摘要
文章介绍了某尾矿的工艺矿物学性质,根据尾矿的矿石性质,确定采用硫浮选→磨矿→磁选工艺流程,获得了全铁63.44%、含硫0.54%的铁精矿;硫35.58%的硫精矿。
This paper describes the mineralogical composition of the tailings. According to the characteristics, by the process of Sulfur flotation→grinding→magnetic separation, an iron concentrate of 63.44% Fe with content of 0.54% S and a Sulfur concentrate of 35.58% S can be obtained.
出处
《湖南有色金属》
CAS
2009年第3期15-18,共4页
Hunan Nonferrous Metals
关键词
尾矿
浮选
磨矿
磁选
tailings
flotation
grinding
magnetic separation