摘要
将含134g/LMo,89g/LWO3,2619g/LCO2-3的Na2WO4原料溶液,用膜电解回收游离碱后,转变钼为硫代钼酸盐,调整溶液浓度,并让其通过三根d200mm及一根d300mm的串联的交换柱,Mo、P、As、Si在一列交换柱的不同部位被除去,而得到纯(NH4)2WO4溶液。
The Na 2WO 4 solution containing Mo 1.34 g/L, WO 3 89 g/L, CO 2 3 26.19 g/L was processed in the expanding test.MoO 2- 4 in aqueous feed was converted into MoS 2- 4 after recovering excess alkali with electromembrane.Thenthe input concentration of feed was regulated, and the feed passed through a series of columns which consist of three d 200 mm and one d 300 mm exchange columns.Mo,P,As,Si were removed in different position of columns. The purified (NH 4) 2WO 4 solution was obtained and the quality of products reached the grade of APT 0(GB10116 88,P R C)
出处
《中国有色金属学报》
EI
CAS
CSCD
1996年第3期54-56,共3页
The Chinese Journal of Nonferrous Metals
关键词
离子交换
膜电解
钨
钼
仲钨酸铵
electromembrane tungsten molybdenum ion exchange