Development of high quality Fe_3O_4/rGO composited electrode for low energy water treatment 被引量:3
1
作者 Ngoc Tuan Trinh Sangho Chung +1 位作者 Jae Kwang Lee Jaeyoung Lee 《Journal of Energy Chemistry》 SCIE EI CAS CSCD 2016年第3期354-360,共7页
Electrochemical water treatment is an attractive technology for water desalination and softening due to its low energy consumption. Especially, capacitive Deionization(CDI) is promising as a future technology for wate... Electrochemical water treatment is an attractive technology for water desalination and softening due to its low energy consumption. Especially, capacitive Deionization(CDI) is promising as a future technology for water treatment. Graphene(rGO) has been intensively studied for CDI electrode because of its advantages such as excellent electrical conductivity and high specific surface area. However, its 2D dimensional structure with small specific capacitance, high resistance between layers and hydrophobicity degrades ion adsorption efficiency. In this work, we successfully prepared uniformly dispersed Fe3O4/rGO nanocomposite by simple thermal reactions and applied it as effective electrodes for CDI. Iron oxides play a role in uniting graphene sheets, and specific capacitance and wettability of electrodes are improved significantly;hence CDI performances are enhanced. The hardness removal of Fe3O4/rGO nanocomposite electrodes can reach 4.3 mg/g at applied voltage of 1.5V, which is 3 times higher than that of separate r GO electrodes.Thus this material is a promising candidate for water softening technology. 展开更多
关键词 Electrochemical water treatment Capacitive deionization Water softening GRAPHEME fe_3o_4/rgo nanocomposite fe_3o_4 nanoparticle
在线阅读 下载PDF
微波响应Fe_(3)O_(4)/ZnTCPP纳米材料抗菌性能研究
2
作者 王柏惠 程昊 张翔宇 《功能材料》 北大核心 2026年第1期235-242,共8页
智能响应抗菌材料在生物医学领域具有广阔应用前景,目前研究较广泛的主要是光响应抗菌材料。然而,光的穿透能力有限,限制其在深部感染领域的应用。针对此问题,研究采用水热法成功制备出微波响应Fe_(3)O_(4)/ZnTCPP复合纳米抗菌材料,并通... 智能响应抗菌材料在生物医学领域具有广阔应用前景,目前研究较广泛的主要是光响应抗菌材料。然而,光的穿透能力有限,限制其在深部感染领域的应用。针对此问题,研究采用水热法成功制备出微波响应Fe_(3)O_(4)/ZnTCPP复合纳米抗菌材料,并通过SEM、TEM、XRD、FT-IR、XPS对其表征,发现球状Fe_(3)O_(4)成功复合在层片状ZnTCPP表面。通过分析材料的反射损耗值(RL)和电磁参数综合考察了复合材料的微波吸收性能,在不同频率条件下复合材料显示出不同的微波吸收性能。Fe_(3)O_(4)/ZnTCPP展现出良好的微波热效应和微波动力性能。体外抗菌测试表明,由于微波热和产生的活性氧协同作用,造成细菌裂解、蛋白质泄露,Fe_(3)O_(4)/ZnTCPP对金黄色葡萄球菌展现出优良抗菌效果,抗菌率达到(99.8±0.14)%。细胞骨架染色实验和MTT实验证明了Fe_(3)O_(4)/ZnTCPP具有良好的生物相容性。这种微波响应Fe_(3)O_(4)/ZnTCPP复合纳米抗菌材料在深部感染治疗方面具有潜在的应用前景。 展开更多
关键词 微波响应 fe_(3)o_(4) ZnTCPP 抗菌纳米材料
在线阅读 下载PDF
以开放实验提高学生创新能力——应用光镊研究Fe_(3)O_(4)微粒的光热转化性能
3
作者 刘帅 杨宇涵 +2 位作者 易天海 傅钟鼎 朱元强 《化工设计通讯》 2026年第2期89-92,共4页
开放实验为本科生提供了认识—实践—再认识的具体途径。光热剂的局部光热转化效率对其在肿瘤临床治疗领域的应用具有决定性意义。光热剂光热转换性能的测定从宏观向局部测量发展,但目前对Fe_(3)O_(4)微粒的局部光热转换效率的测定还未... 开放实验为本科生提供了认识—实践—再认识的具体途径。光热剂的局部光热转化效率对其在肿瘤临床治疗领域的应用具有决定性意义。光热剂光热转换性能的测定从宏观向局部测量发展,但目前对Fe_(3)O_(4)微粒的局部光热转换效率的测定还未见报道。因此,实验通过光镊激光照射固定的Fe_(3)O_(4)微粒,测定了气泡的生长动力学,并通过局部温度的计算,最终得到气泡生长速度与Fe_(3)O_(4)局部光热转化效率的关系。此项目让本科生自己设计并实验,不仅锻炼了他们的动手能力,还激发了他们的创新性。 展开更多
关键词 创新 光热剂 fe_(3)o_(4)微粒 光镊 光热转化效率
在线阅读 下载PDF
Fe_(3)O_(4)@SA纳米酶凝胶微球比色法检测植物性食用油过氧化值
4
作者 王玲 胡逸飞 刘霞 《食品安全质量检测学报》 2026年第1期82-91,共10页
目的 制备具有类过氧化物酶活性的Fe_(3)O_(4)@海藻酸钠(sodium alginate, SA)纳米酶凝胶微球,用于构建检测植物性食用油过氧化值(peroxide value, POV)的比色传感器。方法 通过酶标仪和智能手机采集不同氧化程度油样显色反应后溶液的... 目的 制备具有类过氧化物酶活性的Fe_(3)O_(4)@海藻酸钠(sodium alginate, SA)纳米酶凝胶微球,用于构建检测植物性食用油过氧化值(peroxide value, POV)的比色传感器。方法 通过酶标仪和智能手机采集不同氧化程度油样显色反应后溶液的吸光度值和三原色(red, green, blue, RGB)信息,建立了不同类型植物性食用油POV的标准曲线,并评估了检测方法的准确性及实用性。结果 5种类型植物性食用油的POV在0~0.40 g/100 g的范围内呈现良好的线性关系。与国家标准方法的检测结果相比较,酶标仪比色法和智能手机数字图像比色法的决定系数(determination coefficient, R^(2))均大于0.9500,均方根误差(root mean square error, RMSE)均小于0.1。结论 基于Fe_(3)O_(4)@SA纳米酶凝胶微球活性建立的比色检测体系,具有良好的准确性与实用性,该研究成果将为食品安全因子的检测提供新思路。 展开更多
关键词 fe_(3)o_(4)@SA纳米酶凝胶微球 植物性食用油 比色检测 过氧化值
原文传递
Recyclable Fe_(3)O_(4)-decorated MoS_(2)Nanosheets for Photocatalytic Degradation of Tetracycline
5
作者 SHEN He WANG Yanyan 《发光学报》 北大核心 2026年第2期348-356,共9页
In this work,we report a fabrication of recyclable iron oxide decorated MoS_(2)nanosheets via a facile liq-uid exfoliation approach and solvothermal reaction for visible-light photodegradation of tetracycline.The prep... In this work,we report a fabrication of recyclable iron oxide decorated MoS_(2)nanosheets via a facile liq-uid exfoliation approach and solvothermal reaction for visible-light photodegradation of tetracycline.The prepared Fe_(3)O_(4)-MoS_(2)was characterized by X-ray diffraction,transmission electron microscopy,X-ray photoelectron spectros-copy,Raman spectroscopy,magnetic hysteresis,and nitrogen adsorption-desorption isotherms.Experimental results indicate that,successful attachment of Fe_(3)O_(4)nanoparticles to MoS_(2)sheets has been achieved.The enhanced surface area of Fe_(3)O_(4)-MoS_(2)induced high rates of adsorption and the adsorbed tetracycline was degraded to 90%after 150 min of visible exposure,which is better than that from pure MoS_(2).The introduction of Fe_(3)O_(4)not only enhances the photo-catalytic performance of Fe_(3)O_(4)-MoS_(2),but also enables its convenient recovery from water by an external magnetic field.Furthermore,both the photocatalytic activity and composite phase of Fe_(3)O_(4)-MoS_(2)were well-retained over cy-cles.Owing to its efficient photocatalytic activity,good stability and magnetic recyclability,the Fe_(3)O_(4)-MoS_(2)nano-composite is considered to be a promising photocatalyst for wastewater treatment. 展开更多
关键词 fe_(3)o_(4) MoS_(2) photocatalyst magnetic recyclability
在线阅读 下载PDF
原位构筑双S-Scheme NiO/Fe_(2)O_(3)/g-C_(3)N_(4)异质结协同可见光-Fenton催化降解土霉素
6
作者 毛娜 马欣玥 唐嘉璇 《高校化学工程学报》 北大核心 2026年第1期146-158,共13页
针对g-C_(3)N_(4)对可见光响应效率低和光生电子-空穴分离效率较低的问题,提出将半导体负载到g-C_(3)N_(4)表面的方法,可以提升g-C_(3)N_(4)在光催化降解有机污染物中的应用。文中采用浸渍法合成了三元复合材料NiO/Fe_(2)O_(3)/g-C_(3)N... 针对g-C_(3)N_(4)对可见光响应效率低和光生电子-空穴分离效率较低的问题,提出将半导体负载到g-C_(3)N_(4)表面的方法,可以提升g-C_(3)N_(4)在光催化降解有机污染物中的应用。文中采用浸渍法合成了三元复合材料NiO/Fe_(2)O_(3)/g-C_(3)N_(4),对复合材料进行X射线衍射(XRD)、傅里叶变换红外光谱(FT-IR)、荧光光谱(PL)等表征,研究NiO/Fe_(2)O_(3)/g-C_(3)N_(4)复合材料对土霉素(OTC)光催化降解的性能。研究结果表明,在可见光-类Fenton体系中,OTC的降解率达89.1%。在添加空穴捕获剂三乙醇胺后,OTC溶液的降解效率由89.1%下降至42.1%,空穴(h^(+))、超氧自由基(·O_(2)^(-))和羟基自由基(·OH)是OTC降解过程的主要影响因素。复合材料具有良好的光催化性能是因为Fe_(2)O_(3)与NiO半导体和g-C_(3)N_(4)形成双S-Scheme异质结可以有效地将电子和空穴分离,抑制电子空穴复合。研究结论为异质结催化剂协同光-Fenton在污水处理中的应用提供参考。 展开更多
关键词 光催化降解 双S-Scheme Nio/fe_(2)o_(3)/g-C_(3)N_(4)复合材料 异质结 可见光-fenton体系 土霉素
在线阅读 下载PDF
ZIF-8/PSF@Fe_(3)O_(4)-ZIF-8有机中空纤维复合膜的制备及其O_(2)/N_(2)分离性能研究
7
作者 张如月 苗泽凤 +1 位作者 刘聪聪 杨腾飞 《现代化工》 北大核心 2026年第2期116-121,共6页
以磁性Fe_(3)O_(4)-ZIF-8核壳粒子作为填料,采用嵌入晶种法在PSF有机中空纤维上制备了ZIF-8/PSF@Fe_(3)O_(4)-ZIF-8复合膜,并对膜结构和O_(2)/N_(2)分离性能进行研究。结果表明,优化条件下PSF中空纤维表面制备了厚度为8.67μm的连续ZIF-... 以磁性Fe_(3)O_(4)-ZIF-8核壳粒子作为填料,采用嵌入晶种法在PSF有机中空纤维上制备了ZIF-8/PSF@Fe_(3)O_(4)-ZIF-8复合膜,并对膜结构和O_(2)/N_(2)分离性能进行研究。结果表明,优化条件下PSF中空纤维表面制备了厚度为8.67μm的连续ZIF-8膜,其O_(2)渗透通量为3.52×10^(-8) mol/(m^(2)·s·Pa),O_(2)/N_(2)理想选择性为4.05。经过216 h运行和20次压力循环(0.1~0.2 MPa)测试,复合膜的O_(2)渗透通量以及O_(2)/N_(2)理想选择性基本保持恒定,表现出优异的长期运行稳定性和良好的制备重现性。相比掺杂纯ZIF-8晶种制备的有机中空纤维膜,ZIF-8/PSF@Fe_(3)O_(4)-ZIF-8有机中空纤维复合膜的O_(2)/N_(2)分离性能得到提升,证实磁性Fe_(3)O_(4)纳米粒子弱吸附和ZIF-8孔道筛分的协同增效作用。 展开更多
关键词 fe_(3)o_(4)-ZIF-8核壳粒子 ZIF-8复合膜 PSF有机中空纤维 嵌入晶种法 o_(2)/N_(2)分离
原文传递
氮碳包覆Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)比例优化与电化学性能研究
8
作者 唐佳城 王超杰 +1 位作者 刘宝生 张绍辉 《电源技术》 北大核心 2026年第2期224-231,共8页
Fe基聚阴离子Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)(NFPP)因其资源丰富,原材料价格低廉而有望成为钠离子电池正极的理想材料。但由于其电子导电率低和离子扩散缓慢的问题使其在实际电池系统中的规模化应用受限。本研究通过固相球磨法梯... Fe基聚阴离子Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)(NFPP)因其资源丰富,原材料价格低廉而有望成为钠离子电池正极的理想材料。但由于其电子导电率低和离子扩散缓慢的问题使其在实际电池系统中的规模化应用受限。本研究通过固相球磨法梯度添加聚乙烯吡咯烷酮(PVP,0%~7%),构建氮掺杂碳包覆NFPP正极材料。该材料表征表明,NFPP展现出不规则的纳米颗粒,适量添加PVP可优化晶体结构并形成多孔形貌,形成三维蜂窝状碳网络。电化学数据显示,NFPP-PVP5%表现出优异的电化学性能,0.2 C时首次充放电的容量为104.15 mAh/g,同时还拥有较好的循环稳定性和倍率性能。通过计算可知NFPP-PVP5%表现出最高的钠离子扩散系数。性能的提升归因于适量的氮掺杂碳层与多孔结构的协同作用,该策略为高性能钠电正极材料设计提供新思路。 展开更多
关键词 钠离子电池 正极材料 Na_(4)fe_(3)(Po_(4))_(2)P_(2)o_(7) 氮碳包覆 电化学性能
在线阅读 下载PDF
碳包覆Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)@C正极材料的制备及其钠离子电池性能
9
作者 裴满 马恬 +3 位作者 陈宇 周熙 陈雷 刘炜 《电池工业》 2026年第1期17-23,共7页
采用溶胶-凝胶法成功制备了碳包覆的磷酸焦磷酸铁钠[Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)@C,缩写为NFPP@C]复合材料,其最优化热处理温度为600℃,烧结时间为10 h。将NFPP@C作为钠离子电池正极材料,分别以金属钠(Na)和硬碳(HC)作为负极材... 采用溶胶-凝胶法成功制备了碳包覆的磷酸焦磷酸铁钠[Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)@C,缩写为NFPP@C]复合材料,其最优化热处理温度为600℃,烧结时间为10 h。将NFPP@C作为钠离子电池正极材料,分别以金属钠(Na)和硬碳(HC)作为负极材料,评测其电化学储钠性能。在1.5~4.0 V(vs. Na+/Na)电压区间下,NFPP@C||Na半电池在0.1 C和5 C电流密度下的放电比容量分别为112.2 mAh/g和96.2 mAh/g,且电流密度为1 C时,循环200次后的容量保持率高达99.7%。在1.5~3.5 V(vs. HC)电压区间、1 C电流密度下,3.5 Ah全电池(即NFPP@C||HC软包单体电池)在25℃常温和45℃高温环境中循环2 800次后的容量保持率分别为92%和89.1%,表现出优异的长循环稳定性和高温工作性能。 展开更多
关键词 钠离子电池 正极材料 碳包覆 Na_(4)fe_(3)(Po_(4))_(2)P_(2)o_(7)@C 储钠性能
在线阅读 下载PDF
Fe_(3)O_(4)/TiO_(2)核壳结构的制备及其对染料废水的光催化降解性能研究
10
作者 高树会 王楠楠 +1 位作者 彭佃钦 朱孟龙 《工业催化》 2026年第1期80-84,共5页
根据Fe_(3)O_(4)包覆TiO_(2)原理,制备了Fe_(3)O_(4)/TiO_(2)核壳结构,并利用X射线衍射对其进行表征,以染料废水为模型分子对其光催化降解性能研究。结果表明,以m(Fe_(3)O_(4))∶m(TiO_(2))=1∶2时制备的Fe_(3)O_(4)+2TiO_(2)作为催化剂... 根据Fe_(3)O_(4)包覆TiO_(2)原理,制备了Fe_(3)O_(4)/TiO_(2)核壳结构,并利用X射线衍射对其进行表征,以染料废水为模型分子对其光催化降解性能研究。结果表明,以m(Fe_(3)O_(4))∶m(TiO_(2))=1∶2时制备的Fe_(3)O_(4)+2TiO_(2)作为催化剂,在催化剂用量2500 mg·L^(-1)、染料废水溶液浓度40 mg·L^(-1)、pH值为3.0和反应时间250 s的最优条件下,对染料废水降解率可达100%。Fe_(3)O_(4)与TiO_(2)之间形成最佳协同效应时,Fe_(3)O_(4)有效增强了光生电子-空穴分离,增强了TiO_(2)光催化性能,提供更多活性位点,扩大了催化接触面积,提升了整体催化性能,达到高效降解染料废水的效果。 展开更多
关键词 水污染防治工程 fe_(3)o_(4)/Tio_(2)核壳结构 染料废水 光催化降解
在线阅读 下载PDF
Facile synthesis of porous Fe_(3)O_(4)/C composites derived from waste residues of soybean and electrolytic manganese for superior electromagnetic wave absorption
11
作者 Zihao Liu Kaixiong Xiang +4 位作者 Yujia Nie Yiting Cheng Shaohua Jiang Han Chen Wei Zhou 《International Journal of Minerals,Metallurgy and Materials》 2026年第2期704-715,共12页
With growing concerns regarding electromagnetic pollution,low-cost,environmentally friendly,and high-performance electromagnetic wave absorption(EWA)materials have attracted significant attention.This paper reports on... With growing concerns regarding electromagnetic pollution,low-cost,environmentally friendly,and high-performance electromagnetic wave absorption(EWA)materials have attracted significant attention.This paper reports on the synthesis of porous Fe_(3)O_(4)/C composites that incorporate dielectric and magnetic loss mechanisms via the carbothermal reduction method and optimization of waste ratio to enhance EWA performance.The Fe_(3)O_(4)/C composites with 10wt%soybean residues(Fe_(3)O_(4)/C-10),demonstrated the best EWA performance,achieving the minimum reflection loss of−56.4 dB and a bandwidth of 2.14 GHz at a thickness of 2.23 mm.This enhanced EWA performance is primarily attributable to improved impedance matching and the synergistic effect between dielectric and magnetic losses.Furthermore,radar cross-sectional simulations confirmed the practical feasibility of the porous Fe_(3)O_(4)/C composites.This study proposes a viable strategy for utilizing soybean residue and electrolytic manganese residue,highlighting their potential applications in EWA. 展开更多
关键词 biomass-derived porous carbon electrolytic manganese residue fe_(3)o_(4) electromagnetic wave absorption
在线阅读 下载PDF
MoS_(2)@Fe_(3)O_(4)类Fenton体系催化降解碘帕醇的性能 被引量:3
12
作者 李昊 石楠 +2 位作者 武道吉 傅凯放 罗从伟 《工业水处理》 北大核心 2025年第1期66-72,共7页
以十六烷基三甲基溴化铵(CTAB)为软模板,以硫代乙酰胺为硫源、钼酸钠为钼源,采用水热两步法制备了MoS_(2)@Fe_(3)O_(4)复合材料。采用SEM、XRD等对MoS_(2)@Fe_(3)O_(4)的形态结构进行了表征分析,考察了MoS_(2)@Fe_(3)O_(4)/H_(2)O_(2)... 以十六烷基三甲基溴化铵(CTAB)为软模板,以硫代乙酰胺为硫源、钼酸钠为钼源,采用水热两步法制备了MoS_(2)@Fe_(3)O_(4)复合材料。采用SEM、XRD等对MoS_(2)@Fe_(3)O_(4)的形态结构进行了表征分析,考察了MoS_(2)@Fe_(3)O_(4)/H_(2)O_(2)体系催化降解碘帕醇(IPM)的效能和作用机理。结果显示,Fe_(3)O_(4)成功负载在MoS_(2)表面,且MoS_(2)@Fe_(3)O_(4)呈均匀分散的花球状结构,提供了更多催化活性位点。在溶液初始pH为4,MoS_(2)@Fe_(3)O_(4)投加量为0.15 g/L,H_(2)O_(2)浓度为0.5 mmol/L,IPM浓度为5μmol/L条件下,反应30 min后MoS_(2)@Fe_(3)O_(4)/H_(2)O_(2)体系对IPM的降解率达到89.85%,与Fe_(3)O_(4)/H_(2)O_(2)体系相比,对IPM的降解率提高约12%。MoS_(2)@Fe_(3)O_(4)/H_(2)O_(2)体系降解IPM的主要活性物种为·OH和^(1)O_(2)。利用外加磁场能够实现MoS_(2)@Fe_(3)O_(4)催化剂的循环再利用,6次循环使用后,反应30 min时MoS_(2)@Fe_(3)O_(4)/H_(2)O_(2)体系对IPM的降解率仍在80%以上,表明MoS_(2)@Fe_(3)O_(4)在反应过程中具有良好的稳定性。 展开更多
关键词 非均相feNToN 二硫化钼 四氧化三铁 碘帕醇
在线阅读 下载PDF
二次碳包覆+N掺杂Na_(4)Fe_(2.91)Cu_(0.09)(PO_(4))_(2)P_(2)O_(7)钠离子电池高倍率正极材料 被引量:1
13
作者 宋登峰 黎扬 +3 位作者 韩影 董静静 王义飞 王新东 《广东化工》 2026年第1期24-28,共5页
钠离子电池(SIB)由于钠资源的高丰度、广泛可用性和低成本而被认为是EES的候选者。Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)(NFPP)具有结构稳定性强、电压窗口适中、成本低、无绿色污染等优点,被认为是一种极具研究价值的钠离子电池正极材料... 钠离子电池(SIB)由于钠资源的高丰度、广泛可用性和低成本而被认为是EES的候选者。Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)(NFPP)具有结构稳定性强、电压窗口适中、成本低、无绿色污染等优点,被认为是一种极具研究价值的钠离子电池正极材料。Na_(4)Fe_(3)(PO_(4))_(2)P_(2)O_(7)的低的电子电导率和铁铝尖晶石不可避免的电化学惰性,在制备过程中,NaFePO_(4)杂质的存在,导致其可逆容量低,循环稳定性差。在此,我们通过一种溶胶凝胶法+球磨法的改进合成方法制备了具有表面N掺杂的二次碳包覆NFCPP正极。表面掺杂、二次碳包覆以及离子掺杂三者协同为NFCPP正极提供了优异的倍率性能(在10 C倍率下82.68 mAh·g^(-1))和出色的循环稳定性,无论是在低倍率(在1.0 C倍率下,100次循环后93.00 mAh·g^(-1),99.00%容量保持率)还是高倍率(在10 C倍率下,1000次循环后77.00 mAh·g^(-1),94.25%容量保持率)。优异电化学性能表明,Cu掺杂减少了NaFePO_(4)杂相的出现,生成了NFPP纯相,同时表面N掺杂的二次碳包覆层和Cu掺杂的结合有利于提高NFPP正极材料的电子导电性,提升了其电化学性能。 展开更多
关键词 钠离子电池 正极材料 铁基磷酸盐 Na_(4)fe_(3)(Po_(4))_(2)P_(2)o_(7)
在线阅读 下载PDF
材料物理实验的创新设计与实践——以Fe_(3)O_(4)/C纳米复合材料的制备及其微波吸收性能分析为例 被引量:1
14
作者 戴鹏 蒋童童 《延边大学学报(自然科学版)》 2025年第2期163-167,共5页
为了改善材料物理实验课程的教学效果,以Fe_(3)O_(4)/C纳米复合材料的制备及其微波吸收性能分析为例,探讨了材料物理实验的创新设计与实践.在实验课程中,将纳米复合材料制备实验,X射线衍射仪、扫描电子显微镜和透射电子显微镜结构表征实... 为了改善材料物理实验课程的教学效果,以Fe_(3)O_(4)/C纳米复合材料的制备及其微波吸收性能分析为例,探讨了材料物理实验的创新设计与实践.在实验课程中,将纳米复合材料制备实验,X射线衍射仪、扫描电子显微镜和透射电子显微镜结构表征实验,以及矢量网络分析仪性能分析实验5个常规实验项目相结合,形成了一个科研驱动式的创新型综合实验课.研究表明,该实验创新设计与实践能够充分提高学生的创新思维、实践技能和团队协作能力,进而可促进学生全面发展和提高高校实验课程的教学质量. 展开更多
关键词 材料物理实验 实验课 fe_(3)o_(4)/C纳米复合材料 微波吸收性能
在线阅读 下载PDF
超级电容器八面体状Fe_(3)O_(4)高性能负极材料的制备与表征
15
作者 张卫国 杨盼 +1 位作者 王宏智 姚素薇 《化学工业与工程》 北大核心 2025年第4期18-26,共9页
采用一步溶剂热法,以Fe^(2+)为铁源制备了Fe_(3)O_(4),并将其作为超级电容器的负极活性材料。通过XRD、SEM、TEM等表征手段结合电化学测试技术研究了Fe_(3)O_(4)的微观结构及电化学性能。调节溶剂热过程中1,2-丙二醇(PG)的添加量,可以... 采用一步溶剂热法,以Fe^(2+)为铁源制备了Fe_(3)O_(4),并将其作为超级电容器的负极活性材料。通过XRD、SEM、TEM等表征手段结合电化学测试技术研究了Fe_(3)O_(4)的微观结构及电化学性能。调节溶剂热过程中1,2-丙二醇(PG)的添加量,可以得到不同形貌的Fe_(3)O_(4),最适宜制备工艺下制备的八面体状Fe_(3)O_(4)在1 A·g^(-1)时比电容为218.7 F·g^(-1)。以Fe_(3)O_(4)为负极,MnO_(2)为正极,组装扣式混合超级电容器(ASC),在5 A·g^(-1)的电流密度下经5000次循环后,ASC的比电容保持率为70%,器件循环稳定性良好。证明Fe_(3)O_(4)作为低成本铁基超级电容器负极材料,具有较高的应用价值。 展开更多
关键词 四氧化三铁 非对称超级电容器 八面体状纳米材料
在线阅读 下载PDF
纳米CuO-Fe_(3)O_(4)高效活化过硫酸氢钾降解含酚废水 被引量:1
16
作者 杨鹏辉 李睿雯 +4 位作者 李高辉 王潇宇 周功睿 邹林涛 鱼涛 《石油化工应用》 2025年第2期93-96,113,共5页
利用共沉淀法制备了纳米CuO-Fe_(3)O_(4)催化剂,用X射线衍射与物理吸附仪对催化剂进行了表征。研究了纳米CuO-Fe_(3)O_(4)高效活化过硫酸氢钾降解含酚废水的性能,考察了催化剂的稳定性,讨论了反应的机理。研究结果表明,纳米CuO-Fe_(3)O_... 利用共沉淀法制备了纳米CuO-Fe_(3)O_(4)催化剂,用X射线衍射与物理吸附仪对催化剂进行了表征。研究了纳米CuO-Fe_(3)O_(4)高效活化过硫酸氢钾降解含酚废水的性能,考察了催化剂的稳定性,讨论了反应的机理。研究结果表明,纳米CuO-Fe_(3)O_(4)中Fe、Cu具有协同效应,与纯相Fe_(3)O_(4)或CuO相比,催化性能显著提高。纳米CuO-Fe_(3)O_(4)高效活化过硫酸氢钾降解含酚废水,在30 min内苯酚去除率可达到92%以上,且pH适用范围广。纳米CuO-Fe_(3)O_(4)催化剂稳定性良好,循环使用4次后去除率仍可达到70%以上。催化剂中的双金属可协同活化过硫酸氢钾,形成高效的氧化降解体系。 展开更多
关键词 Cuo-fe_(3)o_(4) 过硫酸氢钾 苯酚 降解
在线阅读 下载PDF
壳-核结构的Fe_(3)O_(4)/MoS_(2)@MoO_(2)磁性吸附剂性能研究
17
作者 赵红丽 孙涛 +2 位作者 和芹 舒世立 陈伟 《唐山师范学院学报》 2025年第3期1-7,共7页
采用水热法成功制备了具有壳-核结构的Fe_(3)O_(4)/MoS_(2)@MoO_(2)磁性吸附剂,利用控制变量法确定了Fe_(3)O_(4)/MoS_(2)@MoO_(2)吸附剂的组成及最佳吸附条件。实验结果表明25MFO吸附剂具有较好的磁性及吸附性能。25MFO用量为10 mg,罗... 采用水热法成功制备了具有壳-核结构的Fe_(3)O_(4)/MoS_(2)@MoO_(2)磁性吸附剂,利用控制变量法确定了Fe_(3)O_(4)/MoS_(2)@MoO_(2)吸附剂的组成及最佳吸附条件。实验结果表明25MFO吸附剂具有较好的磁性及吸附性能。25MFO用量为10 mg,罗丹明B的初始浓度为1500 mg/L,吸附温度25℃,溶液初始pH值,最大吸附量为3871 mg/g。热力学和动力学分析揭示,25MFO吸附罗丹明B的过程为非均质表面上的多层化学自发吸附。循环5次后25MFO仍具有较高的吸附性能。 展开更多
关键词 fe_(3)o_(4)/MoS_(2)@Moo_(2) 罗丹明B 吸附
在线阅读 下载PDF
钢渣中Fe_(3)O_(4)含量及惰性矿物含量的测定
18
作者 侯新凯 樊晓淇 +2 位作者 王颖 黄树森 王向锋 《建筑材料学报》 北大核心 2025年第10期1046-1052,共7页
采用稀硝酸溶解钢渣测定其Fe_(3)O_(4)含量时,残渣中非晶相和耐火材料杂质(FR)的物理分离较困难。本文提出将稀硝酸溶解后的残渣在NaOH溶液中于90℃下反应1 h以完全溶解非晶相,得到二次残渣S_(12)。对S_(12)有2种处理方式:用溶解法去除F... 采用稀硝酸溶解钢渣测定其Fe_(3)O_(4)含量时,残渣中非晶相和耐火材料杂质(FR)的物理分离较困难。本文提出将稀硝酸溶解后的残渣在NaOH溶液中于90℃下反应1 h以完全溶解非晶相,得到二次残渣S_(12)。对S_(12)有2种处理方式:用溶解法去除Fe_(3)O_(4),拆分测定Fe_(3)O_(4)和FR的含量;或将测得的Fe含量换算成Fe_(3)O_(4)含量。采用乙二胺四乙酸二钠(EDTA)-三乙醇胺(TEA)-二乙胺(DEA)法测定钢渣中惰性矿物含量时,残渣中铁酸二钙(C_(2)F)残留率较高且FR分离困难;采用pH值为12.9的EDTA-TEA复合络合法时,残渣中无C_(2)F残留,此时扣除已知FR含量即可得到惰性矿物含量。 展开更多
关键词 钢渣 fe_(3)o_(4)含量 惰性矿物含量 Ro相含量 消除非晶相
在线阅读 下载PDF
Fe_(3)O_(4)基电磁损耗性能的优化策略和方法
19
作者 肖莉娜 朱街禄 《涂层与防护》 2025年第8期42-48,56,共8页
随着通信技术的快速发展,电磁波在给人类带来便利同时也带来威胁。为了制备出理想的“薄、轻、宽、强”电磁损耗材料,本研究从电磁损耗原理出发,分析影响电磁损耗的关键因素,针对Fe_(3)O_(4)易氧化、密度大、频带窄、阻抗差等缺点,将Fe_... 随着通信技术的快速发展,电磁波在给人类带来便利同时也带来威胁。为了制备出理想的“薄、轻、宽、强”电磁损耗材料,本研究从电磁损耗原理出发,分析影响电磁损耗的关键因素,针对Fe_(3)O_(4)易氧化、密度大、频带窄、阻抗差等缺点,将Fe_(3)O_(4)尺寸纳米化、与其他材料复合及结构设计的优化方式,通过协同作用,提升Fe_(3)O_(4)基电磁损耗性能。 展开更多
关键词 电磁损耗 吸波 铁氧体 fe_(3)o_(4)
在线阅读 下载PDF
Fe_(3)O_(4)/SiO_(2)光热超疏水涂层制备及防除冰性能研究
20
作者 庞杰 王晓鹏 +3 位作者 谢磊 邱文礼 周俊杰 岳越 《稀有金属材料与工程》 北大核心 2025年第8期2118-2124,共7页
固体表面积冰问题对工业领域和人类生活造成了重大影响,因此研究新型防除冰材料具有重要意义。本研究在铝板表面采用低表面能的聚二甲基硅氧烷作为粘合剂,分别喷涂Fe_(3)O_(4)和Fe_(3)O_(4)/SiO_(2)分散液,形成具有光热效应的疏水涂层。... 固体表面积冰问题对工业领域和人类生活造成了重大影响,因此研究新型防除冰材料具有重要意义。本研究在铝板表面采用低表面能的聚二甲基硅氧烷作为粘合剂,分别喷涂Fe_(3)O_(4)和Fe_(3)O_(4)/SiO_(2)分散液,形成具有光热效应的疏水涂层。Fe_(3)O_(4)提供光热效应并在涂层表面形成一定的微纳米粗糙结构,同时加入SiO_(2)修饰后,疏水性进一步增强,接触角可达到155°,可以极大程度地延缓结冰时间并加速冰霜融化。在一个太阳光照度下,温升达到71.8℃。此外,该涂层具有自清洁能力,能够有效避免严重污染,并展现出了一定的抗沙土冲击能力以及良好的机械稳定性,为防冰材料的发展提供了新的方向。 展开更多
关键词 四氧化三铁 二氧化硅 超疏水 除冰性 光热效应 自清洁
原文传递