期刊文献+

单斜相纺锤形纳米ZrO_2富集分离电感耦合等离子体质谱法测定痕量Ni(Ⅱ) 被引量:1

Determination of Trace Nickel(Ⅱ) by Inductively Coupled Plasma Mass Spectrometry after Pre-concentration/ Separation with Monoclinic Fusiform Nanometer-Size Zirconium Dioxide
在线阅读 下载PDF
导出
摘要 采用水热法合成单斜相纺锤形纳米二氧化锆(ZrO2),建立以单斜相纺锤形纳米ZrO2为吸附剂电感耦合等离子体质谱(ICP-MS)测定痕量Ni2+的方法。本方法对Ni2+的检出限为0.029μg/L,相对标准偏差为2.7%(n=6);结果表明,在pH 9.0、吸附10 min时,纳米ZrO2对Ni2+的吸附率可达99%以上;以2 mL 0.5mol/L HCl为洗脱剂洗脱30 min,可定量洗脱纳米ZrO2上吸附的Ni2+,洗脱率达98%以上;纳米ZrO2对Ni2+的静态吸附容量为198μg/g、富集倍数可达250倍;考察了共存离子的影响以及其再生性能。将本方法应用于实际水样中痕量镍的测定,方法回收率为96.3%~101.4%。 Monoclinic fusiform zirconium dioxide(ZrO2) nanoparticles were synthesized by hydrothermal method,a method for the determination of Nickel2+ was developed by inductively coupled plasma mass spectrometry(ICP-MS) with monoclinic fusiform nanometer-sized ZrO2 as absorbent.The detection limit to Ni2+ was 0.029 μg/L and the relative standard deviation was 2.7%(n=6).Optimal adsorption and elution conditions of nanometer-sized ZrO2 to Ni2+ were studied,adsorption percentage of nanometer-sized ZrO2 to Ni2+ was more than 99% under pH 9.0 and 10 min,2 mL 0.5 mol/L HCl was sufficient for elution to Ni2+ more than 98%.The static adsorption capacity of ZrO2 to Ni2+ was 198.4 μg/g and enrichment factor reached 250.Effects of co-existing ions and regeneration properties were discussed.The method has been applied to the determination of trace Ni2+ in real water samples,the recoveries were 96.3%-101.4%.
出处 《分析化学》 SCIE EI CAS CSCD 北大核心 2012年第12期1890-1896,共7页 Chinese Journal of Analytical Chemistry
基金 国家自然科学基金(No.20871043)资助
关键词 纳米二氧化锆 富集 分离 电感耦合等离子体质谱(ICP-MS) Nanometer-sized zirconium dioxide Pre-concentration Separation Inductively coupled plasma mass spectrometry Nickel
  • 相关文献

参考文献15

二级参考文献167

共引文献168

同被引文献21

引证文献1

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部