摘要
应用交流阻抗,交流伏安和循环伏安等方法研究了Pb-Ca-Sn-Re合金和Pb-Ca-Sn合金在1.28 V(vs.SCE)和4.5 mol/L硫酸溶液中的阳极行为.结果表明:稀土铅钙合金提高了合金的耐腐蚀性能,同时抑制其阳极膜中Pb(Ⅱ)化合物的生长,从而降低阳极膜的阻抗,提高膜的导电性能,这对改善电池的深循环性能十分有利.
The anodic behaviors of Pb-Ca-Sn-Re and Pb-Ca-Sn alloys were investigated at 1.28 V (vsHg/ H2SO4 ) in 4.5 mol/L sulfuric acid solution by means of ac voltammetry, ac impedance and cyclic voltammetry. The results showed that the corrosion-resistance property of Pb-Ca-Sn-Re alloy is better than that of tradditional Pb-Ca-Sn alloy, the growth of Pb( Ⅱ ) compounds was inhibited in the film of Pb-Ca-Sn-Re alloy, and the film impedance of Pb-Ca-Sn-Re alloy was decreased, indicating that the conductivity of the film was increased, which is helpful to enhance the deep recycling property for lead acid battery.
出处
《电化学》
CAS
CSCD
北大核心
2006年第1期46-49,共4页
Journal of Electrochemistry
基金
科技部中小企业创新基金(03C26216111166)资助