期刊文献+

石化特种设备中的硫化氢应力腐蚀与残余应力 被引量:7

Stress corrosion and residual stress of H_2S in petrochemical special equipment
在线阅读 下载PDF
导出
摘要 针对石化特种设备中硫化氢(H2S)应力腐蚀问题现状,综合比较了国际权威机构NACE,EFC以及ISO发布的最新标准、规范,对H2S应力腐蚀的环境界定、试验方法、影响因素、应力腐蚀评价准则及对材料的要求等做了扼要的综述。同时对焊接残余应力的产生、测定方法、消除措施等进行了论述,列举了实际参与研究的发生应力腐蚀容器的实例及残余应力的影响。 To understand the present status of the issue of H2S stress corrosion in petrochemical special equipment, an integrative comparison among the latest standards released from international authorities such as NACE, EFC and ISO is conducted in this paper. A compendious overview containing the environment definition, test method, influence factor, evaluation standard of stress corrosion and the material demand in H2 S stress corrosion issue is accomplished. Meanwhile, a discussion of the causation, test method and elimination measure of welding residual stress has also been done.
机构地区 北京工业大学
出处 《中国工程科学》 2009年第8期38-43,共6页 Strategic Study of CAE
基金 "十一五"国家科技支撑计划课题(2006BAK02B02)
关键词 H2S应力腐蚀 规范指南 评价准则 焊接残余应力 H2S stress corrosion operation manual evaluation standard welding residual stress
  • 相关文献

参考文献12

  • 1Task Group 081. NACE MR 0175 -2003 ,Version 1 [ S]. Houston : NACE ,2003.1 -41.
  • 2Task Group 085. NACE TM0177 -2006 , Version 1 [S]. Houston : NACE ,2006.1 - 39.
  • 3Task Group 082. NACE TM0284 -2003, Version 1 [ S]. Houston: NACE ,2003.1 - 12.
  • 4Smith L. EFC Publications No. 16, Guidelines on Materials Requirements for Carbon and Low Alloy Steels for H2S - Containing Environments in Oil and Gas Production, 2th edition [ M ]. Great Britain :the European Federation of Corrosion by The Institute of Materials, 1998.1 - 53.
  • 5Fowler C. EFC PublicationNo. 17, Corrosion Resistant Alloys for Oil and Gas Production: Guidelines on General Requirements and Test Methods for H2S Service, Version 1 [ M ]. Great Britain : the European Federation of Corrosion by The Institute of Materials, 1996.
  • 6Zhang Yiliang, Zhang Zhenhai, Xu Xuedong . Repeatedly Dehiscence and Residual Stress of Liquefied Gas Spherical Vessel [ A ]. Advanced Materials Research Vol. 33 - 37 PART 2. [ C ]. Germany: 7^th International Conference on Fracture and Strength of Solids,2008. 1333 - 1336.
  • 7Zhang Yiliang, Xu Xuedong, Sun Yaofeng. Stress Analysis of Large Spherical Vessel with X -ray Diffractometer and Strain Gauge Measurement[A]. Proceedings of the SPIE - The International Society for Optical Engineering vol. 4537 [ C ]. USA: Third International Conference on Experimental Mechanics. 2001.198 -201.
  • 8兰州石油机械研究所.防止湿硫化氢环境中压力容器失效的推荐方法[J].石油化工设备,1986,15(1):33-42.
  • 9陈数俊,应自纯.GB4157-84,金属抗硫化物应力腐蚀开裂恒负荷拉伸试验方法第1版[S].北京:中国标准出版社,1984.436-441.
  • 10王玮,金明秀,柳泽艳,等.GB/T15970.6-2007,金属和合金的腐蚀应力腐蚀试验第6部分:恒载荷或恒位移下预裂纹试样的制备和应用第1版[S].北京:中国标准出版社,2007.1-30.

共引文献12

同被引文献48

引证文献7

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部