL) film was determined with TG-DTG and DTG. The thermo-dynamic parameters of the PPVL films with different anti-agers added were determined in order to evaluate their thermo-ox- idative resistance. PPVL films added with selected anti-agers 2246 and 2246/264 displayed ed thermo-oxidative resistance. The combination of anti-agers 2246 and 264 shows syner- getic action.
出处 《热带作物学报》 CSCD 2000年第3期9-14,共6页 Chinese Journal of Tropical Crops
关键词 橡胶 胶乳 预硫化天然胶乳 热氧降解 防老剂 rubbver latex puevulcanized latex hermo-oxidative degradation anti-ager
  • 相关文献

参考文献7

二级参考文献14

共引文献27

同被引文献18

  • 1H.G.Oikland.R,J.M.Hulskotte,L.van der Docs,辜晓乐.在三烯丙基氰脲酸酯活性剂存在下EPDM过氧化物硫化的机理[J].橡胶参考资料,1994,24(4):54-59. 被引量:1
  • 2冲仓元治.有机过氧化物硫化胶乳及其应用[J].胶乳工业,1983,(1):34-24.
  • 3华南热带农业大学工学院.胶乳与生胶的分析与试验[M].海南:华南热带农业大学,1997..
  • 4高分子科学研究所.平衡溶胀法测定交联聚合物的溶度参数与交联度-高分子试验技术[M].上海:复旦大学出版社,1996.50-52.
  • 5高分子教研室高分子化学小组.高分子化学实验[M].广州:中山大学出版社,1993.50.
  • 6刘晓冬(译).胶乳预硫化工艺的化学过程[J].胶乳工业,1993,(4):43-54.
  • 7袁子成.一些因素对硫化胶乳性质的影响[J].热带作物学报,1986,7(2):1-11.
  • 8Low E H.天然胶乳预硫化的研究[J].胶乳工业,1985,(4):27-34.
  • 9黄良平.赴印尼参加天然胶乳辐射硫化培训的技术报告[J].胶乳工业,1992,(1):4-9.
  • 10Blackley D C.天然胶乳的机械稳定性[J].胶乳工业,1985,(3):12-18.

引证文献1

二级引证文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部