摘要
通过Nb+Ti IF钢在1700mm机组上进行的铁素体区热轧试验,表明在现有设备能力条件下,此钢完全可进行铁素体区轧制,若在较高温度(720℃)下卷取,则钢卷中部的伸长率将能达到53%。
The ferritic hot rolling testing of Nb+Ti-IF steel was carried out on the 1700mm mill.The result show that the technology can be realized for the steel under the current equipment condition.If the strip is coiled at high temperature(750℃),the elongation at central coil can be reached 53%.
出处
《轧钢》
2004年第2期7-9,共3页
Steel Rolling
基金
鞍山钢铁集团公司技术中心重点攻关项目(50104004)