以ITO导电玻璃为基材,采用溶液化学法分两步制备CePO4及Eu3+掺杂CePO4一维纳米薄膜.研究底膜液提拉次数、底膜厚度、陈化液pH值和陈化时间等对薄膜形貌的影响.采用扫描电子显微镜、X射线衍射仪和荧光分光光度计等对CePO4及Eu3+掺杂CePO4一维纳米薄膜进行表征.结果表明,用无水乙醇底膜液,提拉3~6次,经350℃煅烧,在pH值为1.4~1.6的水相陈化液中,90℃水浴陈化3~6 h,即可在ITO导电玻璃上制得平整致密,具有较大比表面积的六方晶相CePO4及Eu3+掺杂CePO4一维纳米薄膜.
Eu^3 + doped one-dimensional nanostructured CePO4 thin films were prepared by a two-step solution chemical method on ITO conductive glass. The effects of substrate membrane liquid, dip-coating times, thickness of substrate membrane, pH values of aging solution and aging time on the morphology of CePO4 thin films were systematically studied. The Eu^3+ doped one-dimensional nanostructured CePO4 films were characterized by scan-ning electron microscope, X-ray diffratometer, and fluorescence spectrophotometer. These results indicate that Eu^3 + doped one-dimensional nanostructured CePO4 thin films with hexagonal phase and a larger specific surface can be prepared by dipping-coating 3 - 6 times in the anhydrous ethanol with further heat treatment at 350 ℃, then aged in the 1.4 - 1.6 pH liquid for 3 - 6 h at 90 ℃.
出处
《深圳大学学报(理工版)》
EI
CAS
北大核心
2013年第1期17-22,共6页
Journal of Shenzhen University(Science and Engineering)
基金
国家自然科学基金资助项目(50674068)~~