摘要
通过对氟碳铈矿煅烧处理,将其中的氟进行回收利用,减少了对大气的污染。实验研究碳酸钠的用量对氟碳锌矿中氟回收率的影响。结果表明:当碳酸钠用量为20%时,氟的回收效果最好。
The paper introduces disposing mine of fluorocarbon cerium, reclaiming fluorin from mine of flu orocarbon cerium,and reducing atmosphere pollution. The experiment researches the influence of sodium carbonate's dose on the rate of reclaiming fluorin from mine of flouro carbon. The results show that the effects of reclaiming fluorin from mine of fluorocarbon cerium is the best under the conditions of 20 persent of sodium carbonate's dose.
出处
《西南科技大学学报》
CAS
2003年第4期63-64,68,共3页
Journal of Southwest University of Science and Technology