摘要
开发了60t钢包炉喂Al线,Ti芯线和B芯线工艺.实践结果表明,Al的平均回收率为78.0%.Ti为92.7%.B为85.0%。
The technology of aluminium, titanium and boron wire-feeding in a 60 t ladle furnace was exploited. The practice results showed that the average yield of 78% for aluminium, 92. 7% for titanium and 85% for boron was obtained.
出处
《特殊钢》
北大核心
1997年第2期30-32,共3页
Special Steel
关键词
钢包炉
喂线
应用
炼钢
Ladle Furnace,Wire-Feeding,Application