安钢6号高炉短期休风后炉况的快速恢复 被引量:6

Rapid Reblowing of Angang's No.6 BF Condition after Short Term Damping-down
在线阅读 下载PDF
导出
摘要 安钢6号高炉在长期稳定顺行时,通过精心操作,可以在短期休风后快速恢复炉况,主要方法是:做好前期准备工作;休风时出净渣铁,逐步减风,适当控制水压、水量及顶温;复风时处理好料动、赶料线、恢复富氧喷煤及出铁操作。高炉曾经短期休风108min后,在33min之内恢复全风作业,而炉况稳定顺行。 Rapid re.blowing of Angang's No.6 BF condition after short term damping-down can be realized by aborative operation at the conditions d continuous stable smooth operation. The main methods are introduced as follows: doing anterior prepared work well; a few measures are adopted when short term blowing-down, such as acquiring the mollen slag and iron of computing the quantity from BF theoretietically, reducing the blast pressure gradually, controlling proper water pressure and quantity and furnace top temperature; a aeries of works are suitably carried out when reblowing, including handling BF burden move, achieving to fill ore and coke according to stockline, resumption of oxygen--onriebed pulverized coal-injection and tapping hot metal from taphole. No.6 blast furnace ever recovered the whole blast pressure operation within 32 minutes after blowing-down for 108 minutes, but a stabilizing smoothing of BF operation is ensured.
出处 《山东冶金》 CAS 2006年第6期7-8,共2页 Shandong Metallurgy
关键词 高炉 短期休风 复风 blast furnace short term damping-down reblow
  • 相关文献

参考文献2

共引文献86

同被引文献43

引证文献6

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部