A novel ion-imprinted polymer, lead ion-imprinted micro-beads with combination of two functional monomers, was synthesized using the W/O/W polymerization method. Two functional monomers, 1,12-dodecanediol-O,O’-diphen...A novel ion-imprinted polymer, lead ion-imprinted micro-beads with combination of two functional monomers, was synthesized using the W/O/W polymerization method. Two functional monomers, 1,12-dodecanediol-O,O’-diphenyl-phosphonic acid (DDDPA) and 4-vinylpyridine, were used to form a suitable construction with micro-pores fitting the template and recognition sites. The eflects of adsorbent dosage, solution pH and the competitive ions on the adsorption and separation eflciency of lead ions were investigated. The lead ion-imprinted micro-beads were eflcient for lead ions removal from aqueous solution in a broad pH range (4–9), when the adsorbent dosage was above 0.1 g/L. The adsorption process obeyed the pseudo second-order kinetics model and it only took half an hour to reach the equilibrium. The adsorption isotherm of lead ion was described by the Langmuir model (R2 0.99) with a maximum adsorption capacity of 116.9 mg/g. In the presence of competitive ions Co2+ and Cd2+, the lead ion-imprinted micro-beads showed a high selectivity for lead ions. The selectivity coeficient of Pb2+/Cd2+ and Pb2+/Co2+are 99.3 and 114.7, respectively.展开更多
基金supported by the National Natural Science Foundation of China (No. 41072173)the National Science & Technology Pillar Program in the Eleventh Five-year Plan Period of China (No. 2006BAJ04A07)
文摘A novel ion-imprinted polymer, lead ion-imprinted micro-beads with combination of two functional monomers, was synthesized using the W/O/W polymerization method. Two functional monomers, 1,12-dodecanediol-O,O’-diphenyl-phosphonic acid (DDDPA) and 4-vinylpyridine, were used to form a suitable construction with micro-pores fitting the template and recognition sites. The eflects of adsorbent dosage, solution pH and the competitive ions on the adsorption and separation eflciency of lead ions were investigated. The lead ion-imprinted micro-beads were eflcient for lead ions removal from aqueous solution in a broad pH range (4–9), when the adsorbent dosage was above 0.1 g/L. The adsorption process obeyed the pseudo second-order kinetics model and it only took half an hour to reach the equilibrium. The adsorption isotherm of lead ion was described by the Langmuir model (R2 0.99) with a maximum adsorption capacity of 116.9 mg/g. In the presence of competitive ions Co2+ and Cd2+, the lead ion-imprinted micro-beads showed a high selectivity for lead ions. The selectivity coeficient of Pb2+/Cd2+ and Pb2+/Co2+are 99.3 and 114.7, respectively.