期刊文献+
共找到5,508篇文章
< 1 2 250 >
每页显示 20 50 100
Unidirectionally Sensitive Flexible Resistance Strain Sensor Based on AgNWs/PDMS
1
作者 LIU Xinyue SUN Weiming +6 位作者 HE Mengfan FANG Yuan DJOULDE Aristide DLING Wei LIU Mei MENG Lingjun WANG Zhiming 《Journal of Shanghai Jiaotong university(Science)》 2025年第2期209-219,共11页
The fexible strain sensor has found widespread application due to its excellent fexibility,extensibility,and adaptability to various scenarios.This type of sensors face challenges in direction identification owing to ... The fexible strain sensor has found widespread application due to its excellent fexibility,extensibility,and adaptability to various scenarios.This type of sensors face challenges in direction identification owing to strong coupling between the principal strain and transverse resistance.In this study,a silver nanowires(Ag-NWs)/polydimethylsiloxane(PDMS)strain sensor was developed,using a filtration method for preparing the AgNWs film which was then combined with PDMS to create a unidirectional,highly sensitive,fast-responsive,and linear fexible strain sensor.When the grid width is 0.25 mm,the AgNWs/PDMS strain sensor demonstrates an outstanding unidirectional sensitivity,with a strain response solely along the parallel direction of the grid lines(noise ratioα≈8%),and a fast reaction time of roughly 106.99 ms.In the end,this sensor's ability to detect curvature was also demonstrated through LEDs,demonstrating its potential applications in various fields,including automotive,medical,and wearable devices. 展开更多
关键词 fexible strain sensor silver nanowires(agnws) polydimethylsiloxane(pdms) unidirectional sensitivity
原文传递
PU/AgNWs/PDMS弹性导电复合材料的制备及性能研究 被引量:2
2
作者 张太亮 李黎明 +1 位作者 田天 张径晗 《化工新型材料》 CAS CSCD 北大核心 2016年第5期60-62,66,共4页
通过在预拉伸、经多巴胺改性处理的聚氨酯(PU)薄膜表面喷涂银纳米线(AgNWs),再用聚二甲硅氧烷(PDMS)固化处理得到了性能优良的PU/AgNWs/PDMS弹性导体。研究了PU/AgNWs/PDMS弹性导体在拉伸、弯曲形变下的电学性能。结果表明:经多... 通过在预拉伸、经多巴胺改性处理的聚氨酯(PU)薄膜表面喷涂银纳米线(AgNWs),再用聚二甲硅氧烷(PDMS)固化处理得到了性能优良的PU/AgNWs/PDMS弹性导体。研究了PU/AgNWs/PDMS弹性导体在拉伸、弯曲形变下的电学性能。结果表明:经多巴胺改性处理的PU薄膜对AgNWs的吸附性能增强。所制备的PU/AgNWs/PDMS弹性导体在未形变下的电阻约为0.91Ω,1000次拉伸试验后导体在0%~20%拉伸形变范围内电阻变化很小(〈6%)。PU/AgNWs/PDMS弹性导体经过1000次的弯曲循环后电阻值未增加。 展开更多
关键词 弹性导体 多巴胺改性 银纳米线 电阻 导电复合材料
原文传递
AgNWs/PDMS柔性应变传感器的研制 被引量:3
3
作者 杨镕琛 张庆华 +3 位作者 杜琬婷 许琪 李晨曦 吴子剑 《合成技术及应用》 2021年第1期17-22,共6页
应变传感器凭借其在个人电子设备和工业监控领域的广泛应用推动着现代社会科学技术的飞速发展。基于高分子材料的应变传感器具有可拉伸性及可弯曲性和低成本的独特优势,目前在人工智能系统和可穿戴医疗保健设备中的应用最为广泛。本文... 应变传感器凭借其在个人电子设备和工业监控领域的广泛应用推动着现代社会科学技术的飞速发展。基于高分子材料的应变传感器具有可拉伸性及可弯曲性和低成本的独特优势,目前在人工智能系统和可穿戴医疗保健设备中的应用最为广泛。本文介绍了一种具有高灵敏度的柔性传感器;首先采用了多元醇还原法制备了银纳米线(AgNWs),然后以银纳米线作为中间层,聚二甲基硅氧烷(PDMS)作为包覆层制备具有三明治结构的传感器。将制备的银纳米线通过电子扫描显微镜进行形貌表征,发现AgNWs表面光滑,直径均匀,其长度在20μm左右,直径约为100 nm,长径比在200左右。采用万用电表与拉伸试验机协同工作来表征应变传感器的电阻-应变曲线,发现其响应灵敏,GF值为12.27。滞后性小,电阻与应变间具有较好的线性关系,电学性能的稳定性较高。 展开更多
关键词 柔性应变传感器 银纳米线 聚二甲基硅氧烷 线性 柔韧性
在线阅读 下载PDF
基于激光诱导金属化的PI-PDMS柔性传感器研究
4
作者 潘荣耀 李东亚 +2 位作者 任俊 谷奕丰 刘禹 《传感器与微系统》 北大核心 2026年第1期14-18,共5页
柔性传感器在可穿戴设备、人机交互、医疗、机器人等领域具有巨大的应用潜力,但是柔性传感器制备受到材料特性和工艺制造成本等多方面的制约。本文使用选择性激光诱导金属化和封装工艺相结合,利用力学性能优良的聚二甲基硅氧烷(PDMS)作... 柔性传感器在可穿戴设备、人机交互、医疗、机器人等领域具有巨大的应用潜力,但是柔性传感器制备受到材料特性和工艺制造成本等多方面的制约。本文使用选择性激光诱导金属化和封装工艺相结合,利用力学性能优良的聚二甲基硅氧烷(PDMS)作为介电层,在柔性聚酰亚胺(PI)表面附着铜层作为极板,封装制备出柔性电容式传感器。其关键传感特性的测试结果验证了其应用可行性。结果表明:柔性电容式传感器具有良好的灵敏度(6.29 kPa^(-1))、较快的响应时间(375~625 ms),较低的迟滞性(Δ3.52)以及良好的循环稳定性(循环≥300次)。最后,通过将其布置在皮肤表面和机械臂夹爪等示例,证明本方法及制备的柔性电容式传感器在电子皮肤、可穿戴设备、机器人等领域内具有多样化的应用前景。 展开更多
关键词 柔性电容式传感器 聚二甲基硅氧烷 聚酰亚胺 激光诱导 金属化
在线阅读 下载PDF
用于监测民航试飞员手部运动信号的AgNWs/LIG柔性应变传感器
5
作者 张德银 吴章辉 +2 位作者 范红云 钟勉 李首庆 《电子元件与材料》 北大核心 2025年第12期1398-1407,共10页
石墨烯基柔性应变传感器因其高灵敏度与稳定性,在健康监测和智能可穿戴设备中具有重要应用潜力。然而,石墨烯与柔性衬底之间的弹性模量差异导致界面键合不足,限制了传感器的拉伸性和性能优化。为克服这一瓶颈,采用激光诱导石墨烯(LIG)技... 石墨烯基柔性应变传感器因其高灵敏度与稳定性,在健康监测和智能可穿戴设备中具有重要应用潜力。然而,石墨烯与柔性衬底之间的弹性模量差异导致界面键合不足,限制了传感器的拉伸性和性能优化。为克服这一瓶颈,采用激光诱导石墨烯(LIG)技术,以聚二甲基硅氧烷(PDMS)为衬底,并在石墨烯表面掺杂银纳米线(AgNWs)以构建复合导电网络,制备出高性能柔性应变传感器。实验结果表明,在激光功率密度0.6×10^(6) W/cm^(2)的条件下,器件在15%~17%应变区间表现出优异的灵敏特性,应变系数(GF)高达1517。传感器能够精确捕捉民航试飞员手部运动细节,并在2000次循环拉伸测试后仍保持稳定电学响应,显示出良好的机械耐久性和长期可靠性。AgNWs/LIG复合结构为提升石墨烯柔性应变传感器的性能提供了有效路径,同时为柔性电子器件的设计与应用开辟了新思路。 展开更多
关键词 LIG 柔性应变传感器 手部运动信号 agnws 试飞员
在线阅读 下载PDF
微流控PDMS芯片打孔器在制作免疫组化多组织外对照中的应用
6
作者 李丽 李葵芳 +1 位作者 王雯雯 刘晔 《诊断病理学杂志》 2025年第7期910-912,共3页
目的探索微流控PDMS(聚二甲基硅氧烷)芯片打孔器在制作免疫组化多组织外对照中的可行性及在基层医院病理科推广的优势。方法查询江阴市中医院病理科2021年至2024年的乳腺癌病例,在满足病理诊断后,筛选出剩余肿瘤组织免疫组化HER2蛋白表... 目的探索微流控PDMS(聚二甲基硅氧烷)芯片打孔器在制作免疫组化多组织外对照中的可行性及在基层医院病理科推广的优势。方法查询江阴市中医院病理科2021年至2024年的乳腺癌病例,在满足病理诊断后,筛选出剩余肿瘤组织免疫组化HER2蛋白表达0、1+、2+、3+的蜡块,用PDMS芯片打孔器采样,将采样组织条包埋制成HER2多组织外对照复合块。结果用PDMS芯片打孔器采样制作的HER2多组织对照与待检测组织贴附于同一载玻片,经免疫组化染色后,对照组织排列整齐,节省空间,阳性定位准确,背景清晰,方便阅片。结论本研究在制作免疫组化多组织外对照方法简单实用,所使用的PDMS芯片打孔器价格低廉,操作简单,在基层医院病理科有很好的推广价值,为免疫组化质量评估提供了重要依据。 展开更多
关键词 免疫组织化学 质量控制 多组织外对照复合块 微流控pdms芯片打孔器
原文传递
基于PDMS介质层的双层柔性电容式传感器
7
作者 朱源祥 黄尧 +5 位作者 吴大鸣 许红 郑秀婷 孙靖尧 庄俭 高小龙 《塑料》 北大核心 2025年第4期71-75,共5页
为了得到人体运动状态信息,需精准测量人体关节处的应变,提出了一种制作柔性电容式传感器的方法。采用聚二甲基硅氧烷(PDMS)薄膜作为传感器的介电层,设计了丝网印板的图案,采用丝网印刷的方法将电极材料印刷在介电层薄膜上,使其作为电极... 为了得到人体运动状态信息,需精准测量人体关节处的应变,提出了一种制作柔性电容式传感器的方法。采用聚二甲基硅氧烷(PDMS)薄膜作为传感器的介电层,设计了丝网印板的图案,采用丝网印刷的方法将电极材料印刷在介电层薄膜上,使其作为电极层,形成了具有“三明治”结构的柔性电容式传感器单元。然后,将2个传感器单元贴合在一起,制备为双层柔性电容式传感器。将其放置在测试平台上进行测试。实验结果表明,双层传感器的电极层厚度均匀,其值约为60μm。双层传感器具有更高的初始电容,其值为1.793 nF,在相同应变下,能得到更大的电容变化量,即具有更高的分辨率,能检测到1%的应变。无论是在压力测试还是应变测试下,双层传感器均比单层传感器具有更高的灵敏度(S=0.29 kPa^(-1),GF=0.73),并且,具有较好的耐疲劳性和稳定性。 展开更多
关键词 传感器 pdms 双层 柔性 可穿戴
原文传递
PDMS微流控芯片亲疏水改性方法研究
8
作者 金少搏 刘曾豪 +1 位作者 曹阳 韦学勇 《机械设计与制造》 北大核心 2025年第8期63-66,共4页
作为微流控技术的重要组成部分,液滴微流控技术已成为生物、化学、医疗、材料制备研究的重要手段。囿于微流控芯片自身的亲疏水特性,在不同种类的微液滴制备方面还存在限制,针对PDMS微流控芯片的亲疏水改性问题,通过在PDMS微流道表面制... 作为微流控技术的重要组成部分,液滴微流控技术已成为生物、化学、医疗、材料制备研究的重要手段。囿于微流控芯片自身的亲疏水特性,在不同种类的微液滴制备方面还存在限制,针对PDMS微流控芯片的亲疏水改性问题,通过在PDMS微流道表面制备亲水性聚合物层,探究了基于聚乙烯醇(PVA)涂层的PDMS亲水性处理方法。通过实验研究了该方法对PDMS微流控芯片亲水改性的有效性,并将亲水的PDMS微流控芯片成功用于水包油液滴的制备。该方法进一步发展了PDMS基微流控芯片的亲疏水性改性方法,为拓展PDMS基微流控芯片的功能应用提供了技术支持。 展开更多
关键词 微流控 pdms 亲疏水 微液滴 微流道
在线阅读 下载PDF
多孔PDMS基-凝胶介质材料的疏冰特性研究
9
作者 顾兴士 易贤 李科 《表面技术》 北大核心 2025年第12期195-206,共12页
目的探究孔径对多孔PDMS基-有机凝胶介质材料(GIP-PDMS)疏冰特性的影响,揭示GIP-PDMS的疏冰机制。方法采用“模板析出-浸渍-固化”三步法制备了~200、~400和~1000μm^(3)种不同孔径的GIP-PDMS材料;实验研究了不同孔径GIP-PDMS在静态/动... 目的探究孔径对多孔PDMS基-有机凝胶介质材料(GIP-PDMS)疏冰特性的影响,揭示GIP-PDMS的疏冰机制。方法采用“模板析出-浸渍-固化”三步法制备了~200、~400和~1000μm^(3)种不同孔径的GIP-PDMS材料;实验研究了不同孔径GIP-PDMS在静态/动态结冰、表面磨损、酸碱腐蚀及油污污染等多因素下的疏冰特性;基于内聚力单元仿真模型分析了GIP-PDMS材料的疏冰机制。结果实验表明:GIP-PDMS材料的冰黏附强度显著低于多孔PDMS,且其冰黏附强度与孔隙尺寸呈正相关关系;在-25~-5℃温度范围内、静态/动态结冰条件下~200μm孔径GIP-PDMS材料的冰黏附强度稳定性最好(变化量仅为3.8 kPa);在经历100次重复磨损后,~400μm和~1000μm孔径材料分别表现出最小和最大的冰黏附强度增幅;在动态结冰温度持续降低(-5~-25℃)、表面磨损程度加剧的情况下,孔径为~200μm材料的冰黏附强度呈减小趋势,疏冰性能增强;在强酸(pH=1)强碱(pH=13)腐蚀和油污污染条件下,不同孔径GIP-PDMS冰黏附强度均基本保持不变。仿真表明:在切向除冰过程中GIP-PDMS的骨架与凝胶之间因不同的弹性模量导致材料-冰界面在多位置处出现裂纹萌生与扩展,从而获得优异的疏冰性能。结论GIP-PDMS材料在不同结冰气候条件、表面磨损、酸碱腐蚀及油污污染下仍具有优异的疏冰特性,可为高性能防除冰材料的选择提供参考。 展开更多
关键词 防除冰 冰黏附强度 pdms 多孔介质 界面裂纹 疏冰机制
在线阅读 下载PDF
基于曲面响应法的PDMS硅胶墨水增材制造工艺优化研究
10
作者 付哲 杨树峰 崔向佩 《电加工与模具》 北大核心 2025年第3期60-65,共6页
基于硫醇烯点击化学机理开发了PDMS硅胶墨水,利用气相二氧化硅颗粒增强了光敏PDMS硅胶墨水的初始剪应力,使其能通过挤出式打印方式成形。以二氧化硅颗粒的质量分数、紫外交联时间、紫外曝光距离为变量,交联强度为响应性指标建立回归方程... 基于硫醇烯点击化学机理开发了PDMS硅胶墨水,利用气相二氧化硅颗粒增强了光敏PDMS硅胶墨水的初始剪应力,使其能通过挤出式打印方式成形。以二氧化硅颗粒的质量分数、紫外交联时间、紫外曝光距离为变量,交联强度为响应性指标建立回归方程,对光敏PDMS硅胶墨水的工艺参数进行优化。结果表明,工艺参数对交联强度的影响顺序为:二氧化硅质量分数>紫外交联时间>紫外曝光距离;最优工艺参数组合为:二氧化硅质量分数6.8%,紫外交联时间156.8 s,紫外曝光距离35.0 mm,此时强度的预测值和试验值分别为219.3 kPa和228.8 kPa,两者之间的误差率为4.2%。通过该工艺参数组合可实现PDMS硅胶墨水的高强度成形。 展开更多
关键词 pdms硅胶 紫外交联 增材制造 曲面响应法 工艺优化
在线阅读 下载PDF
Hydrophilic-substrate-assisted Fabrication of Flexible and Transparent Au NTOH@PDMS Film for SERS In-situ Detection of Crystal Violet 被引量:1
11
作者 ZHANG Xin-tong LIU Hong-yu +2 位作者 DONG Ming-yuan WANG Li LIN Xiang 《分析测试学报》 北大核心 2025年第3期411-419,共9页
This article presented a facile fabrication process for polydimethylsiloxane(PDMS)composite gold nanotris⁃octahedra(Au NTOH)for a flexible SERS sensor with high sensitivity.Specifically,Au NTOH with excellent SERS beh... This article presented a facile fabrication process for polydimethylsiloxane(PDMS)composite gold nanotris⁃octahedra(Au NTOH)for a flexible SERS sensor with high sensitivity.Specifically,Au NTOH with excellent SERS behaviors was synthesized using a seed-mediated growth method and the dimensions of the Au NTOH was easily tuned.In addition,the influence of size on the SERS performance of their monolayers was systematically investigated,and the Au NTOH with the size of 61 nm possessed the best SERS performance.Importantly,a hydrophilic-substrateassisted interfacial self-assembled monolayer transfer technique was proposed to transfer Au NTOH onto PDMS films,resulting in forming flexible and transparent Au NTOH@PDMS substrates.Furthermore,the excellent signal homoge⁃neity of this substrate was demonstrated and the sensitivity was verified by a measurement of crystal violet(CV)as low as 1×10^(-8) mol/L.As a result,this SERS sensor is progressing for applying in the identification of trace contaminants in broad fields. 展开更多
关键词 Au NTOH pdms interfacial self-assembly SERS crystal violet
在线阅读 下载PDF
仿Janus结构双层多功能AgNWs-Fe_(3)O_(4)/ANF复合薄膜的制备及性能
12
作者 卞福萍 蔡欣欣 +1 位作者 李韦龙 林树东 《广州化学》 2025年第1期34-38,I0003,共6页
用AgNWs、芳纶及Fe_(3)O_(4)等原料通过真空辅助过滤(TVAF)和热压方法制备了一种模仿Janus结构的高强度AgNWs-Fe_(3)O_(4)/ANF双层异质复合膜,利用XPS、XRD和SEM对合成的AgNWs-Fe_(3)O_(4)/ANF薄膜的结构进行了表征,表明薄膜的成功制备... 用AgNWs、芳纶及Fe_(3)O_(4)等原料通过真空辅助过滤(TVAF)和热压方法制备了一种模仿Janus结构的高强度AgNWs-Fe_(3)O_(4)/ANF双层异质复合膜,利用XPS、XRD和SEM对合成的AgNWs-Fe_(3)O_(4)/ANF薄膜的结构进行了表征,表明薄膜的成功制备。得益于其独一无二的Janus状结构,该双层AgNWs-Fe_(3)O_(4)/ANF复合薄膜的光学照片表明上表面AgNWs和下表面Fe_(3)O_(4)/ANF呈现两种颜色,分别是银色和棕色。通过拉伸和电磁屏蔽测试表明,该复合薄膜拉伸强度为140.1 MPa,断裂应变为13.1%。在8.5 GHz时,AgNWs-Fe_(3)O_(4)/ANF的EMI SE可以达到80.0 dB。AgNWs-Fe_(3)O_(4)/ANF复合薄膜有优良的拉伸性能和电磁屏蔽性能。 展开更多
关键词 agnws 芳纶 类Janus结构 拉伸 电磁屏蔽
在线阅读 下载PDF
直流电压下PDMS/SiO_(2)纳米复合材料的电荷积聚和输运特性
13
作者 张琛 吕泽鹏 +3 位作者 徐子航 曹丹 张馨月 吴锴 《中国电机工程学报》 北大核心 2025年第10期4055-4066,I0041,共13页
介电弹性体(dielectric elastomers,DE)常与柔性电极配合广泛应用于聚合物换能设备中。在高压直流作用下DE材料中的空间电荷积聚和输运过程会引起局部电场畸变,加速绝缘老化及损伤失效,进而影响换能设备长期可靠运行。该文通过红外光谱... 介电弹性体(dielectric elastomers,DE)常与柔性电极配合广泛应用于聚合物换能设备中。在高压直流作用下DE材料中的空间电荷积聚和输运过程会引起局部电场畸变,加速绝缘老化及损伤失效,进而影响换能设备长期可靠运行。该文通过红外光谱、热刺激电流、宽带介电谱、电导测量和直流击穿测试方法表征聚二甲基硅氧烷(polydimethylsiloxane,PDMS)及其纳米复合材料的宏观介电性能;采用电声脉冲法(pulse electroacoustic method,PEA)得到20 kV/mm下不同样品的动态空间电荷分布。结果表明,通过添加适量的纳米二氧化硅(SiO_(2))可以有效降低PDMS低频下的介电损耗,降低直流电导率,提高直流击穿场强。其二,在较高掺杂浓度(>2 phr)的复合材料中,经过表面处理的纳米粒子由于疏水基团相互排斥在PDMS中具有更好的分散性,击穿和电导性能仍有所缓慢提升。此外,热刺激电流和多层阻挡结构的空间电荷测量结果表明引入纳米SiO_(2)增大了深陷阱电荷量和陷阱密度,降低了PDMS的离子电离率和负载流子迁移率,进一步解释了直流高压下复合材料中的空间电荷积聚得到抑制的现象。研究通过添加纳米填料改善直流电压下PDMS的绝缘性能,可用于提升换能装置中DE材料的综合性能。 展开更多
关键词 聚二甲基硅氧烷/二氧化硅 空间电荷 陷阱 迁移率 电离
原文传递
四季海棠花瓣与仿生PDMS微结构的表面浸润性研究
14
作者 王雨萌 刘福军 +1 位作者 孙毅 安伟伟 《科学技术创新》 2025年第19期221-224,共4页
本文利用模板法复制四季海棠花瓣表面微结构,制备得到了聚二甲基硅氧烷(PDMS)仿生微结构表面;采用扫描电子显微镜(SEM)和接触角测量对花瓣和复制样品的表面微观结构及浸润性进行表征。结果表明,花瓣表面具有层次复合微结构,PDMS复制得... 本文利用模板法复制四季海棠花瓣表面微结构,制备得到了聚二甲基硅氧烷(PDMS)仿生微结构表面;采用扫描电子显微镜(SEM)和接触角测量对花瓣和复制样品的表面微观结构及浸润性进行表征。结果表明,花瓣表面具有层次复合微结构,PDMS复制得到的阴结构具有单一结构特征;花瓣表面接触角为139°,仿生PDMS表面接触角为131.3°,均显示出良好的疏水性。本研究利用PDMS复制得到了四季海棠花瓣表面的阴结构,对大面积制备仿生微结构材料具有参考意义。 展开更多
关键词 四季海棠花瓣 pdms 仿生微结构 浸润性
在线阅读 下载PDF
SiO_(2)改性PDMS/E51复合涂层的制备及其疏水性能研究
15
作者 王天琦 姚红蕊 +1 位作者 王娜 刘国凯 《当代化工研究》 2025年第12期66-68,共3页
采用十二烷基三乙氧基硅烷(DTES)对二氧化硅(SiO_(2))进行改性,获得疏水性功能填料(D-SiO_(2)),并将其添加至环氧树脂(E51)与聚二甲基硅氧烷(PDMS)中,制备超疏水涂层。研究结果表明,当PDMS与E51的质量比为6:4时,D-SiO_(2)改性PDMS/E51... 采用十二烷基三乙氧基硅烷(DTES)对二氧化硅(SiO_(2))进行改性,获得疏水性功能填料(D-SiO_(2)),并将其添加至环氧树脂(E51)与聚二甲基硅氧烷(PDMS)中,制备超疏水涂层。研究结果表明,当PDMS与E51的质量比为6:4时,D-SiO_(2)改性PDMS/E51涂层的综合性能最佳。 展开更多
关键词 超疏水涂层 机械耐久性 pdms SiO_(2)
在线阅读 下载PDF
改性SiO_(2)/环氧树脂/PDMS涂层超疏水及耐磨性研究 被引量:1
16
作者 辜雪洋 胡雅 +7 位作者 刘盈 李景旺 袁泽峰 孙嘉庚 汪予安 阮世诚 陶志杰 伍林 《材料保护》 2025年第8期116-127,共12页
为了提高聚二甲基硅氧烷(PDMS)涂层的疏水性及耐磨性,采用KH-570对无定形SiO_(2)颗粒进行改性,将其作为复合涂层的填料提高涂层疏水性,使用环氧树脂E-51提高涂层的耐磨性.研究了填料含量及制备工艺对复合涂层疏水性及耐磨性的影响.结果... 为了提高聚二甲基硅氧烷(PDMS)涂层的疏水性及耐磨性,采用KH-570对无定形SiO_(2)颗粒进行改性,将其作为复合涂层的填料提高涂层疏水性,使用环氧树脂E-51提高涂层的耐磨性.研究了填料含量及制备工艺对复合涂层疏水性及耐磨性的影响.结果表明:KH-570成功对SiO_(2)颗粒改性,KH-570改性SiO_(2)颗粒的加入使得PDMS涂层获得超疏水且具有自清洁功能,确定KH-570改性SiO_(2)颗粒填料含量为5%(质量分数)、混合搅拌时间为20min和固化时间为2h可以制备静态水接触角为154°和水滚动角为2°的耐磨超疏水涂层.添加0.4g的E-51能够使复合涂层的附着力提升到0级且磨损百分比降至2.49%,同时拥有152.7°的静态接触角和9°的水滚动角,且腐蚀电压为-0.364V,腐蚀电流为1.331×10^(-7)A/cm^(2),研究成果预期在海洋防腐工程、微流体器件及智能表面等领域具有重要应用前景. 展开更多
关键词 改性SiO_(2) 超疏水涂层 聚二甲基硅氧烷 耐磨性 环氧树脂
在线阅读 下载PDF
ZIF-67/PDMS复合膜分离废次烟草的中性香气组分
17
作者 刘雨 蔡振波 +1 位作者 纪利俊 马晓华 《化工学报》 北大核心 2025年第5期2337-2347,共11页
从废次烟草中分离中性香气组分是废次烟草资源化利用的重要途径之一。以聚偏氟乙烯(PVDF)为基膜,沸石咪唑酯骨架材料ZIF-67为改性填充物,制备了聚二甲基硅氧烷(PDMS)渗透汽化复合膜用于分离烟草的中性香气组分。采用SEM、FTIR、XRD和接... 从废次烟草中分离中性香气组分是废次烟草资源化利用的重要途径之一。以聚偏氟乙烯(PVDF)为基膜,沸石咪唑酯骨架材料ZIF-67为改性填充物,制备了聚二甲基硅氧烷(PDMS)渗透汽化复合膜用于分离烟草的中性香气组分。采用SEM、FTIR、XRD和接触角测量仪等对复合膜材料进行表征,考察了复合膜对烟草中性香气组分的渗透汽化性能。结果表明,ZIF-67与PDMS基质为物理共混,膜的疏水性增强。随着ZIF-67添加量的增加,渗透通量和分离因子均先增大后减小。当填充量为5%(质量)时,复合膜的分离效果最佳,对2-苯乙醇、大马酮和二氢猕猴桃内酯的最大渗透汽化通量分别为3.61、2.07和0.81 g·m^(-2)·h^(-1);最大分离因子分别为115.5,191.2和109.1。考察了复合膜对实际烟草提取液的分离效果,2-苯乙醇、大马酮和二氢猕猴桃内酯的平均渗透通量分别为16.2、11.6和9.8 mg·m^(-2)·h^(-1)。 展开更多
关键词 渗透汽化 聚二甲基硅氧烷 ZIF-67 中性香气组分 废次烟草
在线阅读 下载PDF
铁路供电调度PDMS系统与SCADA及CTC系统数据交互应用研究
18
作者 李忠源 张博 卫佳乐 《中国铁路》 北大核心 2025年第10期149-154,共6页
铁路供电调度是铁路运输调度的重要组成部分,是实现铁路运输高质量发展的重要环节。随着电气化铁路的快速发展,供电调度承担着日常计划检修、停送电以及协同多工种专业调度开展应急处置,安全风险日益加剧。为提高铁路供电调度管理和应... 铁路供电调度是铁路运输调度的重要组成部分,是实现铁路运输高质量发展的重要环节。随着电气化铁路的快速发展,供电调度承担着日常计划检修、停送电以及协同多工种专业调度开展应急处置,安全风险日益加剧。为提高铁路供电调度管理和应急指挥水平,实现现代化铁路高质量发展,当前国铁企业正在全面建设应用铁路供电调度智能化管理系统(PDMS)。基于“人防、物防、技防”三位一体基本原则,结合兰州局集团公司PDMS系统应用,深度探究各专业、各工种之间技防手段的数据融合,打通各相关系统关联数据壁垒,高效应用关联基础数据,强化铁路运输调度各工种之间的协调配合,实现供电调度主工作平台、铁路供电调度控制主站系统(SCADA)、调度集中系统(CTC)等与供电调度生产关联的外部系统进行数据交换互联,应用数智化技术提高卡控安全能力,进一步提高铁路调度指挥水平,从而保障铁路运输高效安全。 展开更多
关键词 铁路供电调度 pdms SCADA CTC 应急指挥 数据交互 数智化
在线阅读 下载PDF
Research on the Hydrophobic Performance of Bamboo Surface Treated via Coordinated Plasma and PDMS Solution Treatments 被引量:1
19
作者 Zihan Ma Yan Wu +2 位作者 Hongyan Wang Shaofei Yuan Jian Zhang 《Journal of Renewable Materials》 2025年第5期931-955,共25页
Herein,the surface of Moso bamboo was hydrophobically modified by combining O_(2)/N_(2)plasma treatments with polydimethylsiloxane(PDMS)solution treatment as the hydrophobic solution.The effects of plasma treatment pr... Herein,the surface of Moso bamboo was hydrophobically modified by combining O_(2)/N_(2)plasma treatments with polydimethylsiloxane(PDMS)solution treatment as the hydrophobic solution.The effects of plasma treatment process(power and time),PDMS solution concentration,and maceration time on the hydrophobic performance of bamboo specimens were studied,and the optimal treatment conditions for improving the hydrophobicity were determined.Scanning electron microscopy(SEM),fourier transform infrared(FTIR),X-ray diffraction(XRD),and X-ray photoelectron spectroscopy(XPS)were used to analyze the surface morphology,chemical structure,and functional groups in the specimens before and after the plasma and PDMS solution treatments under optimal conditions.Response surface analysis was also performed to determine the optimal treatment conditions.Results show that the hydrophobic performance of the Moso bamboo surface is effectively improved and the surface energy is reduced after the coordinated treatment.The optimal conditions for improving the hydrophobic performance of Moso bamboo surface are a treatment power of 800 W,treatment time of 15 s,O_(2)flow rate of 1.5 L/min,PDMS solution concentration of 5%,and maceration time of 60 min for O_(2)plasma treatment and a treatment power of 1000 W,treatment time of 15 s,N_(2)flow rate of 1.5 L/min,PDMS solution concentration of 5%,and maceration time of 60 min for N_(2)plasma treatment.After treatment,silicone oil particles and plasma etching traces are observed on the bamboo surface.Moreover,Si-O bonds in the PDMS solution are grafted to the bamboo surface via covalent bonds,thereby increasing the contact angle and decreasing the surface energy to achieve the hydrophobic effect. 展开更多
关键词 Moso bamboo pdms MODIFICATION surface hydrophobicity
在线阅读 下载PDF
基于PDMS平台的定制化三维碰撞检查方法研究
20
作者 梁乐 赵千里 +2 位作者 孙冠宇 邬芝胜 蔡鼎阳 《科技与创新》 2025年第8期12-16,共5页
核电站反应堆厂房内部空间紧凑,管道、设备、钢结构等物项之间干涉风险大,因此,对三维综合碰撞检查的需求较高。由于舱室内部模型量较大,干涉检查对计算资源要求高,单次耗费时间长,设计人员布置方案迭代效率低。针对此问题,基于PDMS(Pla... 核电站反应堆厂房内部空间紧凑,管道、设备、钢结构等物项之间干涉风险大,因此,对三维综合碰撞检查的需求较高。由于舱室内部模型量较大,干涉检查对计算资源要求高,单次耗费时间长,设计人员布置方案迭代效率低。针对此问题,基于PDMS(Plant Design Management System)平台、利用平台开发接口,提出了一种优化三维综合碰撞检查的方法。在了解碰撞检查基本原理和逻辑的基础上,筛选出不同的碰撞等级和类型,从而实现对干涉处理的优先级划分。结合设计人员的工程经验,根据不同的系统布置情况定制干涉参数,使碰撞检查更具有针对性,可以减少单次检查时间,节约计算资源,同时预先剔除重复、冗余的干涉报告,大大提高干涉检查的效率和准确性,减少人力浪费,提升布置方案的迭代效率。 展开更多
关键词 pdms平台 优化布置 碰撞检查 干涉分析
在线阅读 下载PDF