纱线有机硅柔软处理后强力下降的原因分析 被引量:4

Cause Analysis of strength Lowering of Yarns after Softening Finishing with Silicone
在线阅读 下载PDF
导出
摘要 纯棉纱线在漂染加工后进行的柔软处理时,其强力不同程度都受到影响,严重时降强达30%左右,这是由于柔软剂中的氨基硅油降低了纤维与纤维之间的摩擦系数,导致纤维的抱合力降低致使其纱线强力下降。只有合理的选择柔软剂,优选柔软工艺,才能使加工后的纱线既有良好的手感,又能使强力下降控制在最小范围,以达到后道加工的上机要求。 Amino-silicone reduces the friction coefficient between fibre to fibre which results in the lowering of cohesion of the fibres and yarn strength. Only through rational selection of softeners and softening finishing process, can good handle and proper yarn strength be obtained.
出处 《染整技术》 CAS 2005年第10期21-24,共4页 Textile Dyeing and Finishing Journal
关键词 柔软剂 柔软处理 摩擦系数 纱线强力 silicone softener softening finishing friction coefficient yarn strength
  • 相关文献

参考文献2

二级参考文献2

  • 1Sabia A J.Modification of the Tactile and Physical Properties of Microfiber Fabric Blends with Silicone Polymers[J]. TCC,1995,27(9): 79-81.
  • 2Drstephem, Mr Graham Budden. Chemical Routes to the Feelgood Factor[J].Textile Month, 1996,(3):33-37.

共引文献9

同被引文献32

引证文献4

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部