摘要
介绍了某铁粗精矿的工艺矿物学性质,根据试样的矿石性质,确定采用硫浮选—磨矿—磁选工艺流程,获得了全铁66.25%、含硫0.50%的铁精矿。
This paper describes mineralogical composition of the iron crude concentrate.According to the characteristics,by the process of sulfur flotation—grinding—magnetic separation,an iron concentrate of 66.25% Fe with sulfur content of 0.5% can be obtained.
出处
《湖南有色金属》
CAS
2012年第1期17-20,63,共5页
Hunan Nonferrous Metals
关键词
铁粗精矿
浮选
磨矿
磁选
iron crude concentrate
flotation
regrinding
magnetic separation