摘要
运用高压静电纺丝和程序焙烧方法,制备α-K_7P_2W_(17)FeO_(61)纳米纤维丝。通过红外光谱(FTIR),X射线粉末衍射(XRD)进行了表征,结果表明制备的纳米纤维是纯α-K_7P_2W_(17)FeO_(61),扫描电子显微镜照片(SEM)显示焙烧后产物为纳米纤维丝,直径分布图显示其平均直径大约为1 55nm。
The nanofibers of α-K7P2W17FeO61 were obtained through electrospun and calcinations methods. FTIR spectroscopy and XRD showed that nanofibrous polyoxometalates was α-K7P2W17FeO61. Scanning electron microscopy images and diameter distribution curves of the fibrous membranes indicated that the average diameter of α-K7P2W17FeO61 fibers was about 155nm.