期刊文献+

抛光加工参数对KDP晶体材料去除和表面质量的影响 被引量:10

Effect of Polishing Parameter on Material Removal and Surface Quality of KDP Crystal
在线阅读 下载PDF
导出
摘要 针对软脆易潮解KDP功能晶体材料的加工难点,提出了一种基于潮解原理的无磨料化学机械抛光新方法,研制了一种非水基无磨料抛光液,该抛光液结构为油包水型微乳液。通过控制抛光液中的含水量可以方便地控制KDP晶体静态蚀刻率和抛光过程中材料的去除率。实验中还研究了不同加工参数对晶体材料去除率和已加工表面质量的影响。该抛光液的设计为易潮解晶体的超精密抛光加工提供了一条新的技术途径。 KDP crystal is extremely soft,brittle and hygroscopic,which make it difficult to form a flawless surface via conventional processing methods.In this paper,chemical mechanical abrasive-free polishing technique based on deliquescence theory was applied to obtain the KDP crystal with super smooth surface.A non-aqueous slurry (W/O structure) was designed to carry out the polishing process.Water concentration in the slurry was changed to control the static etch rate and material removal rate in polishing process.The effect of different parameters such as platen speed and pressure on material removal and surface quality were studied.The design of such slurry provides a new technique for polishing process of hygroscopic crystals.
出处 《人工晶体学报》 EI CAS CSCD 北大核心 2010年第1期29-33,43,共6页 Journal of Synthetic Crystals
基金 国家自然科学基金重点资助项目(No.50535020) 山东大学晶体材料国家重点实验室开放基金(KF0904)
关键词 KDP晶体 无磨料抛光 材料去除 表面质量 KDP crystal abrasive-free polishing material removal surface quality
  • 相关文献

参考文献9

  • 1The National Ignition Facility:Ushering in a New Age for Science[EB/OL].Livermore,CA:Lawrence Livermore National Laboratory,2009.https://lasers.llnl.gov/programs/nif/.
  • 2王奔,吴东江,高航,康仁科.清洗方法对KDP晶体抛光表面质量的影响[J].人工晶体学报,2009,38(2):525-528. 被引量:8
  • 3Katagiri M,Namba Y.Optical Surface Generation of KDP Inorganic Nonlinear Crystals by Ultraprecision Surface Grinding[J].Journal of the Japan Society for Precision Engineering,1999,65(6):888-892.
  • 4Arrasmith S R,Kozhinova I A,Gregg L L,et al.Details of the Polishing Spot in Magnetorheological Finishing (MRF)[A].Proceedings of SPIE[C].1999,3782:92-99.
  • 5张飞虎,郭少龙,张勇.磷酸二氢钾晶体潮解抛光方法[P].中国专利:CN101310922A,2008-11-26.
  • 6Wang B,Gao H.Experimental Study on KDP Crystal Polishing[A].Proceedings of SPIE[C],2007,6722:672209.
  • 7Nikogosyan D N.Nonlinear Optical Crystal:A Complete Survey[M].New York:Springer Press,2005:115-132.
  • 8Li Y.Microelectronic Applications of Chemical Mechanical Planarization[M].New Jersey:Wiley-Interscience,2007:201-247.
  • 9Shinn G B,Korthuis V,Grover G,et al.Chemical-mechanical Polishing[M].Boca Raton:CRC Press,2008:17-1.

二级参考文献13

  • 1Fedder R H, Robey H, Biesiada H, et al. Rapid Growth of Very Large KDP and KD * P Crystals in Support of the National Ignition Facility[ J ]. Proc. of SPIE, 2000,4102 : 152-161.
  • 2Wang B L, Gao H. Experimental Study on KDP Crystal Polishing[J]. Proc. of SPIE, 2007, 6722: 672209-1-672209-6.
  • 3Hawley-Fedder R, Geraghty P, Locke S, et al. NIF Pockels Cell and Frequency Conversion Crystals[ J]. Proc. of SPIE ,2004 ,5341:121-126.
  • 4Xu Q, Wang J, Li W, et al. Defects of KDP Crystal Fabricated by Single Point Diamond Turning[ J]. Proc. of SPIE, 1999, 3862:236-239.
  • 5Rhodes M A, Boley C D, Tarditi A G, et al. Plasma Electrode Pockels Cell for ICF lasers[J]. Proc. of SPIE, 1995,2633:94-104.
  • 6Paisner J A, Boyes J D, Kumpan S A, et al. Conceptual Design of the National Ignition Facility [ J ]. Proc. of SPIE, 1995,2633:2-12.
  • 7滕晓辑.KDP晶体潮解机理及材料溶解可加工性试验研究[D].大连:大连理工大学硕士学位论文,2008.
  • 8Lee T C, Chan C W. Mechanism of the Ultrasonic Machining of Ceramic Composites [ J ]. Journal of Material Processing Technology, 1997,71 (2) :195-201.
  • 9钟迪生.光学元件表面的清洗.激光与红外,1985,4:15-18.
  • 10Xu D L, Xue D F. Ratajczak H, Morphology and Structure Studies of KDP and ADP Crystallites in the Water and Ethanol Solutions[J]. Journal of Molecular Structure,2005. 740:37-45.