摘要 主要研究了不同原料、不同工艺条件对纤维素包装薄膜力学性能的影响。结果表明,棉浆浓度为5%,凝固浴浓度为20%,凝固浴温度为25℃时,可制得有较好力学性能的纤维素包装膜。 The effects of different materials and process factors on mechanical properties were studied. The results showed that when the NMMO concentration of coagulation bath is 20% , the temperature is 25℃, and the cotton pulp concentration is 5%, cellulose packaging films with the excellent mechanical properties can be prepared.
机构地区 天津科技大学
出处 《包装工程》 CAS CSCD 北大核心 2007年第4期7-8,18,共3页 Packaging Engineering
关键词 NMMO 纤维素 包装薄膜 凝固浴 力学性能 NMMO cellulose packaging film coagulation bath mechanical properties
  • 相关文献

参考文献3

  • 1FINK H P,WEIGEL P,PURZ H J,et al.Structural Formation of Regenerated Cellulose Materials from NMMO-solutions[J].Progress in Polymer Science,2001,(26):1473-1524.
  • 2张耀鹏,邵惠丽,沈新元.NMMO工艺绿色薄膜的生产设备[J].产业用纺织品,2000,18(2):32-35. 被引量:6
  • 3FINK H P,WEIGEL P,BOHN A.Supermolecular Structure and Orientation of Blown Cellulose Films[J].Macromol Sci Phys,1999,38(5、6):603-613.

共引文献5

同被引文献64

引证文献5

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部