期刊文献+
共找到7,781篇文章
< 1 2 250 >
每页显示 20 50 100
磁性核壳结构SO_(4)^(2-)/Fe_(3)O_(4)@Al_(2)O_(3)-TiO_(2)催化剂的构建及应用
1
作者 黄雨菲 郑建仙 《食品与机械》 北大核心 2025年第5期19-26,共8页
[目的]构建抗坏血酸棕榈酸酯的磁性固体超强酸催化合成法,解决传统浓硫酸法分离困难、底物氧化及污染问题。[方法]采用共沉淀—溶胶凝胶法制备SO_(4)^(2-)/Fe_(3)O_(4)@Al_(2)O_(3)-TiO_(2),通过Hammett指示剂法、NH3-TPD、VSM进行表征... [目的]构建抗坏血酸棕榈酸酯的磁性固体超强酸催化合成法,解决传统浓硫酸法分离困难、底物氧化及污染问题。[方法]采用共沉淀—溶胶凝胶法制备SO_(4)^(2-)/Fe_(3)O_(4)@Al_(2)O_(3)-TiO_(2),通过Hammett指示剂法、NH3-TPD、VSM进行表征,使用单因素试验验证催化剂对抗坏血酸棕榈酸酯合成的催化活性并优化其反应参数,最后通过循环试验探究催化剂的稳定性。[结果]SO_(4)^(2-)/Fe_(3)O_(4)@Al_(2)O_(3)-TiO_(2)具备超强酸性(Hammett酸度函数表示为H0<-13.75)与高磁响应性(47.08 emu/g),且在反应底物摩尔比(n棕榈酸∶n抗坏血酸)6∶5、反应温度70℃、催化剂质量分数7%、反应时间11 h的优化条件下,抗坏血酸棕榈酸酯产率达61.45%(纯度98.58%),循环5次后仍保持大于50%的抗坏血酸棕榈酸酯产率及高磁分离性能(>20 emu/g)。[结论]制备的固体超强酸SO_(4)^(2-)/Fe_(3)O_(4)@Al_(2)O_(3)-TiO_(2)稳定性好,兼具可回收性与酯化催化活性。 展开更多
关键词 抗坏血酸棕榈酸酯 So_(4)^(2-)/fe_(3)o_(4)@Al_(2)o_(3)-Tio_(2) 固体超强酸 酯化合成 非均相催化剂
在线阅读 下载PDF
Preparation of a Fe_(3)O_(4)@SiO_(2)@Fe-MIL-101 for the Adsorption Removal of Fluoride in Zinc Sulfate Electrolyte
2
作者 LIAO Jia WANG Chunmei +4 位作者 LI Fei YANG Chengcheng GUO Xianyu TAN Wentao LI Hui 《吉首大学学报(自然科学版)》 2025年第3期46-61,共16页
To remove the fluoride in zinc sulfate electrolyte to an appropriate level,mitigate environmental fluoride pollution,and drive the development of the hydrometallurgy industry of zinc,a novel Fe_(3)O_(4)@SiO_(2)@Fe-MIL... To remove the fluoride in zinc sulfate electrolyte to an appropriate level,mitigate environmental fluoride pollution,and drive the development of the hydrometallurgy industry of zinc,a novel Fe_(3)O_(4)@SiO_(2)@Fe-MIL-101 magnetic composite material was successfully synthesized via the one-pot method.Preparation conditions were optimized and structural characterization of this material conducted using FTIR,SEM,EDS,XRD and Hysteresis analysis.The results show that this composite exhibits a more rapid fluoride adsorption dynamics and a higher fluoride adsorption capacity(18.34 mg/g)and its adsorption behavior fitted for the first order dynamic model and the Freundlich isotherm model.The adsorption of fluorine by this composite is mainly physical adsorption according to the mean adsorption energy(1.216 kJ/mol).The interfering ions co-existed in fluoride-containing solutions,like HCO_(3)^(-),NO^(-)and Cl^(-),have a significant effect on fluorine adsorption.This composite has also been proved with magnetism,higher adsorption selectivity and satisfactory reusability.When this composite is employed as an adsorbent for adsorption removing fluoride in zinc sulfate electrolyte,it exhibits higher pH-dependent behavior as well as high fluoride removal efficiency at pH 6.5. 展开更多
关键词 fe_(3)o_(4)@Sio_(2)@fe-MIL-101 composite FLUoRIDE REMoVAL ADSoRPTIoN zinc sulfate electrolyte
在线阅读 下载PDF
Fe/Mg改性γ-Al_(2)O_(3)复合吸附剂硒吸附性能研究
3
作者 谷梦瑶 郭士豪 +3 位作者 樊昊天 刘皓 陈娟 姚洪 《燃烧科学与技术》 北大核心 2025年第4期435-442,共8页
通过浸渍法制备不同摩尔比的Fe/γ-Al_(2)O_(3)复合吸附剂及Mg/Al/Fe三元复合吸附剂,并在固定床上进行硒吸附实验.探讨400~700℃下Fe/γ-Al_(2)O_(3)吸附剂的吸附性能及H_(2)O浓度对两种吸附剂硒吸附特性的影响.结果表明,在500℃、8%H_(... 通过浸渍法制备不同摩尔比的Fe/γ-Al_(2)O_(3)复合吸附剂及Mg/Al/Fe三元复合吸附剂,并在固定床上进行硒吸附实验.探讨400~700℃下Fe/γ-Al_(2)O_(3)吸附剂的吸附性能及H_(2)O浓度对两种吸附剂硒吸附特性的影响.结果表明,在500℃、8%H_(2)O条件下,Fe/Al摩尔比为1∶10的吸附剂表现出最佳硒吸附性能,吸附量为10.968 mg/g,而Mg/Al/Fe吸附剂在20%H_(2)O条件下硒吸附性能最佳,吸附量为9.7606 mg/g.XPS结果显示,烟气中的SeO2与Mg/Al/Fe吸附剂表面的晶格氧结合,提高吸附剂表面的氧缺陷,从而改善吸附性能. 展开更多
关键词 fe-Al_(2)o_(3)复合吸附剂 吸附性能 H_(2)o
在线阅读 下载PDF
ZnFe_(2)O_(4)@Ti_(3)C_(2)T_(x)掺杂复合纳滤膜及其水体中模拟放射性核素ReO_(4)^(−)去除研究
4
作者 吴梦雅 刘晗翀 +2 位作者 周平 吴礼光 王挺 《环境科学学报》 北大核心 2025年第3期185-194,共10页
高效去除水环境中的放射性核素是当前核能开发及其生态环境领域的重要课题.本文基于Ti_(3)C_(2)T_(x)的层状结构、比表面积较大、亲水性较好的特点,采用共沉淀法制备ZnFe_(2)O_(4)插层Ti_(3)C_(2)T_(x)的纳米复合物ZnFe_(2)O_(4)@Ti_(3)... 高效去除水环境中的放射性核素是当前核能开发及其生态环境领域的重要课题.本文基于Ti_(3)C_(2)T_(x)的层状结构、比表面积较大、亲水性较好的特点,采用共沉淀法制备ZnFe_(2)O_(4)插层Ti_(3)C_(2)T_(x)的纳米复合物ZnFe_(2)O_(4)@Ti_(3)C_(2)T_(x),再将其添加到水相介质中通过界面聚合制备ZnFe_(2)O_(4)@Ti_(3)C_(2)T_(x)掺杂聚酰胺复合纳滤膜,用于模拟放射性废水中核素的去除.纳米复合物的结构分析显示,插层在Ti_(3)C_(2)T_(x)片层状中的ZnFe_(2)O_(4)分散均匀,ZnFe_(2)O_(4)的插层可增大Ti_(3)C_(2)T_(x)的层间距;复合纳滤膜结构和性能研究发现,ZnFe_(2)O_(4)@Ti_(3)C_(2)T_(x)的掺杂可增加复合纳滤膜的水传质通道,增强膜的亲水性和荷负电性,复合纳滤膜的水通量较未掺杂TFC膜有较大的提高,盐的截留率也略有增大;复合纳滤膜的孔径,亲水性随纳米复合物中ZnFe_(2)O_(4)/Ti_(3)C_(2)T_(x)质量比的增加而增大,但质量比增加到一定程度后,插层在Ti_(3)C_(2)T_(x)片层中的ZnFe_(2)O_(4)会发生团聚,导致复合纳滤膜的荷负电性减弱,表现为复合纳滤膜的水通量随质量比的增加持续增大,盐的截留率呈先增大后略有下降的趋势.所构建的复合纳滤膜TFN-II-8在处理模拟放射性核素废水时水通量大于25 L·m^(-2)·h^(-1),ReO_(4)^(-)的截留率高于73%,NaCl的截留率在29%左右,且具有较好的运行稳定性. 展开更多
关键词 Ti_(3)C_(2)T_(x) Znfe_(2)o_(4)@Ti_(3)C_(2)T_(x) 纳滤膜 Reo_(4)^(-)的去除
原文传递
Si_(3)N_(4)/Si_(2)N_(2)O复相粉体对Al_(2)O_(3)-SiC-C浇注料性能的影响
5
作者 李有奇 何健 +2 位作者 陈俊峰 张嘉良 李正坤 《耐火材料》 北大核心 2025年第1期1-7,共7页
为了提高Al_(2)O_(3)-SiC-C浇注料的综合服役性能,采用化学燃烧法合成的微晶氮化硅/氮氧化硅(Si_(3)N_(4)/Si_(2)N_(2)O)复相粉体为添加物,以棕刚玉、板状刚玉、碳化硅、活性α-Al_(2)O_(3)微粉、SiO_(2)微粉、纯铝酸钙水泥、单质Si粉... 为了提高Al_(2)O_(3)-SiC-C浇注料的综合服役性能,采用化学燃烧法合成的微晶氮化硅/氮氧化硅(Si_(3)N_(4)/Si_(2)N_(2)O)复相粉体为添加物,以棕刚玉、板状刚玉、碳化硅、活性α-Al_(2)O_(3)微粉、SiO_(2)微粉、纯铝酸钙水泥、单质Si粉和球沥青为原料,制备了Al_(2)O_(3)-SiC-C浇注料。研究了复相粉体外加量(外加质量分数分别为0、1%、2%、3%和5%)对浇注料性能的影响,同时探究Si_(3)N_(4)/Si_(2)N_(2)O增强试样综合性能的作用机制。结果表明:1)Si_(3)N_(4)/Si_(2)N_(2)O复相粉可以显著改善Al_(2)O_(3)-SiC-C浇注料的力学性能、抗氧化性能和抗热震性;2)Si_(3)N_(4)/Si_(2)N_(2)O复相粉通过填充孔隙、促进烧结反应进行、生成晶须状物质等途径优化了浇注料的显微结构,提高了浇注料的综合性能;3)当Si_(3)N_(4)/Si_(2)N_(2)O复相粉外加量为3%(w)时,浇注料的性能最佳。 展开更多
关键词 Si_(3)N_(4)/Si_(2)N_(2)o复相粉 Al_(2)o_(3)-SiC-C浇注料 抗氧化性 抗热震性
在线阅读 下载PDF
杂质烃类对Pt/SO_(4)^(2-)/ZrO_(2)/Al_(2)O_(3)催化剂上正构烷烃异构化的影响
6
作者 周晶晶 宋月芹 黄磊 《当代化工研究》 2025年第16期70-72,共3页
考察了含杂质烃类的正构烷烃在固定床微型反应器和脉冲反应器的异构化规律,进一步通过程序升温表面反应,探索了杂质烃类对正戊烷/正己烷异构化活性影响的原因。结果表明,原料中少量甲基环戊烷,环己烷及苯的存在显著抑制了正构烷烃的异... 考察了含杂质烃类的正构烷烃在固定床微型反应器和脉冲反应器的异构化规律,进一步通过程序升温表面反应,探索了杂质烃类对正戊烷/正己烷异构化活性影响的原因。结果表明,原料中少量甲基环戊烷,环己烷及苯的存在显著抑制了正构烷烃的异构转化。不同原料组分存在竞争性吸附,杂质烃类的吸附能力更强,优先吸附在催化剂上的活跃位点,从而导致正构烷烃的吸附减弱及异构化活性下降。 展开更多
关键词 异构化 轻质烷烃 环烷烃 Pt/So_(4)^(2-)/Zro_(2)/Al_(2)o_(3)
在线阅读 下载PDF
柔性CuFe_(2)O_(4)/Fe_(2)O_(3)纤维的制备及其对Pb(II)的吸附性能
7
作者 施淑颖 刘泽涛 +3 位作者 杨艾霖 游泳霜 郭孜涛 高鹏飞 《西南科技大学学报》 2025年第3期11-18,共8页
开发了一种溶胶-凝胶法体系制备可纺性优良的静电纺丝溶液,利用静电纺丝技术制备前驱体纤维,热处理后制得具有优异柔韧性的磁性CuFe_(2)O_(4)/Fe_(2)O_(3)纤维,并将制得的磁性CuFe_(2)O_(4)/Fe_(2)O_(3)纤维用于吸附重金属离子Pb(II)。... 开发了一种溶胶-凝胶法体系制备可纺性优良的静电纺丝溶液,利用静电纺丝技术制备前驱体纤维,热处理后制得具有优异柔韧性的磁性CuFe_(2)O_(4)/Fe_(2)O_(3)纤维,并将制得的磁性CuFe_(2)O_(4)/Fe_(2)O_(3)纤维用于吸附重金属离子Pb(II)。结果表明:CuFe_(2)O_(4)/Fe_(2)O_(3)纤维的饱和磁化强度达到11.6 emu/g,比表面积为13.162 m^(2)/g;CuFe_(2)O_(4)/Fe_(2)O_(3)纤维不易团聚的结构优势,既可充分发挥材料表面活性位点的吸附作用,使其具有优异的吸附性能,又易于分离,在吸附实验中由Langmuir模型计算出CuFe_(2)O_(4)/Fe_(2)O_(3)纤维对Pb(II)的吸附容量为50.53 mg/g,吸附性能优于CuFe_(2)O_(4)和Fe_(2)O_(3)纳米粒子;CuFe_(2)O_(4)/Fe_(2)O_(3)纤维对Pb(II)有较强的亲和力和优异的循环使用性能,重金属离子在CuFe_(2)O_(4)/Fe_(2)O_(3)纤维上的吸附顺序为Pb(II)>Cu(II)>Cr(II)>Zn(II)>Ni(II),在5次吸附-解吸循环之后纤维吸附剂仍然保持着原始吸附容量的71%以上。具有柔性的磁性纤维为同时提高污染物吸附能力和实现快速磁分离提供了新的解决方案。 展开更多
关键词 磁性吸附剂 Cufe_(2)o_(4)/fe_(2)o_(3) 溶胶-凝胶法 柔性纤维 Pb(Ⅱ)
在线阅读 下载PDF
La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)材料的制备及其光催化还原六价铬的研究
8
作者 刘宇轩 胡蓉仪 刘志华 《环境化学》 北大核心 2025年第10期3717-3730,共14页
通过机械搅拌法原位在O-MoS_(2)上合成可见光驱动的La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)光催化剂,使用XRD、XPS、SEM、TEM和UV-Vis DRS等手段进行表征,研究了材料的光电化学性能和处理Cr(Ⅵ)的性能和机理.结果表明,光催化反应30 min... 通过机械搅拌法原位在O-MoS_(2)上合成可见光驱动的La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)光催化剂,使用XRD、XPS、SEM、TEM和UV-Vis DRS等手段进行表征,研究了材料的光电化学性能和处理Cr(Ⅵ)的性能和机理.结果表明,光催化反应30 min后,La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)(9%)对Cr(Ⅵ)的还原率为85.44%,还原速率(0.06423 min^(−1))远高于Bi_(4)O_(5)Br_(2)(0.02455 min^(−1))和La(OH)_(3)/Bi_(4)O_(5)Br_(2)(0.04334 min^(−1)).根据自由基捕获实验,证明e^(−)是参与Cr(Ⅵ)还原过程的主要活性物质.此外,中性和弱碱性的条件更有利于该材料对六价铬的还原,表明制备的新型La(OH)_(3)/Bi_(4)O_(5)Br_(2)@O-MoS_(2)材料具有良好的实际应用价值. 展开更多
关键词 La(oH)_(3)/Bi_(4)o_(5)Br_(2)@o-MoS_(2) Cr (Ⅵ) 可见光催化.
原文传递
热处理工艺对激光熔覆Ti-10V-2Al-3Fe合金粉末修复Ti-6Al-4V合金组织和性能的影响
9
作者 黄兆亮 魏翔宇 +4 位作者 王红顺 王艳 张峰 高俊杰 刘保侠 《机械工程材料》 北大核心 2025年第9期83-89,共7页
采用激光熔覆Ti-10V-2Al-3Fe合金粉末的方法对轧制态Ti-6Al-4V合金表面进行修复,分别进行650℃×2 h退火和750℃×2 h固溶+510℃×8 h时效处理,研究了热处理工艺对试样不同区域显微组织、硬度和拉伸性能的影响。结果表明:... 采用激光熔覆Ti-10V-2Al-3Fe合金粉末的方法对轧制态Ti-6Al-4V合金表面进行修复,分别进行650℃×2 h退火和750℃×2 h固溶+510℃×8 h时效处理,研究了热处理工艺对试样不同区域显微组织、硬度和拉伸性能的影响。结果表明:沉积态激光熔覆层组织由原始柱状β晶粒以及β晶粒内部的网篮状α相组成,热影响区组织为过饱和针状马氏体;退火后熔覆层的部分网篮组织长大,部分层片状α相转化为等轴α相,热影响区中马氏体减少,形成弥散的(α+β)相,原始组织为片状α相延伸晶粒和β晶界的基体中出现α等轴晶;与退火态相比,固溶时效态激光熔覆层部分网篮组织进一步长大,更多层片状α相转化为等轴α相,热影响区中马氏体进一步减少,基体中出现更多α等轴晶。退火和固溶时效处理降低了激光熔覆层的硬度,对基体和热影响区的总体硬度影响不大。退火处理后基体和激光熔覆层的抗拉强度和屈服强度降低,断后伸长率提高;固溶时效处理使得基体强度降低,断后伸长率提高,使得激光熔覆层强度和断后伸长率同步提高。经750℃×2 h固溶和500℃×8 h时效处理后试样的综合力学性能最好,基体和激光熔覆层的硬度分别为349,373 HV,抗拉强度分别为888,1003 MPa,断后伸长率分别为22.1%和20.9%。 展开更多
关键词 激光熔覆 Ti-10V-2Al-3fe合金熔覆层 热处理 TI-6AL-4V合金 显微组织 拉伸性能
在线阅读 下载PDF
Pharmacokinetic study of 3-(4-chlorophenyl)-7-[2-(piperazin-1-yl)ethoxy]-4H-chromen-4-one,a derivative of soybean isoflavone by LC-MS/MS in normal rats
10
作者 Junrong Hao Mengqiang Lian +2 位作者 Shuang Li Hongyan Yin Chunyan Guo 《Journal of Chinese Pharmaceutical Sciences》 2025年第7期633-643,共11页
3-(4-Chlorophenyl)-7-[2-(piperazin-1-yl)ethoxy]-4H-chromen-4-one(CPEO-43)is a derivative of soybean isoflavone(SI),synthesized by introducing a chlorine atom and a piperazine group into the structure of natural SI.In ... 3-(4-Chlorophenyl)-7-[2-(piperazin-1-yl)ethoxy]-4H-chromen-4-one(CPEO-43)is a derivative of soybean isoflavone(SI),synthesized by introducing a chlorine atom and a piperazine group into the structure of natural SI.In vitro experiments have demonstrated that CPEO-43 exhibits a notable inhibitory effect on both A549 cells and HCT116 cells.For the further development and utilization of CPEO-43,this study aims to establish and validate a liquid chromatography-tandem mass spectrometry(LC-MS/MS)quantitative analysis method for the pharmacokinetic study of CPEO-43.Normal rats were intragastrically administered different doses(2,6,and 20 mg/kg)of CPEO-43,and blood was taken from the ocular venous plexus at different time points.The blood concentration of CPEO-43 at different time points was determined using LC-MS/MS technology,and the pharmacokinetic parameters of the compound were calculated using the pharmacokinetic software DAS.The results indicated that the established LC-MS/MS method complies with the standards for bioanalytical method validation in the Chinese Pharmacopoeia(CHP)and can be applied to the pharmacokinetic study of CPEO-43.The pharmacokinetic software DAS non-compartmental model was successfully used to calculate the C_(max),T_(max),t_(1/2),AUC_(0-∞),MRTs,CL,and Vd pharmacokinetic parameters of the compound at different doses.The results were as follows:62.0±10.5,222.0±28.7,and 1384.5±376.4 ng/mL;8.5±1.2,6.0±0.0,and 11.0±6.2 h;15.6,15.0,and 18.5 h;1517.8±317.0,5328.7±864.4,and 45556.3±22735.6 ng·h/mL;17.8±1.2,17.7±0.8,and 20.0±3.2 h;1370.3±305.9,1153.5±205.6,and 505.3±179.8 mL/kg/h;30843.0±7458.0,24344.0±5237.0,and 13950.3±5996.9 mL/kg.These characteristics are of great significance for understanding the in vivo process of the drug,formulating dosing regimens,and evaluating the safety and efficacy of the drug. 展开更多
关键词 3-(4-Chlorophenyl)-7-[2-(piperazin-l-yl)ethoxy]-4H-chromen-4-one Soybean isoflavone LC-MS/MS Pharmacokinetics
原文传递
Co_(3)(PO_(4))_(2)@rGO-900复合催化剂在析氧反应、锌-空气电池中的应用
11
作者 陈苏苹 李水根 +4 位作者 黄凡 许钧玮 张娜 李玉龙 谢翔宇 《新余学院学报》 2025年第2期1-7,共7页
采用水热法合成了一种磷酸钴与还原型氧化石墨烯的复合材料(Co_(3)(PO_(4))_(2)@rGO)。通过烧结温度的调控,制备了微米级形貌的磷酸盐(2μm)。电化学测试表明,900℃下制得的样品(Co_(3)(PO_(4))_(2)@rGO-900)表现出良好的析氧反应催化活... 采用水热法合成了一种磷酸钴与还原型氧化石墨烯的复合材料(Co_(3)(PO_(4))_(2)@rGO)。通过烧结温度的调控,制备了微米级形貌的磷酸盐(2μm)。电化学测试表明,900℃下制得的样品(Co_(3)(PO_(4))_(2)@rGO-900)表现出良好的析氧反应催化活性(100 mA/cm^(2)下过电位为422 mV,Tafel斜率为103.53 mV/dec)和稳定性。以Co_(3)(PO_(4))_(2)@rGO-900为空气阴极催化剂组装的锌-空气电池器件也表现出良好的催化性能(最大功率密度达62.1 mW/cm)。 展开更多
关键词 Co_(3)(Po_(4))_(2) 还原型氧化石墨烯 氧析出反应 -空气电池
在线阅读 下载PDF
2-(4-氨基-3-氟苯基)-1,1,1,3,3,3-六氟丙-2-醇的微波合成方法研究
12
作者 马婵媛 刘颖楠 《山东化工》 2025年第13期44-46,共3页
含三氟甲基的芳香族化合物在药物化学中具有重要地位,其中2-(4-氨基-3-氟苯基)-1,1,1,3,3,3-六氟丙-2-醇作为关键中间体,其高效合成对新药研发至关重要,本研究以2-氟苯胺与六氟丙酮三水化合物为原料合成该中间体,通过微波辅助技术考察... 含三氟甲基的芳香族化合物在药物化学中具有重要地位,其中2-(4-氨基-3-氟苯基)-1,1,1,3,3,3-六氟丙-2-醇作为关键中间体,其高效合成对新药研发至关重要,本研究以2-氟苯胺与六氟丙酮三水化合物为原料合成该中间体,通过微波辅助技术考察溶剂类型、酸催化剂种类及用量、反应温度和时间对产物收率的影响。实验结果表明,在无溶剂条件下,以对甲苯磺酸为催化剂(1.0 mol),于150℃微波加热30 min,目标产物收率可达92%,较传统甲苯溶剂法(产率25%~30%)显著提升。该方法兼具反应速率快、环境友好、操作简便等优势,为含三氟甲基药物中间体的绿色合成提供了新策略。 展开更多
关键词 2-氟苯胺 六氟丙酮 微波合成 2-(4-氨基-3-氟苯基)-1 1 1 3 3 3-六氟丙-2-
在线阅读 下载PDF
miR-221-3p通过NRF2/GPX4轴调节铁死亡促进乳腺癌细胞转移的分子机制研究 被引量:2
13
作者 张倩 马楠 +2 位作者 李琦 丁伟 张卫群 《河北医学》 2025年第1期22-28,共7页
目的:探究微小RNA(miR)-221-3p通过调节铁死亡对乳腺癌细胞转移的影响及机制。方法:培养人乳腺癌细胞系MCF-7,采用miR-221-3p模拟物(mimic)及mimic阴性对照(NC)转染MCF-7细胞,实时荧光定量PCR(RT-qPCR)检测转染后细胞中miR-221-3p表达,... 目的:探究微小RNA(miR)-221-3p通过调节铁死亡对乳腺癌细胞转移的影响及机制。方法:培养人乳腺癌细胞系MCF-7,采用miR-221-3p模拟物(mimic)及mimic阴性对照(NC)转染MCF-7细胞,实时荧光定量PCR(RT-qPCR)检测转染后细胞中miR-221-3p表达,试剂盒测定转染后细胞中二价铁离子(Fe^(2+))、活性氧(ROS)、还原型谷胱甘肽(GSH)水平。将MCF-7细胞分为对照组、mimic NC组(转染mimic NC)、miR-221-3p mimic组(转染miR-221-3p mimic)、miR-221-3p mimic+Erastin组(转染miR-221-3p mimic并用10μmoL/L Erastin处理),CCK-8检测各组MCF-7细胞增殖活性,Transwell实验检测各组MCF-7细胞迁移数目与侵袭数目,试剂盒测定各组细胞中Fe^(2+)、ROS、GSH水平,细胞免疫荧光双标记染色观察各组MCF-7细胞中核因子E2相关因子2(NRF2)与谷胱甘肽过氧化物酶4(GPX4)表达,蛋白质免疫印记(Western blot)观察各组MCF-7细胞中NRF2、GPX4、溶质载体家族7成员11(SLC7A11)和铁蛋白轻链(FTL)蛋白表达。结果:转染miR-221-3p mimic后,MCF-7细胞中miR-221-3p相对表达量上调(P<0.05),Fe^(2+)含量减少、ROS水平降低(P<0.05),GSH水平升高(P<0.05)。与对照组、mimic NC组比较,miR-221-3p mimic组MCF-7细胞增殖活性升高(P<0.05),迁移数目和侵袭数目增加(P<0.05),Fe^(2+)含量减少、ROS水平降低(P<0.05),GSH水平升高(P<0.05),NRF2和GPX4荧光强度明显增强,NRF2、GPX4、SLC7A11和FTL蛋白相对表达量上调(P<0.05);与miR-221-3p mimic组比较,miR-221-3p mimic+Erastin组MCF-7细胞增殖活性降低(P<0.05),迁移数目和侵袭数目减少(P<0.05),Fe^(2+)含量增加、ROS水平升高且GSH水平降低(P<0.05),NRF2和GPX4荧光强度减弱,NRF2、GPX4、SLC7A11和FTL蛋白相对表达量下调(P<0.05)。结论:miR-221-3p通过抑制铁死亡促进乳腺癌细胞转移,其机制可能与激活NRF2/GPX4轴有关。 展开更多
关键词 微小RNA-221-3p 乳腺癌 铁死亡 转移 核因子E2相关因子2/谷胱甘肽过氧化物酶4
暂未订购
BiOI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结光催化剂的合成与性能研究 被引量:1
14
作者 何林 吴敏 《化工时刊》 CAS 2024年第3期15-22,共8页
半导体光催化技术是解决能源危机和环境污染的有效手段。作者采用一步溶剂热法制备了Bi OI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结催化剂。以X射线衍射、扫描电子显微镜等表征方法对样品进行分析,以双酚S为目标污染物考察了催化剂... 半导体光催化技术是解决能源危机和环境污染的有效手段。作者采用一步溶剂热法制备了Bi OI/g-C_(3)N_(4)/NH_(2)-MIL-53(Fe)三元异质结催化剂。以X射线衍射、扫描电子显微镜等表征方法对样品进行分析,以双酚S为目标污染物考察了催化剂的光催化性能,以自由基捕获实验得出·OH、h^(+)和·O_(2)^(-)在降解过程中均发挥强氧化作用,并基于催化剂光芬顿性能研究以及半导体能带结构,提出其催化光芬顿反应的可能的机理。 展开更多
关键词 Bi oI g-C_(3)N_(4) NH_(2)-MIL-53(fe) 光芬顿法
在线阅读 下载PDF
酸处理制备高性能Co_(3)O_(4)催化剂及其催化分解N_(2)O污染研究
15
作者 万思彤 张琬悦 +2 位作者 杜媛婷 熊英 于海彪 《现代化工》 北大核心 2025年第5期125-130,共6页
Co_(3)O_(4)作为氧化亚氮(N_(2)O)催化分解反应中最有潜力的催化剂,面临着反应温度过高、抗杂质气体性能差等问题。在微观结构上对Co_(3)O_(4)催化剂进行设计,采用酸性环境对Co_(3)O_(4)表面进行适当刻蚀,制备富有缺陷的Co_(3)O_(4)催... Co_(3)O_(4)作为氧化亚氮(N_(2)O)催化分解反应中最有潜力的催化剂,面临着反应温度过高、抗杂质气体性能差等问题。在微观结构上对Co_(3)O_(4)催化剂进行设计,采用酸性环境对Co_(3)O_(4)表面进行适当刻蚀,制备富有缺陷的Co_(3)O_(4)催化剂以提高其催化分解N_(2)O的性能。结果表明,采用0.2 mol/L硝酸,在室温下对Co_(3)O_(4)处理1 h后所得到的0.2MCo_(3)O_(4)-N催化剂活性最佳。N_(2)O的完全催化分解温度由单纯Co_(3)O_(4)的475℃降低至0.2MCo_(3)O_(4)-N的400℃。经硝酸处理后,0.2MCo_(3)O_(4)-N表面产生大量缺陷位点,且比表面积也比未处理前增加1倍,具有一定的介孔结构,孔径约为5.6 nm。由于缺陷位的产生,催化剂表面的Co—O键被弱化。此外,所得催化剂具有很好的催化稳定性,在5%O_(2)和100μL/L NO杂质气体共存于反应气的条件下,该催化剂在400℃持续反应10 h后,催化性能几乎没有降低。 展开更多
关键词 催化分解N_(2)o 酸刻蚀 Co_(3)o_(4) 缺陷位点 杂质气体
原文传递
量子点修饰g-C_(3)N_(4)@Fe_(2)O_(3)纳米杂化材料的制备及在水性环氧-丙烯酸酯乳液中的应用 被引量:2
16
作者 陈细芳 肖玉玲 +1 位作者 刘如佳 张凯 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2024年第4期61-71,共11页
水性环氧-丙烯酸酯乳液(WEP)因污染小、附着力好、耐候性好被广泛应用于涂料领域,但其不尽如意的耐腐蚀性大大限制了其在防腐涂料领域的应用。文中采用煅烧法制备了g-C_(3)N_(4)@Fe_(2)O_(3)纳米杂化材料,微波法制备了柠檬酸碳量子点溶... 水性环氧-丙烯酸酯乳液(WEP)因污染小、附着力好、耐候性好被广泛应用于涂料领域,但其不尽如意的耐腐蚀性大大限制了其在防腐涂料领域的应用。文中采用煅烧法制备了g-C_(3)N_(4)@Fe_(2)O_(3)纳米杂化材料,微波法制备了柠檬酸碳量子点溶液,通过傅里叶变换红外光谱、X射线衍射分析、X射线光电子能谱仪和透射电子显微镜分析了g-C_(3)N_(4)@Fe_(2)O_(3)杂化粒子的结构和形态,采用扫描电子显微镜观察了复合涂层的形貌,通过电化学阻抗谱和盐雾实验研究了WEP、g-C_(3)N_(4)@Fe_(2)O_(3)/WEP、经量子点修饰的g-C_(3)N_(4)@Fe_(2)O_(3)/WEP涂层的耐腐性能。结果表明,Fe_(2)O_(3)粒子成功负载到了g-C_(3)N_(4)纳米片上,经柠檬酸量子点修饰后,g-C_(3)N_(4)@Fe_(2)O_(3)在WEP中具有良好的分散性,经柠檬酸量子点修饰的g-C_(3)N_(4)@Fe_(2)O_(3)/WEP乳液涂膜在质量分数3.5%NaCl溶液中浸泡1 d时阻抗高达1.5×10^(10)Ω·cm^(2),较纯WEP乳液涂膜高出2个数量级;浸泡7 d后,复合涂层阻抗值仍高达8.7×10^(9)Ω·cm^(2);盐雾168 h后复合涂层表面锈蚀较少。 展开更多
关键词 g-C_(3)N_(4)@fe_(2)o_(3)纳米杂化材料 量子点 水性环氧-丙烯酸酯乳液 耐腐蚀性
在线阅读 下载PDF
金属有机骨架和g-C_(3)N_(4)共掺杂改性TiO_(2)光催化性能 被引量:1
17
作者 李宁 臧书杰 +1 位作者 蒋托红 赵鹬 《精细化工》 EI CAS CSCD 北大核心 2024年第9期1941-1948,共8页
以钛酸四丁酯、三聚氰胺、二甲基咪唑和Co(NO_(3))_(2)•6H_(2)O为原料,采用溶胶-凝胶法、高温煅烧法,将类石墨相氮化碳(g-C_(3)N_(4))和二甲基咪唑钴(ZIF-67)与TiO_(2)共掺杂,制备了TiO_(2)-g-C_(3)N_(4)-ZIF-67光催化剂。采用XRD、XPS... 以钛酸四丁酯、三聚氰胺、二甲基咪唑和Co(NO_(3))_(2)•6H_(2)O为原料,采用溶胶-凝胶法、高温煅烧法,将类石墨相氮化碳(g-C_(3)N_(4))和二甲基咪唑钴(ZIF-67)与TiO_(2)共掺杂,制备了TiO_(2)-g-C_(3)N_(4)-ZIF-67光催化剂。采用XRD、XPS、SEM和紫外-可见漫反射光谱(UV-Vis DRS)对TiO_(2)-g-C_(3)N_(4)-ZIF-67进行了表征,对TiO_(2)-g-C_(3)N_(4)-ZIF-67光催化降解甲基橙的催化活性进行了评价,并对其催化机理进行了推测。结果表明,TiO_(2)-g-C_(3)N_(4)-ZIF-67同时包含锐钛矿及少量金红石相TiO_(2)、g-C_(3)N_(4)及ZIF-67;g-C_(3)N_(4)的加入使TiO_(2)的带隙降至2.45 eV,ZIF-67将带隙进一步降至1.91 eV;g-C_(3)N_(4)和ZIF-67的共掺杂降低了带隙,显著提高了TiO_(2)可见光吸收范围(492~649 nm);TiO_(2)-g-C_(3)N_(4)-ZIF-67形成了Ⅱ型异质结,TiO_(2)-g-C_(3)N_(4)与金属有机骨架的结合增强了TiO_(2)光催化降解甲基橙的能力。Co质量分数21.5%的TiO_(2)-g-C_(3)N_(4)-ZIF-67-2具有最佳的光催化降解甲基橙活性,在可见光照射40 min时,甲基橙降解率可达79.92%,3次循环后甲基橙降解率为58.86%(90 min),光催化反应对ZIF-67的结晶度有所影响,进而影响了循环时的光催化活性。 展开更多
关键词 光催化 溶胶-凝胶法 高温煅烧法 Tio_(2) g-C_(3)N_(4) ZIF-67 功能材料
原文传递
基于Fe_(3)O_(4)-MoS_(2)-全氟磺酸纳米复合材料的铅离子电化学传感器 被引量:1
18
作者 刘鑫 刘士兴 +1 位作者 邵佳豪 胡海兵 《微纳电子技术》 CAS 2024年第9期65-73,共9页
采用Fe_(3)O_(4)-MoS_(2)-全氟磺酸复合材料修饰玻碳电极(GCE),基于电化学传感原理,使用阳极方波伏安法检测水中微量的铅离子。通过扫描电子显微镜(SEM)、能量色散X射线光谱仪(EDS)、Raman光谱分析仪和X射线光电子能谱仪(XPS)进行物理... 采用Fe_(3)O_(4)-MoS_(2)-全氟磺酸复合材料修饰玻碳电极(GCE),基于电化学传感原理,使用阳极方波伏安法检测水中微量的铅离子。通过扫描电子显微镜(SEM)、能量色散X射线光谱仪(EDS)、Raman光谱分析仪和X射线光电子能谱仪(XPS)进行物理表征。结果表明Fe_(3)O_(4)已较均匀地分布在MoS_(2)上。为了得到良好的实验效果,优化醋酸盐(Hac-NaAc)缓冲溶液的pH值为3.6,最佳沉积时间为120 s,最佳沉积电位为-0.6 V,在滴加5μL的Fe_(3)O_(4)-MoS_(2)和5μL的全氟磺酸条件下进行测试,实验结果表明在0.1~0.6μmol·L^(-1)铅离子浓度范围,Fe_(3)O_(4)-MoS_(2)-全氟磺酸-GCE传感器的线性度良好,灵敏度和检测限分别为25.05μA/(μmol·L^(-1))和0.11μmol·L^(-1)。该检测方法快速便捷,具有低成本、高效率和易操作的特点。 展开更多
关键词 电化学传感器 fe_(3)o_(4)-MoS_(2)-全氟磺酸 方波伏安法 铅离子 重金属检测
原文传递
Fe基分子筛催化剂应用于NH_(3)选择性催化还原和N_(2)O直接催化分解反应的研究进展
19
作者 明淑君 李新楠 +4 位作者 庞磊 苏长罗 程春晖 杨小东 李涛 《低碳化学与化工》 北大核心 2025年第6期97-112,共16页
柴油车排放的氮氧化物(NO_(x))和氧化亚氮(N_(2)O)对人类健康和生态环境造成了显著危害。NH_(3)选择性催化还原(NH_(3)-SCR)技术是当前控制柴油车尾气中NO_(x)排放的有效方法之一,而N_(2)O的直接催化分解(简称“N_(2)O分解”)则被认为... 柴油车排放的氮氧化物(NO_(x))和氧化亚氮(N_(2)O)对人类健康和生态环境造成了显著危害。NH_(3)选择性催化还原(NH_(3)-SCR)技术是当前控制柴油车尾气中NO_(x)排放的有效方法之一,而N_(2)O的直接催化分解(简称“N_(2)O分解”)则被认为是减少N_(2)O排放的最具潜力的技术。这两种技术的核心均依赖于催化剂的开发与应用。Fe基分子筛催化剂在NH_(3)-SCR和N_(2)O分解反应中展现出了卓越的催化性能,为实现NO_(x)和N_(2)O的同步高效去除提供了一条有前途的路径。综述了Fe基分子筛催化剂在NH_(3)-SCR和N_(2)O分解反应中的催化机理,探讨了Fe基分子筛催化剂的制备方法、拓扑结构、助剂金属掺杂,以及反应环境中共存气体对其理化性质、NH_(3)-SCR活性和N_(2)O分解性能的影响。具体而言,Fe基分子筛催化剂的Fe物种形成与分布受到制备方法和分子筛拓扑结构的显著影响。助剂金属的引入不仅能够增大催化剂的酸性位点含量,还能改善Fe物种的分散性,从而优化其催化性能。此外,共存气体(如NO、O_(2)和H2O)对Fe基分子筛催化剂的N_(2)O分解活性产生不同程度的影响。最后,对Fe基分子筛催化剂的未来研究方向进行了展望,并对催化剂设计优化与性能提升提出了建议。 展开更多
关键词 fe基分子筛催化剂 NH_(3)-SCR N_(2)o直接催化分解 催化机理
在线阅读 下载PDF
固体超强酸SO_4^(2-)/Fe_2O_3的制备及其对甲缩醛合成反应的催化性能 被引量:6
20
作者 颜康 贺新 李树白 《化学试剂》 CAS 北大核心 2017年第1期75-77,共3页
以Fe(NO_3)_3、NH_3·H_2O和H_2SO_4为原料,采用直接沉淀法制备了固体超强酸SO_4^(2-)/Fe_2O_3催化剂,用于甲醇与甲醛催化合成甲缩醛的反应。围绕焙烧温度对催化剂催化活性的影响进行了考察,得到了最佳焙烧温度。用X-射线衍射(XRD)... 以Fe(NO_3)_3、NH_3·H_2O和H_2SO_4为原料,采用直接沉淀法制备了固体超强酸SO_4^(2-)/Fe_2O_3催化剂,用于甲醇与甲醛催化合成甲缩醛的反应。围绕焙烧温度对催化剂催化活性的影响进行了考察,得到了最佳焙烧温度。用X-射线衍射(XRD)、红外光谱(IR)、比表面积(BET)、pH测试等方法对催化剂进行了表征,得到了催化剂比表面积、晶型、活性中心结构等性能参数,使用优化条件下制备的催化剂,反应可得59 wt%甲缩醛的馏出液。 展开更多
关键词 固体超强酸 甲缩醛 so2-4/fe2o3 催化
在线阅读 下载PDF
上一页 1 2 250 下一页 到第
使用帮助 返回顶部