摘要
对从天然氧化锰矿(NMD)活化制备得到的活性放电锰(ANMD)的重质化加工技术进行了讨论和试验研究,试验确定了重质化工艺适宜的工艺条件,产品的视比重可达1.8g/cm 3 以上,活性氧化锰的放电性能可达到或接近电解二氧化锰的质量标准。
The technology of increasing the ANMD weight in the activation process of natural manganese ore was discussed.The experiments was undertaken to determin the conditions which can increase the ANMD weight.The visual specific gravity was raised to 1.83g/cm 3 and the discharge property was up to the EMD standard.
出处
《矿产综合利用》
CAS
北大核心
2000年第1期19-21,共3页
Multipurpose Utilization of Mineral Resources