Fe3O4/carbon nanotubes(Fe3O4/CNTs) nanocomposites were prepared by polylol hightemperature decomposition of the precursor ferric chloride and CNTs in liquid triethylene glycol.After surface modification with hexaned...Fe3O4/carbon nanotubes(Fe3O4/CNTs) nanocomposites were prepared by polylol hightemperature decomposition of the precursor ferric chloride and CNTs in liquid triethylene glycol.After surface modification with hexanediamine,folate was covalently linked to the amine group of magnetic Fe3O4/CNTs nanocomposites.The products were characterized by Fourier-transform infrared spectroscopy,transmission electron microscopy,and vibrating sample magnetometry.Then Fe3O4/CNTs were used as a dual-drug carrier to co-delivery of the hydrophilic drug epirubicin hydrochloride and hydrophobic drug paclitaxel.The results indicated that the Fe3O4/CNTs had a favorable release property for epirubicin and paclitaxel,and thus had potential application in tumor-targeted combination chemotherapy.展开更多
为解决TiO_2光催化纳米材料在使用过程中不易回收的问题,采用直接水解法成功制备了磁性核壳结构Fe_3O_4@TiO_2纳米材料,采用扫描电子显微镜(SEM)、透射电子显微镜(TEM)、X-射线衍射仪(XRD)、傅里叶变换红外光谱仪(FT-IR)等对其物理化学...为解决TiO_2光催化纳米材料在使用过程中不易回收的问题,采用直接水解法成功制备了磁性核壳结构Fe_3O_4@TiO_2纳米材料,采用扫描电子显微镜(SEM)、透射电子显微镜(TEM)、X-射线衍射仪(XRD)、傅里叶变换红外光谱仪(FT-IR)等对其物理化学特性进行了表征,并且考察了制备工艺条件,如钛酸四丁酯(TBOT)用量、氨水用量、反应温度、反应时间等因素对Fe_3O_4@TiO_2纳米颗粒光催化效果的影响。结果表明,TiO_2在Fe_3O_4颗粒表面进行了有效的包覆,形成了良好的包覆层,优化后制备工艺条件为:TBOT用量1.0 m L、氨水用量0.3 m L、制备温度85℃、制备时间4h,所得Fe_3O_4@TiO_2纳米材料对罗丹明B的催化降解效率明显提高,罗丹明B降解率达到98%。对负载前后纳米颗粒的磁滞回线进行测试发现,TiO_2的包覆并未明显减弱Fe_3O_4的磁性,所制备的可回收磁性Fe_3O_4@TiO_2催化剂具有良好的稳定性和重复利用性能。展开更多
基金Funded by Natural Science Fund of Jiangsu Overseas Research&Training Program for University Prominent Young&Middleaged Teachers and Presidents,the Natural Science Fund of Jiangsu Province(No.BK20130094)the Enterprise-universities Cooperative Innovation Fund of Jiangsu Province(No.BY2014016)
文摘Fe3O4/carbon nanotubes(Fe3O4/CNTs) nanocomposites were prepared by polylol hightemperature decomposition of the precursor ferric chloride and CNTs in liquid triethylene glycol.After surface modification with hexanediamine,folate was covalently linked to the amine group of magnetic Fe3O4/CNTs nanocomposites.The products were characterized by Fourier-transform infrared spectroscopy,transmission electron microscopy,and vibrating sample magnetometry.Then Fe3O4/CNTs were used as a dual-drug carrier to co-delivery of the hydrophilic drug epirubicin hydrochloride and hydrophobic drug paclitaxel.The results indicated that the Fe3O4/CNTs had a favorable release property for epirubicin and paclitaxel,and thus had potential application in tumor-targeted combination chemotherapy.
文摘为解决TiO_2光催化纳米材料在使用过程中不易回收的问题,采用直接水解法成功制备了磁性核壳结构Fe_3O_4@TiO_2纳米材料,采用扫描电子显微镜(SEM)、透射电子显微镜(TEM)、X-射线衍射仪(XRD)、傅里叶变换红外光谱仪(FT-IR)等对其物理化学特性进行了表征,并且考察了制备工艺条件,如钛酸四丁酯(TBOT)用量、氨水用量、反应温度、反应时间等因素对Fe_3O_4@TiO_2纳米颗粒光催化效果的影响。结果表明,TiO_2在Fe_3O_4颗粒表面进行了有效的包覆,形成了良好的包覆层,优化后制备工艺条件为:TBOT用量1.0 m L、氨水用量0.3 m L、制备温度85℃、制备时间4h,所得Fe_3O_4@TiO_2纳米材料对罗丹明B的催化降解效率明显提高,罗丹明B降解率达到98%。对负载前后纳米颗粒的磁滞回线进行测试发现,TiO_2的包覆并未明显减弱Fe_3O_4的磁性,所制备的可回收磁性Fe_3O_4@TiO_2催化剂具有良好的稳定性和重复利用性能。