阀控式铅酸蓄电池正极寿命影响因素 被引量:8

Factors influencing the positive-plate life of valve-regulated lead-acid batteries
在线阅读 下载PDF
导出
摘要 从正极活物层(PAM),活物聚集层(AMCL)和腐蚀层(CL)阐述影响阀控式铅酸(VRLA)蓄电池正极寿命的因素。它包括极板设计、合金元素、铅膏密度和组份、装配压力等。 The factors influencing the positive-plate life of valve-regulated lead-acid (VRLA) batteries have been disscussed in this paper in terms of positive-activemass layer (PAM ), active-mass collecting layer (AMCL) and corrosion layer (CL). The most important are: plate design; alloy composition; density and components of the paste and assemly compression.
作者 陈体衔
机构地区 厦门大学化学系
出处 《蓄电池》 1996年第1期3-5,共3页 Chinese LABAT Man
关键词 铅酸蓄电池 正极寿命 蓄电池 valve-regulated lead/acid battery, positive-plate life
  • 相关文献

参考文献1

二级参考文献18

  • 1[1]PAVLOV D, RUEVSKI S, NAIDENOV V, et al. Influence of temperature, current and number of cycles on the efficiency of the closed oxygen cycle in VRLA batteries [J]. J Power Sources, 2000,85:164—171.
  • 2[2]PAVLOV D, ROGACHEV T. Dependence of the phase composition of the anodic layer on oxygen evolution and anodic corrosion of lead electrode in lead dioxide potential region [J]. Electrochem Acta, 1978,23:1237—1242.
  • 3[3]PAVLOV D, DIMITROV M, PETKOVA G, et al. The effect of selenium on the electrochemical behaviour and corrosion of Pb-Sn alloys used in lead-acid batteries [J]. J Electrochem Soc, 1995,142:2 919—2 927
  • 4[4]NONOGUCHI M, ANDO K. High reliability stationary lead-acid storage battery [J]. Progress in Batteries and Solar Cells, 1978,1:128—134.
  • 5[5]RUETSCHI P, OCKERMAN J. Sealed cells with auxiliary electrodes [J]. Electrochem Technol, 1966,4:383—392.
  • 6[6]NIKOLOV I, PAPAZOV G, PAVLOV D, et al. Tungsten carbide Electrodes for Gas Recombination in Lead/Acid Batteries [J]. J Power Sources, 1990,31:69—77.
  • 7[7]PAPAZOV G, IKOLOV I, PAVLOV D, et al. Sealed lead/acid battery with auxiliary tungsten Carbide electrodes [J]. J Power Sources, 1990,31:79—88.
  • 8[8]PAPAXOV G, NIKOLOV I, PAVLOV D, et al. Lead-acid battery with WC recombination electrodes [J]. Bulletin of Electrochemistry, 1990,6:255—259.
  • 9[9]AKIRA S, MAKOTO Y, MASAO M. Japanese patent: 44—41 239,1969.
  • 10[10]DICK B H. Private communication. 1992.

共引文献12

同被引文献39

引证文献8

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部