摘要
介绍了二氧化碳激光辐照拉伸纤维的实验方法 ,纤维的形变特征及纤维的结构与性能 ,与传统热拉伸纤维比较 ,二氧化碳激光拉伸纤维最大形变速率超过 10 4s- 1 ,具有较高强度、模量和韧性。
The experimental methods were introduced for drawn fiber exposed to carbon dioxide laser irradiation, as was the relationship between the deformation characteristics and the structure and properties of the fibers. As compared with traditional heat stretching fiber,drawn fibers exposed to carbon dioxide laser irradiation had the maximal deformation rate above 10 4 s -1 and higher strength,modulus and tenacity.
出处
《合成纤维工业》
CAS
CSCD
北大核心
2003年第3期27-30,共4页
China Synthetic Fiber Industry
基金
高等学校博士点专项科研 ( 2 0 0 10 610 0 2 4)