摘要 针对热模法离心铸造球铁管普遍存在的伸长率低问题,从离心铸造的特点出发分析了残余镁的变化。与冷模法比较,较长的凝固过程,使铁水中残余镁的过度氧化是导致热模法离心铸造球铁管伸长率低的根本原因。提高其伸长率的途径是防止氧化和缩短凝固时间。 Low elongation is a general existing problem in hot mold by centrifugal casting for ductile iron pipe. The change of residnal Mg in molten iron was analyzed based on the feature of centrifugal casting. It is found that this disadvantage is attributed to the superoxidation of iron melt and the loss of Mg due to the centrifugal effect and the comparatively long holding time of the molten iron in the hot mold. One way to increase the elongation is to properly prevent Mg from oxidation, and the other is to shorten the solidification time.
出处 《特种铸造及有色合金》 CAS CSCD 北大核心 1999年第3期36-37,共2页 Special Casting & Nonferrous Alloys
基金 国家"九五"科技成果重点推广计划 河北省自然科学基金
关键词 离心铸造 球墨铸铁 伸长率 热模法 Centrifugal Casting, Ductile Iron, Elongation
  • 相关文献

参考文献4

  • 1张博 等 任善之等(译).球墨铸铁[M].北京:机械工业出版社,1988..
  • 2刘庆星,离心铸管,1994年
  • 3安阁英,铸件形成理论,1990年
  • 4任善之(译),三球墨铸铁,1988年

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部