海底管道腐蚀后的剩余强度评价 被引量:2

Evaluation for Residual Intensity of Corroded Pipelines
在线阅读 下载PDF
导出
摘要 海底管道通常会因腐蚀而形成各种不同类型的缺陷,影响管道的承载能力和使用寿命。本研究在准确掌握管道缺陷发展情况的基础上,分别根据行业规范和采用有限元方法对海上油田含有腐蚀缺陷的原油管线进行剩余强度评价,判定海底管道修复的必要性和修复的紧迫程度,以确定最终的管线修复方案,可供类似海底管道修复工程参考。 Subsea pipelines are corroded, which usually leads to different defects, decreases the bearing capacity and service life. Based on grasping the detail of pipeline defects precisely, the industrial standard and finite element analysis are adopted respectively to evaluate residual intensity of the offshore oil pipeline with corrosion defects, define the necessity of subsea pipelines repairing, and determine final pipeline repairing scheme based on the urgent need, which will provide the reference for similar subsea pipelines repairing project.
作者 江锦
出处 《港工技术》 2012年第3期25-27,共3页 Port Engineering Technology
关键词 海底管道 腐蚀 缺陷 剩余强度 管道修复 subsea pipeline corrosion defect residual intensity pipeline repairing
  • 相关文献

参考文献4

  • 1ASMEB31G--2009确定已腐蚀管道剩余强度的手册[S].[s.1.]:美国机械工程师协会,2009.
  • 2马彬,帅健,李晓魁,王俊强,冯庆东.新版ASME B31G—2009管道剩余强度评价标准先进性分析[J].天然气工业,2011,31(8):112-115. 被引量:52
  • 3ASME B31G--1991确定已腐蚀管道剩余强度的手册[S].[S.1.]:美国机械工程师协会,1991.
  • 4DNV RP F101 Corroded Pipelines[S].[S.1.] :挪威船级社.2010.

二级参考文献9

共引文献51

同被引文献14

引证文献2

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部