摘要
研究了常压下糠醛气相加氢制糠醇催化剂 Cu Cr/γ-Al_2O_3的结构,以及结构对加氢活性的影响;随催化剂中 Cu,Cr 含量的增多,Cu,Cr 在载体γ-Al_2O_3上由高度分散且和γ-Al_2O_3有作用的 CuO,CrO_4^(2-)结构逐步转向 CuCrO_4的结构.催化剂母体中,CuCrO_4的生成提高了还原后的催化剂对糠醛加氢制糠醇的活性.
In this paper,the structure of Cu Cr/γ-A1_2O_3 catalysts and the influence of the struc- ture of catalysts on activities of furfural hydrogenation to furfuryl alcohol was studied. With the advance of Cu Cr contents,Cu Cr which had high degree distribution and acted with γ-Al_2O_3 turned from CuO,CrO_4^(-2) into CuCrO_4 gradually.CuCrO_4 formed in catalyst parents enhanced catalyst activities.
出处
《沈阳化工学院学报》
1992年第2期83-91,共9页
Journal of Shenyang Institute of Chemical Technolgy
关键词
催化剂
糠醛加氢
糠醇
Cu Cr/γ-Al_2O_3 catalyst
hydrogenation of furfural
gas phase hydrogenation
furfuryl alcohol