Lithium aluminate (LiAlO<sub>2</sub>) powder was synthesized by sol-gel with EDTA method. The resultant powders were characterized by X-Ray Diffraction (XRD) and Scanning Electronic Microscopy (SEM) techni...Lithium aluminate (LiAlO<sub>2</sub>) powder was synthesized by sol-gel with EDTA method. The resultant powders were characterized by X-Ray Diffraction (XRD) and Scanning Electronic Microscopy (SEM) techniques. In addition, several thermoluminescence properties of synthesized LiAlO<sub>2</sub> powder were reported. The results from X-ray diffraction (XRD), the powder prepared by sol-gel with EDTA method showed pure <em>γ</em>-phase when it was calcined at >900°C. Scanning electron microscopy (SEM) results show that the size of the lithium aluminate particles depended strongly on calcination temperature. The linearity is observed of synthesized LiAlO<sub>2</sub> powder by sol-gel with EDTA with regression coefficient (R<sup>2</sup>) is 0.9971.展开更多
By generalizing the isotope effect for elemental superconductors (SCs) to the case of pairing in the 2-phonon exchange mechanism for composite SCs, we give here an explanation of the well-known increase in the critica...By generalizing the isotope effect for elemental superconductors (SCs) to the case of pairing in the 2-phonon exchange mechanism for composite SCs, we give here an explanation of the well-known increase in the critical temperature (Tc) of Bi2Sr2CaCu2O8 from 95 K to 110 K and of Bi2Sr2Ca2Cu3O10 from 105 to 115 - 125 K when Bi and Sr in these are replaced by Tl and Ba, respectively. On this basis, we also give the estimated Tcs of some hypothetical SCs, assuming that they may be fabricated by substitutions similar to Bi → Tl and Sr → Ba.展开更多
文摘Lithium aluminate (LiAlO<sub>2</sub>) powder was synthesized by sol-gel with EDTA method. The resultant powders were characterized by X-Ray Diffraction (XRD) and Scanning Electronic Microscopy (SEM) techniques. In addition, several thermoluminescence properties of synthesized LiAlO<sub>2</sub> powder were reported. The results from X-ray diffraction (XRD), the powder prepared by sol-gel with EDTA method showed pure <em>γ</em>-phase when it was calcined at >900°C. Scanning electron microscopy (SEM) results show that the size of the lithium aluminate particles depended strongly on calcination temperature. The linearity is observed of synthesized LiAlO<sub>2</sub> powder by sol-gel with EDTA with regression coefficient (R<sup>2</sup>) is 0.9971.
文摘By generalizing the isotope effect for elemental superconductors (SCs) to the case of pairing in the 2-phonon exchange mechanism for composite SCs, we give here an explanation of the well-known increase in the critical temperature (Tc) of Bi2Sr2CaCu2O8 from 95 K to 110 K and of Bi2Sr2Ca2Cu3O10 from 105 to 115 - 125 K when Bi and Sr in these are replaced by Tl and Ba, respectively. On this basis, we also give the estimated Tcs of some hypothetical SCs, assuming that they may be fabricated by substitutions similar to Bi → Tl and Sr → Ba.