摘要
用扫描俄歇探针(SAM)结合真空热处理试验,研究了95W-Ni-Fe合金的脆化 机理,发现烧结态合金中散布着氧的高浓度富集区,这是钨合金脆化的重要因素。1000℃以 上的真空热处理可以消除氧高浓度富集区和降低界面氧浓度,使合金延性、韧性显著提高。
The embrittling mechanism of 95W - Ni - Fe alloy has been researched by using Scanning Auger Microprobe(SAM) combined with heat treatment in vacuum. It has been found that high oxygen con- centration coalescent zones(HQCCZ) scattered in sintered state alloys. HOCCZ is an important embrittling fac- tor of the tungsten alloy. Heat treatment in vacuum over 1000℃ can eliminate OHCCZ, decrease oxygen con- centration at interfaces and allow evident enhancement of elongation and toughness of the alloy.
出处
《兵器材料科学与工程》
CAS
CSCD
北大核心
1999年第1期3-6,11,共5页
Ordnance Material Science and Engineering
基金
天津市自然科学基金