微掺镧钼丝组织和性能 被引量:9

MICROSTRUCTURES AND PROPERTIES OF MOLYBDENUM WIRE DOPED WITH MINIM La_2O_3
在线阅读 下载PDF
导出
摘要 系统地研究了纯钼丝、微掺镧钼丝在不同温度下退火后的组织和性能。结果表明,微掺镧显著地改善了钼丝的强韧性能,提高了钼丝的室温强度和再结晶温度,改善了丝材再结晶后的室温脆性。微掺镧钼丝综合性能明显高于纯钼丝。 The microstructures and properties of molybdenum wire and Mo -La2O3 alloy wire annealed at different temperature are investigated systematically in this paper. It is shown that the recrystallization temperature, toughness and strength at room temperature of this wire are increased greatly by addition of La2O3. The room temperature embrittlement of this wire annealed at high temperature is improved remarkably. It is indicated that the properties of Mo -La2O3 wire are superior to those of pure molybdenum wire.
出处 《中国钼业》 2006年第1期39-41,共3页 China Molybdenum Industry
关键词 钼丝 退火 再结晶 molybdenum wire anneal recrystallization
  • 相关文献

参考文献3

二级参考文献2

  • 1张久兴,Acta Metall Sin,1996年,9卷,2期,94页
  • 2张久兴,Proceedings of 13th Int Plansee Seminar Metallwerk Plansee Reutte,1993年,599页

共引文献12

同被引文献101

引证文献9

二级引证文献45

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部