摘要
本次试验研究了配碳量及碱度对百灵山高硅赤铁矿粉烧结矿自然粉化的影响,并通过配加低硅赤铁矿粉,有效地抑制了烧结矿的自然粉化.
The effects of carbon proportioning rate and basicity on natural degradationof sinters made from Bailing Shan high--sinica hematite were studied. The serious naturaldegradation of this kind of sinter could be effectively supressed by proportioning some lowsinica bearing iron ore concentrates.
出处
《烧结球团》
北大核心
1998年第5期4-7,共4页
Sintering and Pelletizing